# US 2016/0254209 A1 · Power-module substrate with heat-sink and manufacturing method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0254209 A1
- Document ID: US20160254209A1
- Status: Published application
- Kind: A1
- Application number: 15/028,173
- Filed: 2014-10-08
- Published: 2016-09-01
- Earliest claimed: 2013-10-10
- Assignees: Mitsubishi Materials Corporation
- Applicants: Mitsubishi Materials Corporation
- Inventors: Tomoya Oohiraki; Sotaro Oi
- Web page: https://patentgrep.com/patent/US20160254209A1

## CPC

- H10W 70/027: {Mechanical treatments, e.g. deforming, punching or cutting}
- H10W 40/037: {Assembling together parts thereof}
- H10W 40/10: Arrangements for heating
- H10W 40/22: characterised by their shape, e.g. having conical or cylindrical projections
- H10W 40/255: {having a laminate or multilayered structure, e.g. direct bond copper [DBC] ceramic substrates}
- H10W 40/258: {Metallic materials (H10W40/254, H10W40/257, H10W40/255, H10W40/251, H10W40/253 take precedence)}
- H10W 40/47: by flowing liquids, e.g. forced water cooling
- H10W 70/02: of conductive package substrates serving as an interconnection, e.g. of metal plates (manufacture or treatment of leadframes H10W70/04)
- H10W 70/60: Insulating or insulated package substrates; Interposers; Redistribution layers (leadframes H10W70/40)
- H10W 72/071: {Connecting or disconnecting}
- H10W 70/692: Ceramics or glasses
- H10W 90/734: {between a chip and a stacked insulating package substrate, interposer or RDL}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A maximum length of a heat sink is set as “L” and a warp amount of the heat sink is set as “Z”; the warp amount “Z” is set as a positive value if a bonded surface of the heat sink to a metal layer is deformed to be concave or the warp amount “Z” is set as a negative value if the bonded surface is deformed to be convex; a ratio Z/L of the maximum length “L” and the warp amount “Z” measured at 25° C. is in a range not smaller than −0.005 and not larger than 0.005, and the ratio Z/L is in the range not smaller than −0.005 and not larger than 0.005 even when it is heated to 280° C. and then cooled to 25° C.

## Claims

### Claim 1

A power-module substrate with heat-sink comprising:
a power-module substrate provided with a ceramic substrate, a circuit layer provided on one surface of the ceramic substrate, and a metal layer made of aluminum of purity not lower than 99% provided on another surface of the ceramic substrate; and
a heat sink made of aluminum alloy having a larger yield stress than that of the metal layer and bonded on the metal layer of the power-module substrate, wherein
a maximum length of the heat sink is set as “L” and a warp amount of the heat sink is set as “Z”;
the warp amount “Z” is set as a positive value if a bonded surface of the heat sink on the metal layer is deformed to be concave; or is set as a negative value if the bonded surface is deformed to be convex;
a ratio Z/L of the maximum length “L” and the warp amount “Z” measured at 25° C. is in a range not smaller than −0.005 and not larger than 0.005, and
the ratio Z/L is in the range not smaller than −0.005 and not larger than 0.005 even when it is heated to 280° C. and then cooled to 25° C.

### Claim 2 (depends on 1)

The power-module substrate with heat-sink according to claim 1, wherein a difference ΔZ/L between a maximum value and a minimum value of the ratio Z/L when the temperature is varied from 25° C. to 280° C. is not larger than 0.005.

### Claim 3 (depends on 1)

A manufacturing method of the power-module substrate with heat-sink according claim 1, comprising:
laminating the power-module substrate and the heat sink;
heating in a state in which the bonded surface of the heat sink is deformed to concavely warp; and
cooling in a deformed state so as to bond the metal layer of the power-module substrate and the heat sink.

### Claim 4

A power-module substrate with heat-sink comprising:
a power-module substrate provided with a ceramic substrate, a circuit layer provided on one surface of the ceramic substrate, and a metal layer made of aluminum of purity not lower than 99% provided on another surface of the ceramic substrate; and
a heat sink made of copper or copper alloy having linear-expansion coefficient not smaller than 15×10−6/K and not larger than 22×10−6/K and bonded on the metal layer of the power-module substrate, wherein
a maximum length of the heat sink is set as “L” and a warp amount of the heat sink is set as “Z”;
the warp amount “Z” is set as a positive value if a bonded surface of the heat sink on the metal layer is deformed to be concave; or is set as a negative value if the bonded surface is deformed to be convex;
a ratio Z/L of the maximum length “L” and the warp amount “Z” measured at 25° C. is in a range not smaller than −0.015 or not larger than 0.01,
the ratio Z/L is in the range not smaller than −0.015 or not larger than 0.01 even if it is heated to 280° C. and then cooled to 25° C.

### Claim 5 (depends on 4)

The power-module substrate with heat-sink according to claim 4, wherein a difference ΔZ/L between a maximum value and a minimum value of the ratio Z/L when the temperature is varied from 25° C. to 280° C. is not larger than 0.015.

### Claim 6 (depends on 4)

A manufacturing method of the power-module substrate with heat-sink according claim 4, comprising:
laminating the power-module substrate and the heat sink;
heating in a state in which the bonded surface of the heat sink is deformed to concavely warp; and
cooling in a deformed state so as to bond the power-module substrate and the sink.

### Claim 7

A power-module substrate with heat sink comprising:
a power-module substrate including a ceramic substrate, a circuit layer provided on one surface of the ceramic substrate, and a metal layer made of aluminum of purity not lower than 99% provided on another surface of the ceramic substrate; and
a heat sink made of material having linear-expansion coefficient of not smaller than 7×10−6/K and not larger than 12×10−6/K and bonded on the metal layer of the power-module substrate, wherein
a maximum length of the heat sink is set as “L” and a warp amount of the heat sink is set as “Z”;
the warp amount “Z” is set as a positive value if a bonded surface of the heat sink on the metal layer is deformed to be concave; or is set as a negative value if the bonded surface is deformed to be convex;
a ratio Z/L of the maximum length “L” and the warp amount “Z” measured at 25° C. is in a range not smaller than −0.002 and not larger than 0.002, and
the ratio Z/L is in the range not smaller than −0.002 and not larger than 0.002 even when it is heated to 280° and then cooled to 25° C.

### Claim 8 (depends on 7)

The power-module substrate with heat-sink according to claim 7, wherein the heat sink is made from AlSiC matrix composite material, Al graphite composite material, Cu—W alloy, or Cu—Mo alloy.

### Claim 9 (depends on 7)

The power-module substrate with heat-sink according to claim 7, wherein a difference ΔZ/L between a maximum value and a minimum value of the ratio Z/L when the temperature is varied from 25° C. to 280° C. is not larger than 0.002.

### Claim 10 (depends on 7)

A manufacturing method of the power-module substrate with heat-sink according claim 7, comprising:
laminating the power-module substrate and the heat sink;
heating in a state in which the bonded surface of the heat sink is deformed to concavely warp; and
cooling in a deformed state so as to bond power-module substrate and the heat sink.