# US 2016/0254146 A1 · Methods and structures for preparing single crystal silicon wafers for use as substrates for epitaxial growth of crack-free gallium nitride films and devices

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0254146 A1
- Document ID: US20160254146A1
- Status: Published application
- Kind: A1
- Application number: 15/149,190
- Filed: 2016-05-09
- Published: 2016-09-01
- Earliest claimed: 2014-04-13
- Inventors: Ananda H. Kumar
- Web page: https://patentgrep.com/patent/US20160254146A1

## CPC

- H10P 14/6342: {Liquid deposition, e.g. spin-coating, sol-gel techniques or spray coating}
- H10D 62/405: {Orientations of crystalline planes}
- H10D 62/8503: {Nitride Group III-V materials, e.g. AlN or GaN}
- H10P 14/2905: {Silicon, silicon germanium or germanium}
- H10P 14/2926: {Crystal orientations}
- H10P 14/3238: {being insulating materials}
- H10P 14/3258: {Crystal orientation}
- H10P 14/3416: {Nitrides}
- H10P 14/36: {characterised by treatments done before the formation of the materials}
- H10P 90/00: Preparation of wafers not covered by a single main group of this subclass, e.g. wafer reinforcement
- H10P 90/1904: {Preparing vertically inhomogeneous wafers}
- H10H 20/01335: {the light-emitting regions comprising nitride materials}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10H: INORGANIC LIGHT-EMITTING SEMICONDUCTOR DEVICES HAVING POTENTIAL BARRIERS

## Abstract

This document describes the fabrication and use of ceramic stabilizing layer fabricated right on the product silicon wafer to facilitate its use as a substrate for fabrication of gallium nitride films. A ceramic layer is formed and then attached to a single crystal silicon substrate to form a composite silicon substrate that has coefficient of thermal expansion comparable with GaN. The composite silicon substrates prepared by this invention are uniquely suited for use as growth substrates for crack-free gallium nitride films, benefitting from compressive stresses produced by choosing a ceramic having a desired higher coefficient thermal expansion than those of silicon and gallium nitride.

## Claims

### Claim 1

A method comprising
providing a single crystal silicon substrate,
wherein the silicon substrate comprises a first side and a second side;
applying a paste on the first side of the silicon substrate;
sintering the paste to solidify the paste,
wherein the solidified paste has coefficient of thermal expansion (CTE) higher than that of silicon.

### Claim 2 (depends on 1)

A method as in claim 1 wherein the second side of the silicon substrate comprises a (111) crystallographic surface.

### Claim 3 (depends on 1)

A method as in claim 1 wherein the thickness of the silicon substrate is less than 50 microns.

### Claim 4 (depends on 1)

A method as in claim 1 further comprising
applying an adhesive to the first side of the silicon substrate before applying the paste.

### Claim 5 (depends on 1)

A method as in claim 1 the paste comprises a refractory metal, ceramic, a powder of ceramic, glass, metal, or a mixture thereof.

### Claim 6 (depends on 1)

A method as in claim 1 wherein the paste comprises an adhesive additive.

### Claim 7 (depends on 1)

A method as in claim 1 wherein the sintering process is between 850 and 950 C.

### Claim 8 (depends on 1)

A method as in claim 1 wherein the sintering process is between 800 and 1200 C.

### Claim 9 (depends on 1)

A method as in claim 1 wherein the silicon substrate and the solidified paste form a composite substrate, and wherein the effective CTE of the composite substrate is higher than that of GaN.

### Claim 10

A method comprising
providing a single crystal silicon substrate,
wherein the silicon substrate comprises a first side and a second side;
placing the silicon substrate in a deposition chamber;
depositing a layer on the first side of the silicon substrate in vacuum,
wherein the layer has coefficient of thermal expansion (CTE) higher than that of silicon.

### Claim 11 (depends on 10)

A method as in claim 10 the layer comprises a refractory metal, ceramic, glass, metal, or a mixture thereof.

### Claim 12 (depends on 10)

A method as in claim 10 wherein the silicon substrate and the deposited layer form a composite substrate, and wherein the effective CTE of the composite substrate is higher than that of GaN.

### Claim 13

A method comprising
providing a single crystal silicon substrate,
wherein the silicon substrate comprises a first side and a second side;
applying a slurry on the first side of the silicon substrate;
sintering the slurry to solidify the slurry,
wherein the solidified slurry has coefficient of thermal expansion (CTE) higher than that of silicon.

### Claim 14 (depends on 13)

A method as in claim 13 wherein the thickness of the silicon substrate is less than 50 microns.

### Claim 15 (depends on 13)

A method as in claim 13 further comprising
applying an adhesive to the first side of the silicon substrate before applying the slurry.

### Claim 16 (depends on 13)

A method as in claim 13 the paste comprises a refractory metal, ceramic, a powder of ceramic, glass, metal, or a mixture thereof.

### Claim 17 (depends on 13)

A method as in claim 13 wherein the slurry comprises an adhesive additive.

### Claim 18 (depends on 13)

A method as in claim 13 wherein the sintering process is between 850 and 950 C.

### Claim 19 (depends on 13)

A method as in claim 13 wherein the sintering process is between 800 and 1200 C.

### Claim 20 (depends on 13)

A method as in claim 13 wherein the silicon substrate and the solidified slurry form a composite substrate, and wherein the effective CTE of the composite substrate is higher than that of GaN.