# US 2016/0254181 A1 · Aluminum nitride barrier layer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0254181 A1
- Document ID: US20160254181A1
- Status: Published application
- Kind: A1
- Application number: 14/634,512
- Filed: 2015-02-27
- Published: 2016-09-01
- Earliest claimed: 2015-02-27
- Assignees: Applied Materials, Inc.
- Applicants: Applied Materials, Inc.
- Inventors: Deenesh Padhi; Srinivas Guggilla; Alexandros T. Demos; Bhaskar Kumar; He Ren; Priyanka Dash
- Web page: https://patentgrep.com/patent/US20160254181A1

## CPC

- H10W 20/088: {involving partial etching of via holes}
- H10P 14/3216: {Nitrides}
- H10W 20/0523: {by irradiating with ultraviolet or particle radiation}
- H10W 20/076: {in via holes or trenches}
- H10W 20/085: {involving intermediate temporary filling with material}
- H10W 20/47: comprising two or more dielectric layers having different properties, e.g. different dielectric constants
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A method of forming features in a dielectric layer is described. A via, trench or a dual-damascene structure may be present in the dielectric layer prior to depositing a conformal aluminum nitride layer. The conformal aluminum nitride layer is configured to serve as a barrier to prevent diffusion across the barrier. The methods of forming the aluminum nitride layer involve the alternating exposure to two precursor treatments (like ALD) to achieve high conformality. The high conformality of the aluminum nitride barrier layer enables the thickness to be reduced and the effective conductivity of the subsequent gapfill metal layer to be increased.

## Claims

### Claim 1

A method of forming a gap in a low-k dielectric layer, the method comprising:
forming a conformal barrier layer on a patterned substrate, wherein the patterned substrate comprises a gap above an underlying copper layer, wherein sidewalls of the gap comprise low-k dielectric material, wherein the conformal barrier layer is formed by:
exposing the patterned substrate to an aluminum-containing precursor and then,
exposing the patterned substrate to a nitrogen-and-hydrogen-containing precursor while concurrently exposing the patterned substrate to ultraviolet light; and
depositing a conductor into the gap.

### Claim 2 (depends on 1)

The method of claim 1 wherein the aluminum-containing precursor is an organometallic precursor.

### Claim 3 (depends on 1)

The method of claim 1 wherein the aluminum-containing precursor comprises comprise one or more of triethylaluminum or trimethylaluminum.

### Claim 4 (depends on 1)

The method of claim 1 wherein a width of the gap is less than 20 nm.

### Claim 5 (depends on 1)

The method of claim 1 wherein a dielectric constant of the low-k dielectric material is between 2.3 and 2.8 following formation of the conformal barrier layer.

### Claim 6

A method of forming a conformal aluminum nitride layer, the method comprising:
forming a conformal aluminum nitride layer on a patterned substrate placed in a substrate processing region by:
i) flowing an organoaluminum precursor into the substrate processing region;
ii) removing process effluents from substrate processing region;
iii) flowing a nitrogen-and-hydrogen-containing precursor into the substrate processing region while shining ultraviolet light onto the patterned substrate; and
(iv) removing process effluents from the substrate processing region.

### Claim 7 (depends on 6)

The method of claim 6 wherein operations i) through iv) occur in the recited order.

### Claim 8 (depends on 6)

The method of claim 6 wherein the conformal aluminum nitride layer is configured to prevent diffusion of copper across the conformal aluminum nitride layer.

### Claim 9 (depends on 6)

The method of claim 6 wherein the conformal aluminum nitride layer consists of aluminum and nitrogen.

### Claim 10 (depends on 6)

The method of claim 6 wherein operations i) through iv) are repeated an integral number of times to form a conformal aluminum nitride layer.

### Claim 11 (depends on 10)

The method of claim 10 wherein a thickness of the conformal aluminum nitride layer is less than 6 nm.

### Claim 12 (depends on 6)

The method of claim 6 further comprising an operation of depositing gapfill metal into the via and the trench following operation iv).

### Claim 13

A method of forming a dual-damascene structure, the method comprising:
forming a conformal silicon carbon nitride layer over a patterned substrate, wherein the patterned substrate comprises a trench and a via below the trench, wherein the via is above an underlying copper layer, wherein sidewalls of the trench and the via comprise low-k dielectric walls, and wherein the trench is fluidly coupled to the via and the conformal silicon carbon nitride layer forms a hermetic seal between the trench and the low-k dielectric walls;
selectively removing a bottom portion of the conformal silicon carbon nitride layer from the underlying copper layer while retaining a side portion of the conformal silicon carbon nitride layer on the low-k dielectric walls;
placing the patterned substrate in a substrate processing region;
i) flowing an aluminum-containing precursor into the substrate processing region
ii) removing process effluents from substrate processing region;
iii) flowing a nitrogen-and-hydrogen-containing precursor into the substrate processing region while shining ultraviolet light onto the dual-damascene structure of the patterned substrate; and
iv) removing process effluents from the substrate processing region.

### Claim 14 (depends on 13)

The method of claim 13 wherein the operation of selectively removing the conformal silicon carbon nitride layer comprises dry-etching the conformal silicon carbon nitride layer.

### Claim 15 (depends on 13)

The method of claim 13 wherein a width of the trench is less than 70 nm.