# US 2016/0254143 A1 · Method of manufacturing semiconductor device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0254143 A1
- Document ID: US20160254143A1
- Status: Published application
- Kind: A1
- Application number: 15/053,481
- Filed: 2016-02-25
- Published: 2016-09-01
- Earliest claimed: 2015-02-27
- Assignees: Renesas Electronics Corporation
- Applicants: Renesas Electronics Corporation
- Inventors: Toshikazu HANAWA; Kazuhide FUKAYA
- Web page: https://patentgrep.com/patent/US20160254143A1

## CPC

- H10W 20/096: {by contacting with gases, liquids or plasmas}
- H10P 14/6342: {Liquid deposition, e.g. spin-coating, sol-gel techniques or spray coating}
- H10P 14/6514: {by exposure to a plasma}
- H10P 14/6532: {by exposure to a plasma}
- H10P 14/69215: {the material being a silicon oxide, e.g. SiO2}
- H10W 20/0633: {using subtractive patterning of the conductive members}
- H10W 20/071: {of dielectric parts thereof}
- H10W 20/092: {by smoothing the dielectric parts}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

To provide a semiconductor device having improved reliability. After formation of a first insulating film for an interlayer insulating film by spin coating, the surface of the first insulating film is subjected to a hydrophilicity improving treatment. A second insulating film for the interlayer insulating film is then formed on the first insulating film by spin coating. The interlayer insulating film is comprised of a stacked insulating film including the first insulating film and the second insulating film thereon. The interlayer insulating film therefore can have improved surface flatness.

## Claims

### Claim 1

A method of manufacturing a semiconductor device having a first interlayer insulating film formed over a semiconductor substrate, comprising the steps of:
(a) forming a first insulating film by spin coating;
(b) subjecting a surface of the first insulating film to a first treatment for improving hydrophilicity; and
(c) after the step (b), forming a second insulating film over the first insulating film by spin coating,
wherein the first interlayer insulating film has a stacked insulating film including the first insulating film and the second insulating film.

### Claim 2 (depends on 1)

The method of manufacturing a semiconductor device according to claim 1,
wherein the first treatment performed in the step (b) is an oxygen plasma treatment.

### Claim 3 (depends on 2)

The method of manufacturing a semiconductor device according to claim 2,
wherein the oxygen plasma treatment is performed at a temperature of 170° C. or less.

### Claim 4 (depends on 1)

The method of manufacturing a semiconductor device according to claim 1,
wherein the first treatment performed in the step (b) is a heat treatment in an ozone-containing atmosphere.

### Claim 5 (depends on 1)

The method of manufacturing a semiconductor device according to claim 1,
wherein the following formula: T1≧T2 is satisfied, where T1 represents a thickness of the first insulating film formed in the step (a) and T2 represents a thickness of the second insulating film formed in the step (c).

### Claim 6 (depends on 1)

The method of manufacturing a semiconductor device according to claim 1,
wherein the first insulating film and the second insulating film include the same material.

### Claim 7 (depends on 6)

The method of manufacturing a semiconductor device according to claim 6,
wherein the first insulating film and the second insulating film each include silicon oxide.

### Claim 8 (depends on 1)

The method of manufacturing a semiconductor device according to claim 1,
wherein after a plurality of cycles of the step (a) and the step (b), the step (c) is performed.

### Claim 9 (depends on 1)

The method of manufacturing a semiconductor device according to claim 1, further comprising, before the step (a), a step of:
(a1) forming a third insulating film by CVD,
wherein in the step (a), the first insulating film is formed over the third insulating film by spin coating, and
wherein the first interlayer insulating film has a stacked insulating film including the third insulating film, the first insulating film, and the second insulating film.

### Claim 10 (depends on 1)

The method of manufacturing a semiconductor device according to claim 1,
wherein by the first treatment performed in the step (b), the first insulating film has improved wettability with a chemical solution to be used for the formation of the second insulating film in the step (c).

### Claim 11 (depends on 1)

The method of manufacturing a semiconductor device according to claim 1, further comprising, before the step (a), a step of:
(a2) providing the semiconductor substrate having, over the main surface thereof, a second interlayer insulating film and a wiring over the second interlayer insulating film,
wherein the first interlayer insulating film is formed over the second interlayer insulating film so as to cover the wiring.

### Claim 12 (depends on 11)

The method of manufacturing a semiconductor device according to claim 11,
wherein the wiring is an aluminum wiring.

### Claim 13 (depends on 1)

The method of manufacturing a semiconductor device according to claim 1, further comprising, before the step (a), a step of:
(a3) providing the semiconductor substrate having, over the main surface thereof, a gate electrode,
wherein the first interlayer insulating film is formed over the semiconductor substrate so as to cover the gate electrode.

### Claim 14

A method of manufacturing a semiconductor device having a first interlayer insulating film formed over a semiconductor substrate thereof, comprising the steps of:
(a) forming a first insulating film by spin coating;
(b) subjecting the surface of the first insulating film to an oxygen plasma treatment; and
(c) after the step (b), forming a second insulating film over the first insulating film by spin coating,
wherein the first interlayer insulating film includes a stacked insulating film having the first insulating film and the second insulating film.

### Claim 15 (depends on 14)

The method of manufacturing a semiconductor device according to claim 14,
wherein the temperature of the oxygen plasma treatment in the step (b) is 170° C. or less.