# US 2016/0252779 A1 · Optical alignment film, its manufacturing method, and liquid crystal display device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0252779 A1
- Document ID: US20160252779A1
- Status: Published application
- Kind: A1
- Application number: 14/436,793
- Filed: 2014-09-24
- Published: 2016-09-01
- Earliest claimed: 2014-05-30
- Assignees: Boe Technology Group Co., Ltd.; Beijing Boe Optoelectronics Technology Co., Ltd.
- Applicants: Boe Technology Group Co., Ltd.; Beijing Boe Optoelectronics Technology Co., Ltd.
- Inventors: Ang Xiao
- Web page: https://patentgrep.com/patent/US20160252779A1

## CPC

- G02F 1/133711: {by organic films, e.g. polymeric films}
- G02F 1/133788: {by light irradiation, e.g. linearly polarised light photo-polymerisation}
- B32B 2457/202: LCD, i.e. liquid crystal displays
- C09K 2323/02: Alignment layer characterised by chemical composition
- G02F: OPTICAL DEVICES OR ARRANGEMENTS FOR THE CONTROL OF LIGHT BY MODIFICATION OF THE OPTICAL PROPERTIES OF THE MEDIA OF THE ELEMENTS INVOLVED THEREIN; NON-LINEAR OPTICS; FREQUENCY-CHANGING OF LIGHT; OPTICAL LOGIC ELEMENTS; OPTICAL ANALOGUE/DIGITAL CONVERTERS
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE

## Abstract

The present disclosure relates to the field of liquid crystal display technology, and provides an optical alignment film, its manufacturing method, and a liquid crystal display device. The method includes steps of: forming an optical alignment thin film on a substrate; aligning the optical alignment thin film by irradiating the optical alignment thin film with a polarized light beam through a mask plate, the mask plate including a transparent region and a non-transparent region beyond the transparent region, the polarized light beam passing through the transparent region to irradiate the optical alignment thin film; and removing the optical alignment thin film corresponding to the non-transparent region, so as to obtain the patterned optical alignment film.

## Claims

### Claim 1

A method for manufacturing an optical alignment film, comprising steps of:
forming an optical alignment thin film on a substrate;
aligning the optical alignment thin film by irradiating the optical alignment thin film with a polarized light beam through a mask plate, the mask plate including a transparent region and a non-transparent region beyond the transparent region, the polarized light beam passing through the transparent region to irradiate the optical alignment thin film; and
removing the optical alignment thin film corresponding to the non-transparent region, so as to obtain the patterned optical alignment film.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the optical alignment thin film is aligned by photopolymerization when the polarized light beam passes through the transparent region.

### Claim 3 (depends on 2)

The method according to claim 2, wherein the polarized light beam is a UV polarized light beam and has an exposure dose of 500 to 2000 mJ/cm2.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the optical alignment thin film corresponding to the non-transparent region is removed by washing the substrate with water, acetone or isopropyl ketone.

### Claim 5 (depends on 1)

The method according to claim 1, wherein subsequent to the step of forming the optical alignment thin film on the substrate and prior to the step of aligning the optical alignment thin film by irradiating the optical alignment thin film with the polarized light beam through the mask plate, the method further comprises a step of subjecting the substrate to first heat treatment.

### Claim 6 (depends on 5)

The method according to claim 5, wherein the first heat treatment is performed at a temperature of 70° C. to 150° C.

### Claim 7 (depends on 5)

The method according to claim 5, wherein the first heat treatment is performed for 60 s to 120 s.

### Claim 8 (depends on 1)

The method according to claim 1, wherein subsequent to the step of aligning the optical alignment thin film by irradiating the optical alignment thin film with the polarized light beam through the mask plate, the method further comprises a step of subjecting the substrate to second heat treatment.

### Claim 9 (depends on 8)

The method according to claim 8, wherein the second heat treatment is performed at a temperature of 220° C. to 250° C.

### Claim 10 (depends on 8)

The method according to claim 8, wherein the second heat treatment is performed for more than 40 min.

### Claim 11 (depends on 1)

An optical alignment film manufactured by the method according to claim 1.

### Claim 12 (depends on 11)

The optical alignment film according to claim 11, wherein the optical alignment film is made of a photopolymerizable material.

### Claim 13 (depends on 12)

The optical alignment film according to claim 12, wherein the photopolymerizable material is a cinnamate compound.

### Claim 14 (depends on 11)

A liquid crystal display device comprising the optical alignment film according to claim 11.

### Claim 15 (depends on 14)

The liquid crystal display device according to claim 14, wherein the optical alignment film is made of a photopolymerizable material.

### Claim 16 (depends on 15)

The liquid crystal display device according to claim 15, wherein the photopolymerizable material is a cinnamate compound.

### Claim 17 (depends on 11)

The optical alignment film according to claim 11, wherein the optical alignment thin film is aligned by photopolymerization when the polarized light beam passes through the transparent region.

### Claim 18 (depends on 17)

The optical alignment film according to claim 17, wherein the polarized light beam is a UV polarized light beam and has an exposure dose of 500 to 2000 mJ/cm2.

### Claim 19 (depends on 11)

The optical alignment film according to claim 11, wherein subsequent to the step of forming the optical alignment thin film on the substrate and prior to the step of aligning the optical alignment thin film by irradiating the optical alignment thin film with the polarized light beam through the mask plate, the substrate is further subjected to first heat treatment.

### Claim 20 (depends on 11)

The optical alignment film according to claim 11, wherein subsequent to the step of aligning the optical alignment thin film by irradiating the optical alignment thin film with the polarized light beam through the mask plate, the substrate is further subjected to second heat treatment.