# US 2016/0252815 A1 · Photoresist with Floating-OOB-Absorption Additive

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0252815 A1
- Document ID: US20160252815A1
- Status: Published application
- Kind: A1
- Application number: 14/632,603
- Filed: 2015-02-26
- Published: 2016-09-01
- Earliest claimed: 2015-02-26
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Applicants: Taiwan Semiconductor Manufacturing Company, Ltd.
- Inventors: Yu-Chung Su; Ching-Yu Chang
- Web page: https://patentgrep.com/patent/US20160252815A1

## CPC

- G03F 7/091: {characterised by antireflection means or light filtering or absorbing means, e.g. anti-halation, contrast enhancement}
- G03F 7/0046: {with perfluoro compounds, e.g. for dry lithography (G03F7/0048 takes precedence)}
- G03F 7/2039: {X-ray radiation}
- G03F 7/38: Treatment before imagewise removal, e.g. prebaking {(G03F7/265 takes precedence)}
- G03F: PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR; (phototypographic composing devices B41B; photosensitive materials or processes for photographic purposes G03C; electrophotography, sensitive layers or processes therefor G03G)

## Abstract

Methods and materials for making a semiconductor device are described. The method includes forming an out-of-bond-wavelength (OOB)-reduction photoresist over a substrate, forming a floating region adjacent to a top surface of the OOB-reduction photoresist. The floating region has a higher absorbance of the OOB wavelength than a bulk region of the OOB-reduction photoresist that is below the floating region. The method also includes exposing the OOB-reduction photoresist to a radiation beam, wherein an OOB radiation portion of the radiation beam is absorbed in the floating region.

## Claims

### Claim 1

A method comprising:
forming an out-of-extreme-ultraviolet-band (OOB)-reduction photoresist over a substrate, which includes forming a floating region adjacent to a top surface of the OOB-reduction photoresist, wherein the floating region has a higher absorbance of OOB wavelengths than a bulk region of the OOB-reduction photoresist that is below the floating region,
wherein the OOB-reduction photoresist includes an OOB-absorption agent bonded with a floating agent, the floating agent having at least an alkyl group that includes C2F5 or C3F7; and
exposing the OOB-reduction photoresist to a EUV radiation beam, wherein an OOB radiation portion of the EUV radiation beam is absorbed in the floating region.

### Claim 2

(canceled)

### Claim 3 (depends on 1)

The method of claim 1, wherein
the OOB-absorption agent floats up with the floating agent to the top surface of the OOB-reduction photoresist when it is applied over the substrate.

### Claim 4 (depends on 3)

The method of claim 3, wherein bonds between the OOB-absorption agent and the floating agent comprise a covalent bond, a hydrogen bond, or an ionic bond.

### Claim 5 (depends on 1)

The method of claim 1, wherein the forming of the floating region includes:
mixing the OOB-absorption agent with a solvent, wherein the OOB-absorption agent obtains a high volatile ability by having a high affinity to the solvent; and
the OOB-absorption agent floats up to form the floating region.

### Claim 6 (depends on 1)

The method of claim 1, wherein the OOB-absorption agent includes one or more aromatic structures.

### Claim 7 (depends on 1)

The method of claim 1, wherein the forming of the OOB-reduction photoresist over the substrate uses a spin-coating technique.

### Claim 8

(canceled)

### Claim 9 (depends on 1)

The method of claim 1, further comprising:
after exposing the OOB-reduction photoresist, baking the OOB-reduction photoresist; and
applying a developer to the OOB-reduction photoresist.

### Claim 10

A method comprising:
spin-coating an out-of-extreme-ultraviolet-band (OOB)-reduction extreme ultraviolet (EUV) photoresist over a substrate, wherein the OOB-reduction EUV photoresist includes an OOB-absorption agent bonded with a floating agent, the floating agent having at least an alkyl group that includes C2F5 or C3F7;
forming a floating region adjacent to a top surface of the OOB-reduction EUV photoresist, wherein the floating region has a higher absorbance of the OOB wavelengths than another region of the OOB-reduction EUV photoresist that is below the floating region;
exposing the OOB-reduction EUV photoresist to an EUV radiation beam, wherein an OOB radiation portion of the EUV radiation beam is absorbed in the floating region;
baking the OOB-reduction EUV photoresist; and
applying a developer to the OOB-reduction EUV photoresist.

### Claim 11

(canceled)

### Claim 12 (depends on 10)

The method of claim 10, wherein
the OOB-absorption agent floats up with the floating agent to the top surface of the OOB-reduction EUV photoresist when it is applied over the substrate.

### Claim 13 (depends on 12)

The method of claim 12, wherein bonds between the OOB-absorption agent and the floating agent comprise a covalent bond, a hydrogen bond, a chromophore bond, or an ionic bond.

### Claim 14 (depends on 10)

The method of claim 10, wherein the forming of the floating region includes:
mixing the OOB-absorption agent with a solvent, wherein the OOB-absorption agent obtains a high volatile ability by having a high affinity to the solvent; and
wherein the OOB-absorption agent floats up to form the floating region.

### Claim 15 (depends on 10)

The method of claim 10, wherein the OOB-absorption agent includes one or more aromatic structures.

### Claim 16 (depends on 10)

The method of claim 10, wherein the floating region is formed having a thickness, which is less than about 50% of a total thickness of the OOB-reduction EUV photoresist.

### Claim 17

A photoresist comprising:
a backbone polymer;
an acid labile group (ALG) bonded to the backbone polymer;
a photo acid generator (PAG);
a solvent;
a surfactant; and
an additive that includes a floating agent bonded with an out-of-extreme-ultraviolet-band(OOB)-absorption agent, wherein the OOB-absorption agent has a high absorbance of OOB wavelengths, wherein the OOB-absorption agent is capable to float up with the floating agent to a top surface of the photoresist when the photoresist is applied to a substrate, wherein the OOB-absorption agent includes one or more aromatic structures, and the floating agent includes at least an alkyl group, wherein the alkyl group includes C2F5 or C3F7.

### Claim 18

(canceled)

### Claim 19

(canceled)

### Claim 20 (depends on 17)

The photoresist of claim 17, wherein the OOB-absorption agent is bonded with the floating agent by a covalent bond, hydrogen bond, or ionic bond.

### Claim 21 (depends on 3)

The method of claim 3, wherein the OOB-absorption agent includes an aromatic structure.

### Claim 22 (depends on 6)

The method of claim 6, wherein the OOB-absorption agent and the floatable polymer include following structure:
wherein each of R and R1 is independently a hydrogen or an alkyl group having 1 to 8 carbon atom(s); R2 is an alkyl group having 1 to 10 carbon atom(s); R3 is a halogen, an alkyl group having 1 to 8 carbon atom(s), an alkoxy group having 1 to 8 carbon atom(s), an alkynyl group having 2 to about 8 carbon atom(s), a cyano group, or a nitro group; and m is an integer from 0 to 9.

### Claim 23

(canceled)

### Claim 24 (depends on 1)

The method of claim 1, wherein the floating region has a thickness less than a thickness of the bulk region.

### Claim 25 (depends on 10)

The method of claim 10, wherein the OOB-reduction EUV photoresist includes: a backbone polymer, an acid labile group (ALG) bonded to the backbone polymer, a photo acid generator (PAG), a solvent, and a surfactant.

### Claim 26 (depends on 1)

The method of claim 1, wherein the OOB wavelengths are within a range from about 200 nm to about 400 nm.