# US 2016/0254157 A1 · Metal Gate Stack Having TaAlCN Layer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0254157 A1
- Document ID: US20160254157A1
- Status: Published application
- Kind: A1
- Application number: 15/149,978
- Filed: 2016-05-09
- Published: 2016-09-01
- Earliest claimed: 2011-09-24
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Applicants: Taiwan Semiconductor Manufacturing Company, Ltd.
- Inventors: SHIU-KO JANGJIAN; TING-CHUN WANG; CHI-CHERNG JENG; CHI-WEN LIU
- Web page: https://patentgrep.com/patent/US20160254157A1

## CPC

- H10D 64/01318: {the conductor comprising a layer of alloy material, compound material or organic material contacting the insulator, e.g. TiN (comprising a layer of alloys of Si, Ge or C H10D64/01314)}
- H10D 30/797: {being in source or drain regions, e.g. SiGe source or drain}
- H10D 62/021: {Forming source or drain recesses by etching e.g. recessing by etching and then refilling}
- H10D 62/151: {of IGFETs (of IGFETs having LDD or DDD structure H10D30/601; of thin film transistors H10D30/6713)}
- H10D 62/822: comprising only Group IV materials heterojunctions, e.g. Si/Ge heterojunctions
- H10D 62/832: being Group IV materials comprising two or more elements, e.g. SiGe
- H10D 62/8325: {Silicon carbide}
- H10D 64/017: {using dummy gates in processes wherein at least parts of the final gates are self-aligned to the dummy gates, i.e. replacement gate processes}
- H10D 64/666: {the conductor further comprising additional layers}
- H10D 64/667: {the conductor comprising a layer of alloy material, compound material or organic material contacting the insulator, e.g. TiN workfunction layers (having lateral variation H10D64/671)}
- H10D 64/669: {the conductor further comprising additional layers of alloy material, compound material or organic material, e.g. TaN/TiAlN}
- H10D 84/014: {the gate conductors having different materials or different implants}
- H10D 84/038: {using silicon technology, e.g. SiGe}
- H10D 84/83: of only insulated-gate FETs [IGFET]
- H10P 14/69393: {the material containing tantalum, e.g. Ta2O5}
- H10D 64/685: {being perpendicular to the channel plane}
- H10D 64/691: {comprising metallic compounds, e.g. metal oxides or metal silicates (insulators comprising nitrogen H10D64/693)}
- H10D 64/693: {the insulator comprising nitrogen, e.g. nitrides, oxynitrides or nitrogen-doped materials}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A method includes forming a gate stack over a semiconductor substrate; forming an interlayer dielectric layer surrounding the gate stack; and at least partially removing the gate stack, thereby forming an opening. The method further includes forming a multi-function wetting/blocking layer in the opening, a work function layer over the multi-function blocking/wetting layer, and a conductive layer over the work function layer. The work function layer, the multi-function wetting/blocking layer, and the conductive layer fill the opening. The multi-function wetting/blocking layer includes aluminum, carbon, nitride, and one of: titanium and tantalum.

## Claims

### Claim 1

A method comprising:
forming a gate stack over a semiconductor substrate;
forming an interlayer dielectric layer surrounding the gate stack;
at least partially removing the gate stack, thereby forming an opening; and
forming a multi-function wetting/blocking layer in the opening, a work function layer over the multi-function blocking/wetting layer, and a conductive layer over the work function layer, wherein the work function layer, the multi-function wetting/blocking layer, and the conductive layer fill the opening, and further wherein the multi-function wetting/blocking layer includes aluminum, carbon, nitride, and one of: titanium and tantalum.

### Claim 2 (depends on 1)

The method of claim 1, wherein the multi-function wetting/blocking layer has a nitrogen atomic concentration ranging from 5% to 15%, and a carbon atomic concentration ranging from 5% to 20%.

### Claim 3 (depends on 2)

The method of claim 2, wherein the multi-function wetting/blocking layer includes titanium and has a Ti:Al ratio ranging from 1:1 to 1:3.

### Claim 4 (depends on 2)

The method of claim 2, wherein the multi-function wetting/blocking layer includes tantalum and has a Ta:Al ratio ranging from 1:1 to 1:3.

### Claim 5 (depends on 1)

The method of claim 1, wherein the work function layer also includes aluminum, carbon, nitride, and the one of: titanium and tantalum.

### Claim 6 (depends on 5)

The method of claim 5, wherein the work function layer has a nitrogen atomic concentration ranging from 2% to 5%.

### Claim 7 (depends on 1)

The method of claim 1, wherein the multi-function wetting/blocking layer is formed over a high-k dielectric layer in the opening.

### Claim 8 (depends on 1)

The method of claim 1, wherein the multi-function blocking/wetting layer includes aluminum, carbon, nitride, and titanium, and the forming of the multi-function wetting/blocking layer includes performing a physical vapor deposition process.

### Claim 9 (depends on 1)

The method of claim 1, wherein the multi-function blocking/wetting layer includes aluminum, carbon, nitride, and tantalum, and the forming of the multi-function blocking/wetting layer includes performing an atomic layer deposition process.

### Claim 10

A method comprising:
forming a gate structure over a semiconductor substrate;
forming an interlayer dielectric layer surrounding the gate stack;
at least partially removing the gate stack, thereby forming an opening; and
forming a multi-function blocking/wetting layer in the opening, a work function layer over the multi-function blocking/wetting layer, and a conductive layer over the work function layer, wherein the multi-function blocking/wetting layer, the work function layer, and the conductive layer fill the opening, and further wherein the multi-function blocking/wetting layer comprises titanium aluminum carbon nitride (TiAlCN).

### Claim 11 (depends on 10)

The method of claim 10, wherein the forming of the multi-function blocking/wetting layer includes performing a physical vapor deposition process.

### Claim 12 (depends on 10)

The method of claim 10, wherein the forming of the multi-function blocking/wetting layer includes forming the multi-function blocking/wetting layer having a nitrogen atomic concentration ranging from 5% to 15% and a carbon atomic concentration ranging from 5% to 20%.

### Claim 13 (depends on 12)

The method of claim 12, wherein the forming of the multi-function blocking/wetting layer further includes forming the multi-function blocking/wetting layer having a Ti:Al ratio ranging from 1:1 to 1:3.

### Claim 14 (depends on 10)

The method of claim 10, wherein the work function layer comprises TiAlCN.

### Claim 15 (depends on 14)

The method of claim 14, wherein the TiAlCN in the work function layer has a nitrogen atomic concentration ranging from 2% to 5%.

### Claim 16

A method comprising:
forming a gate stack over a semiconductor substrate;
forming an interlayer dielectric layer surrounding the gate stack;
at least partially removing the gate stack, thereby forming an opening; and
forming a multi-function blocking/wetting layer in the opening, a work function layer over the multi-function blocking/wetting layer, and a conductive layer over the work function layer, wherein the multi-function blocking/wetting layer, the work function layer, and the conductive layer fill the opening, and further wherein the multi-function blocking/wetting layer includes a first tantalum aluminum carbon nitride (TaAlCN) layer.

### Claim 17 (depends on 16)

The method of claim 16, wherein the forming of the multi-function blocking/wetting layer includes performing an atomic layer deposition process.

### Claim 18 (depends on 16)

The method of claim 16, wherein the forming of the multi-function blocking/wetting layer includes forming the first TaAlCN layer having a nitrogen atomic concentration ranging from 5% to 15%, and a carbon atomic concentration ranging from 5% to 20%.

### Claim 19 (depends on 18)

The method of claim 18, wherein the forming of the multi-function blocking/wetting layer further includes forming the first TaAlCN layer having a Ta:Al ratio ranging from 1:1 to 1:3.

### Claim 20 (depends on 16)

The method of claim 16, wherein the forming of the work function layer includes forming a second TaAlCN layer having a nitrogen atomic concentration ranging from 2% to 5%.