# US 2016/0254292 A1 · Manufacturing method of array substrate, array substrate and display apparatus

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0254292 A1
- Document ID: US20160254292A1
- Status: Published application
- Kind: A1
- Application number: 14/767,759
- Filed: 2015-03-20
- Published: 2016-09-01
- Earliest claimed: 2014-10-22
- Assignees: Boe Technology Group Co., Ltd.; Hefei Boe Optoelectronics Technology Co., Ltd.
- Applicants: Boe Technology Group Co., Ltd.; Hefei Boe Optoelectronics Technology Co., Ltd.
- Inventors: Qiyu SHEN
- Web page: https://patentgrep.com/patent/US20160254292A1

## CPC

- H10D 86/021: {of multiple TFTs}
- G02F 1/13439: {characterised by their electrical, optical, physical properties; materials therefor; method of making}
- G02F 1/136286: {Wiring, e.g. gate line, drain line}
- G02F 1/1368: in which the switching element is a three-electrode device {(G02F1/136277 takes precedence)}
- H10D 86/421: {having a particular composition, shape or crystalline structure of the active layer}
- H10D 86/423: {comprising semiconductor materials not belonging to the Group IV, e.g. InGaZnO}
- H10D 86/441: {Interconnections, e.g. scanning lines}
- H10D 86/451: {characterised by the compositions or shapes of the interlayer dielectrics}
- H10D 86/60: wherein the TFTs are in active matrices
- H10P 14/6334: {using decomposition or reaction of gaseous or vapour phase compounds, i.e. chemical vapour deposition (deposition by physical ablation of a target H10P14/6329)}
- G02F 1/133345: {Insulating layers (G02F1/1335, G02F1/1337, G02F1/135, G02F1/136 take precedence)}
- G02F 1/136295: {Materials; Compositions; Manufacture processes}
- H10D 30/6731: {Top-gate only TFTs}
- H10D 30/6732: {Bottom-gate only TFTs}
- H10D 30/6745: {Polycrystalline or microcrystalline silicon}
- H10D 30/6746: {Amorphous silicon}
- H10D 30/6755: {Oxide semiconductors, e.g. zinc oxide, copper aluminium oxide or cadmium stannate}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- G02F: OPTICAL DEVICES OR ARRANGEMENTS FOR THE CONTROL OF LIGHT BY MODIFICATION OF THE OPTICAL PROPERTIES OF THE MEDIA OF THE ELEMENTS INVOLVED THEREIN; NON-LINEAR OPTICS; FREQUENCY-CHANGING OF LIGHT; OPTICAL LOGIC ELEMENTS; OPTICAL ANALOGUE/DIGITAL CONVERTERS
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

The present invention provides a manufacturing method of an array substrate, an array substrate and a display apparatus. The manufacturing method comprises steps of: forming a thin film transistor and a signal line on a glass substrate, and forming an organic insulating layer above the thin film transistor and the signal line correspondingly; forming a passivation insulating layer on the organic insulating layer, wherein, before forming the passivation insulating layer, the manufacturing method further comprises a step of: performing a pre-heating process on the glass substrate on which the organic insulating layer is formed.

## Claims

### Claim 1

A manufacturing method of an array substrate, comprising steps of: forming a thin film transistor and a signal line on a glass substrate, and forming an organic insulating layer above the thin film transistor and the signal line correspondingly; forming a passivation insulating layer on the organic insulating layer, wherein, before forming the passivation insulating layer, the manufacturing method further comprises a step of: performing a pre-heating process on the glass substrate on which the organic insulating layer is formed.

### Claim 2 (depends on 1)

The manufacturing method of claim 1, wherein the passivation insulating layer includes a first passivation layer, and the signal line includes gate lines and data lines, wherein,
the step of forming the thin film transistor and the signal line on the glass substrate and forming the organic insulating layer above the thin film transistor and the signal line correspondingly comprises: step S10, forming the thin film transistor, the gate lines, the data lines and the organic insulating layer on the glass substrate, the organic insulating layer is formed above the thin film transistor, the gate lines and the data lines;
the step of performing the pre-heating process on the glass substrate on which the organic insulating layer is formed comprises: step S11, performing the pre-heating process on the glass substrate subjected to the step S10; and
the step of forming the passivation insulating layer on the organic insulating layer comprises: step S12, forming the first passivation layer on the glass substrate subjected to the step S11.

### Claim 3 (depends on 2)

The manufacturing method of claim 2, further comprises:
step S13, forming a first transparent electrode on the glass substrate subjected to the step S12.

### Claim 4 (depends on 3)

The manufacturing method of claim 3, wherein the passivation insulating layer further includes a second passivation layer, the manufacturing method further comprises:
step S14, performing pre-heating process on the glass substrate subjected to the step S13;
step S15, forming the second passivation layer on the glass substrate subjected to the step S14.

### Claim 5 (depends on 4)

The manufacturing method of claim 4, wherein the second passivation layer includes a buffer layer, a bottom passivation layer and a top passivation layer, and the step of forming the second passivation layer comprises:
step S101, depositing a buffer layer film for forming the buffer layer on the glass substrate subjected to the pre-heating process;
step S102, depositing a bottom passivation layer film for forming the bottom passivation layer on the glass substrate subjected to the step S101;
step S103, depositing a top passivation layer film for forming the top passivation layer on the glass substrate subjected to the step S102; and
step 104, forming a pattern of the second passivation layer by performing exposure, development and etching process once.

### Claim 6 (depends on 5)

The manufacturing method of claim 5, wherein all of the buffer layer film, the bottom passivation layer film and the top passivation layer film are deposited by chemical vapor deposition method.

### Claim 7 (depends on 6)

The manufacturing method of claim 6, wherein,
in the step S101, a deposition power for depositing the buffer layer film ranges from 6 kW to 20 kW, a deposition thickness ranges from 20 mm to 30 mm, a deposition pressure ranges from 600 mTorr to 1000 mTorr, a deposition gas is a mixed gas of SiH4, NH3 and N2, gas flow ratio among SiH4, NH3 and N2 ranges from 1:2.3:15.6 to 1:16:45, and a deposition temperature ranges from 230° C. to 300° C.; in the step S102, the deposition power for depositing the bottom passivation layer film ranges from 6 kW to 18 kW, the deposition thickness ranges from 20 mm to 26 mm, the deposition pressure ranges from 1000 mTorr to 1500 mTorr, the deposition gas is a mixed gas of SiH4, NH3 and N2, gas flow ratio among SiH4, NH3 and N2 ranges from 1:2.5:7.5 to 1:3.2:9.0, and the deposition temperature ranges from 230° C. to 300° C.; and
in the step S103, the deposition power for depositing the top passivation layer film ranges from 6 kW to 15 kW, the deposition thickness ranges from 20 mm to 26 mm, the deposition pressure ranges from 1500 mTorr to 2000 mTorr, the deposition gas is a mixed gas of SiH4, NH3 and N2, gas flow ratio among SiH4, NH3 and N2 ranges from 1:2.5:7.5 to 1:3.2:9.0, and the deposition temperature ranges from 230° C. to 300° C.

### Claim 8 (depends on 4)

The manufacturing method of claim 4, further comprises:
step S16, forming a second transparent electrode on the glass substrate subjected to step S15.

### Claim 9 (depends on 8)

The manufacturing method of claim 8, wherein the first transparent electrode is a pixel electrode and the second transparent electrode is a common electrode, or, the first transparent electrode is a common electrode and the second transparent electrode is a pixel electrode.

### Claim 10 (depends on 1)

The manufacturing method of claim 1, wherein the passivation insulating layer includes a second passivation layer, and the signal line includes gate lines and data lines, wherein,
the step of forming the thin film transistor and the signal line on the glass substrate and forming the organic insulating layer above the thin film transistor and the signal line correspondingly comprises: step S10′, forming the thin film transistor, the gate lines, the data lines, the organic insulating layer, a first passivation layer and a first transparent electrode on the glass substrate, the first passivation layer is formed above the thin film transistor, the gate lines and the data lines, the organic insulating layer is formed on the first passivation layer, the first transparent electrode is formed above the organic insulating layer;
the step of performing pre-heating process on the glass substrate on which the organic insulating layer is formed comprises: step S11′, performing pre-heating process on the glass substrate subjected to the step S10′; and
the step of forming the passivation insulating layer on the organic insulating layer comprises: step S12′, forming the second passivation layer on the glass substrate subjected to the step S11′.

### Claim 11 (depends on 10)

The manufacturing method of claim 10, wherein the second passivation layer includes a buffer layer, a bottom passivation layer and a top passivation layer, and the step of forming the second passivation layer comprises:
step S101, depositing a buffer layer film for forming the buffer layer on the glass substrate subjected to the pre-heating process;
step S102, depositing a bottom passivation layer film for forming the bottom passivation layer on the glass substrate subjected to the step S101;
step S103, depositing a top passivation layer film for forming the top passivation layer on the glass substrate subjected to the step S102; and
step S104, forming a pattern of the second passivation layer by performing exposure, development and etching process once.

### Claim 12 (depends on 11)

The manufacturing method of claim 11, wherein all of the buffer layer film, the bottom passivation layer film and the top passivation layer film are deposited by chemical vapor deposition method.

### Claim 13 (depends on 12)

The manufacturing method of claim 12, wherein,
in the step S101, a deposition power for depositing the buffer layer film ranges from 6 kW to 20 kW, a deposition thickness ranges from 20 mm to 30 mm, a deposition pressure ranges from 600 mTorr to 1000 mTorr, a deposition gas is a mixed gas of SiH4, NH3 and N2, gas flow ratio among SiH4, NH3 and N2 ranges from 1:2.3:15.6 to 1:16:45, and a deposition temperature ranges from 230° C. to 300° C.;
in the step S102, the deposition power for depositing the bottom passivation layer film ranges from 6 kW to 18 kW, the deposition thickness ranges from 20 mm to 26 mm, the deposition pressure ranges from 1000 mTorr to 1500 mTorr, the deposition gas is a mixed gas of SiH4, NH3 and N2, gas flow ratio among SiH4, NH3 and N2 ranges from 1:2.5:7.5 to 1:3.2:9.0, and the deposition temperature ranges from 230° C. to 300° C.; and
in the step S103, the deposition power for depositing the top passivation layer film ranges from 6 kW to 15 kW, the deposition thickness ranges from 20 mm to 26 mm, the deposition pressure ranges from 1500 mTorr to 2000 mTorr, the deposition gas is a mixed gas of SiH4, NH3 and N2, gas flow ratio among SiH4, NH3 and N2 ranges from 1:2.5:7.5 to 1:3.2:9.0, and the deposition temperature ranges from 230° C. to 300° C.

### Claim 14 (depends on 10)

The manufacturing method of claim 10, further comprises:
step S13′, forming a second transparent electrode on the glass substrate subjected to the step S12′.

### Claim 15 (depends on 14)

The manufacturing method of claim 14, wherein the first transparent electrode is a pixel electrode and the second transparent electrode is a common electrode, or, the first transparent electrode is a common electrode and the second transparent electrode is a pixel electrode.

### Claim 16 (depends on 1)

The manufacturing method of claim 1, wherein a temperature for the pre-heating process ranges from 230° C. to 300° C., and a duration of the pre-heating process ranges from 15 seconds to 25 seconds.

### Claim 17 (depends on 1)

The manufacturing method of claim 1, wherein the thin film transistor comprises an active layer, and the active layer is made of amorphous silicon material, low temperature polycrystalline silicon material or transparent metal oxide material.

### Claim 18 (depends on 1)

The manufacturing method of claim 1, wherein the thin film transistor is of a top gate type or a bottom gate type.

### Claim 19 (depends on 1)

An array substrate which is manufactured by the manufacturing method of claim 1.

### Claim 20 (depends on 19)

A display apparatus, comprising the array substrate of claim 19.