# US 2016/0254294 A1 · Manufacture method of ltps and manufacture method of tft substrate

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0254294 A1
- Document ID: US20160254294A1
- Status: Published application
- Kind: A1
- Application number: 14/423,124
- Filed: 2015-02-06
- Published: 2016-09-01
- Earliest claimed: 2014-10-30
- Assignees: Shenzhen China Star Optoelectronics Technology Co., Ltd.
- Applicants: Shenzhen China Star Optoelectronics Technology Co., Ltd.
- Inventors: Ya LI
- Web page: https://patentgrep.com/patent/US20160254294A1

## CPC

- H10D 86/0225: {using crystallisation-promoting species, e.g. using a Ni catalyst}
- H10D 30/0314: {of lateral top-gate TFTs comprising only a single gate}
- H10D 30/0321: {comprising silicon, e.g. amorphous silicon or polysilicon}
- H10D 86/0212: {comprising manufacture, treatment or coating of substrates}
- H10D 86/411: {characterised by materials, geometry or structure of the substrates}
- H10D 86/421: {having a particular composition, shape or crystalline structure of the active layer}
- H10D 86/60: wherein the TFTs are in active matrices
- H10P 14/2922: {being non-crystalline insulating materials, e.g. glass or polymers}
- H10P 14/2923: {being conductive materials, e.g. metallic silicides}
- H10P 14/3238: {being insulating materials}
- H10P 14/3241: {being conductive materials}
- H10P 14/3248: {consisting of two layers}
- H10P 14/3411: {Silicon, silicon germanium or germanium}
- H10P 14/3454: {Amorphous}
- H10P 14/3806: {using crystallisation-enhancing elements}
- H10P 14/69215: {the material being a silicon oxide, e.g. SiO2}
- H10P 14/69433: {the material being a silicon nitride not containing oxygen, e.g. SixNy or SixByNz}
- H10P 50/642: {Chemical etching}
- H10P 95/90: Thermal treatments, e.g. annealing or sintering
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

The present invention provides manufacture methods of LTPS and a TFT substrate. The manufacture method of LTPS comprises steps of: step 1, providing a substrate (1); step 2, deposing a buffer layer (2) on the substrate (1); step 3, plating a metal mesh film (3) on the buffer layer (2); step 4, deposing an amorphous silicon layer (4) on the metal mesh film (3); step 5, implementing a rapid thermal annealing process to the amorphous silicon layer (4), and the amorphous silicon layer (4) crystallizes and converts to be a polysilicon layer (5); step 6, removing the metal mesh film (3). The method can effectively reduce the crystallization point, and shorten the crystallization time, and decrease the cost of manufacturing the polysilicon thin film in large scale, and improve the crystallization result to make the crystalline grain bigger and more even.

## Claims

### Claim 1

A manufacture method of LTPS, comprising steps of:
step 1, providing a substrate;
step 2, deposing a buffer layer on the substrate;
step 3, plating a metal mesh film on the buffer layer;
step 4, deposing an amorphous silicon layer on the metal mesh film;
step 5, implementing a rapid thermal annealing process to the amorphous silicon layer, and metal material in the metal mesh film and silicon in the amorphous silicon layer are combined to be metal silicide to induce the amorphous silicon layer to crystallize and convert to be a polysilicon layer;
the metal mesh film having metal silicide is moved up on the polysilicon layer;
step 6, removing the metal mesh film having metal silicide.

### Claim 2 (depends on 1)

The manufacture method of LTPS according to claim 1, wherein material of the metal mesh film is Aluminum.

### Claim 3 (depends on 1)

The manufacture method of LTPS according to claim 1, wherein in the step 5, the temperature of the rapid thermal annealing process is 600° C. and the time is 10 minutes.

### Claim 4 (depends on 1)

The manufacture method of LTPS according to claim 1, wherein the buffer layer is a single SiNx layer, a single SiOx layer, a double SiNx layer, a double SiOx layer or a combination of SiNx layer and SiOx layer.

### Claim 5

A manufacture method of a TFT substrate, comprising steps of:
step 1, providing a substrate;
step 2, deposing a buffer layer on the substrate;
step 3, plating a metal mesh film on the buffer layer;
step 4, deposing an amorphous silicon layer on the metal mesh film;
step 5, implementing a rapid thermal annealing process to the amorphous silicon layer, and metal material in the metal mesh film and silicon in the amorphous silicon layer are combined to be metal silicide to induce the amorphous silicon layer to crystallize and convert to be a polysilicon layer;
the metal mesh film having metal silicide is moved up on the polysilicon layer;
step 6, removing the metal mesh film having metal silicide;
step 7, implementing a patterning process to the polysilicon layer and forming a polysilicon semiconductor layer;
step 8, sequentially forming a gate insulation layer, a gate, an interlayer insulation film, a source/a drain on the polysilicon semiconductor layer, and the source/the drain are connected to the polysilicon semiconductor layer.

### Claim 6 (depends on 5)

The manufacture method of the TFT substrate according to claim 5, wherein material of the metal mesh film is Aluminum.

### Claim 7 (depends on 5)

The manufacture method of the TFT substrate according to claim 5, wherein in the step 5, the temperature of the rapid thermal annealing process is 600° C. and the time is 10 minutes.

### Claim 8 (depends on 5)

The manufacture method of the TFT substrate according to claim 5, wherein the buffer layer is a single SiNx layer, a single SiOx layer, a double SiNx layer, a double SiOx layer or a combination of SiNx layer and SiOx layer.

### Claim 9 (depends on 5)

The manufacture method of the TFT substrate according to claim 5, wherein the step 7 employs photo and etch processes to implement the patterning process to the polysilicon layer.

### Claim 10

A manufacture method of LTPS, comprising steps of:
step 1, providing a substrate;
step 2, deposing a buffer layer on the substrate;
step 3, plating a metal mesh film on the buffer layer;
step 4, deposing an amorphous silicon layer on the metal mesh film;
step 5, implementing a rapid thermal annealing process to the amorphous silicon layer, and metal material in the metal mesh film and silicon in the amorphous silicon layer are combined to be metal silicide to induce the amorphous silicon layer to crystallize and convert to be a polysilicon layer;
the metal mesh film having metal silicide is moved up on the polysilicon layer;
step 6, removing the metal mesh film having metal silicide;
wherein material of the metal mesh film is Aluminum;
wherein in the step 5, the temperature of the rapid thermal annealing process is 600° C. and the time is 10 minutes;
wherein the buffer layer is a single SiNx layer, a single SiOx layer, a double SiNx layer, a double SiOx layer or a combination of SiNx layer and SiOx layer.