# US 2016/0254145 A1 · Methods for fabricating semiconductor structure with condensed silicon germanium layer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0254145 A1
- Document ID: US20160254145A1
- Status: Published application
- Kind: A1
- Application number: 14/633,246
- Filed: 2015-02-27
- Published: 2016-09-01
- Earliest claimed: 2015-02-27
- Assignees: Globalfoundries Inc.
- Applicants: Globalfoundries Inc.
- Inventors: Dina H. TRIYOSO; Wei Hua TONG; Haoran SHI; Jeremy Austin WAHL; Amy Lynn CHILD
- Web page: https://patentgrep.com/patent/US20160254145A1

## CPC

- H10P 14/6308: {of Group IV semiconductors}
- H10D 84/0167: {Manufacturing their channels}
- H10D 84/038: {using silicon technology, e.g. SiGe}
- H10P 14/6322: {Formation by thermal treatments (formation by plasma treatment H10P14/6319)}
- H10D 62/822: comprising only Group IV materials heterojunctions, e.g. Si/Ge heterojunctions
- H10D 86/01: Manufacture or treatment
- H10P 10/00: Bonding of wafers, substrates or parts of devices
- H10P 14/24: using chemical vapour deposition [CVD]
- H10P 14/3411: {Silicon, silicon germanium or germanium}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

Methods of forming condensed first layer and semiconductor structures formed from the methods are provided. The methods include, for instance providing at least one layer disposed over a substrate structure of a semiconductor structure, wherein the substrate structure includes an upper silicon region; and performing at least one oxidation process of the semiconductor structure, the at least one oxidation process reducing a thickness of the upper region, wherein the performing facilitates diffusing to form a condensed layer over the substrate structure.

## Claims

### Claim 1

A method comprising:
providing at least one layer disposed over a substrate structure of a semiconductor structure, wherein the substrate structure includes an upper silicon region; and
performing at least one oxidation process of the semiconductor structure, the at least one oxidation process reducing a thickness of the upper silicon region, wherein the performing facilitates diffusing to form a condensed layer over the substrate structure.

### Claim 2 (depends on 1)

The method of claim 1, wherein the performing comprises performing at least one oxidation process to at least partially oxidize the at least one layer forming an oxide layer and at least one atomic species, the at least one atomic species diffusing to form the condensed layer.

### Claim 3 (depends on 2)

The method of claim 2, wherein the diffusing of the at least one atomic species consumes the upper silicon region.

### Claim 4 (depends on 3)

The method of claim 3, wherein the upper silicon region of the substrate structure has a reduced thickness within a range of about 1 to 3 nm.

### Claim 5 (depends on 1)

The method of claim 1, wherein the at least one layer comprises a silicon germanium layer, and a protective layer disposed over the silicon germanium layer, and the performing comprises performing an in-situ steam growth process to selectively oxidize the protective layer forming an oxide layer.

### Claim 6 (depends on 5)

The method of claim 5, wherein the in-situ steam growth process is performed at a temperature within a range of about 950 to 1100° C.

### Claim 7 (depends on 5)

The method of claim 5, wherein the performing comprises performing a rapid thermal oxidation (RTO) process to at least partially oxidize the silicon germanium layer forming an oxide layer and at least one atomic species, the at least one atomic species diffusing into the upper silicon region to form the condensed layer over the substrate structure.

### Claim 8 (depends on 7)

The method of claim 7, wherein the rapid thermal oxidation (RTO) process is performed at a temperature within a range of about 950 to 1100° C.

### Claim 9 (depends on 1)

The method of claim 1, wherein the at least one layer comprises a silicon germanium layer, and the performing comprises performing an in-situ steam growth process to at least partially oxidize the at least one layer to form an oxide layer and at least one atomic species, the at least one atomic species diffusing into the upper silicon region to form the condensed layer over the substrate structure

### Claim 10 (depends on 1)

The method of claim 1, wherein the at least one oxidation process is controlled to reduce the thickness of the upper silicon region.

### Claim 11 (depends on 1)

The method of claim 1, wherein the at least one oxidation process induces an intrinsic strain within the condensed layer disposed over the substrate structure.

### Claim 12 (depends on 1)

The method of claim 1, wherein the substrate structure comprises a first region and a second region, the first region including the at least one layer disposed over the substrate structure, and the providing comprises providing a capping layer over the upper silicon region of the substrate structure in the second region.

### Claim 13 (depends on 12)

The method of claim 12, wherein the performing comprises performing the at least one oxidation process in the first region, wherein the capping layer inhibits oxidizing of the upper silicon region of the substrate structure in the second region during the at least one oxidation process.

### Claim 14 (depends on 12)

The method of claim 12, wherein the capping layer comprises at least one of an oxide material, an oxy nitride material or a nitride material.

### Claim 15 (depends on 14)

The method of claim 14, wherein the capping layer comprises an oxide material, and the providing comprises performing a nitridation process selectively over the capping layer in the second region, the nitridation process forming at least one of an oxynitrided region within an upper portion of the capping layer or a layer of nitride material over the capping layer.

### Claim 16 (depends on 1)

The method of claim 1, wherein the at least one oxidation process comprises a first oxidation process, and a second oxidation process, and wherein the at least one oxidation process occurs within a common oxidizing chamber.

### Claim 17 (depends on 1)

The method of claim 1, wherein the at least one layer comprises at least one of a silicon material or a silicon germanium material, the silicon germanium material having a germanium content of about 15 to 40%, and wherein the condensed layer comprises a germanium-rich silicon germanium layer.

### Claim 18

A semiconductor structure comprising:
a substrate structure with an upper silicon region thereof, the substrate structure including a first region and a second region, wherein the upper silicon region has a first thickness in the first region and a second thickness in the second region, the second thickness being greater than the first thickness; and
a first layer disposed over the upper silicon region of the substrate structure, and a second layer disposed over the first layer.

### Claim 19 (depends on 18)

The semiconductor structure of claim 18, wherein the first layer is a condensed silicon germanium layer in the first region, and wherein the first layer is a silicon layer in the second region.

### Claim 20 (depends on 18)

The semiconductor structure of claim 18, wherein the first thickness is less than 3 nm, and the second thickness is within a range of about 3 to 9 nm.