# US 2016/0252631 A1 · Scintillation crystal including a co-doped rare earth silicate, a radiation detection apparatus including the scintillation crystal, and a process of forming the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0252631 A1
- Document ID: US20160252631A1
- Status: Published application
- Kind: A1
- Application number: 15/046,703
- Filed: 2016-02-18
- Published: 2016-09-01
- Earliest claimed: 2015-02-26
- Assignees: Saint-Gobain Cristaux & Detecteurs
- Applicants: Saint-Gobain Cristaux & DéTecteurs
- Inventors: Samuel BLAHUTA; Vladimir OUSPENSKI
- Web page: https://patentgrep.com/patent/US20160252631A1

## CPC

- G01T 1/2023: {Selection of materials}
- C09K 11/7774: {Aluminates}
- C09K 11/77742: {Silicates}
- C30B 15/00: Single-crystal growth by pulling from a melt, e.g. Czochralski method (under a protective fluid C30B27/00)
- C30B 15/04: adding doping materials, e.g. for n-p-junction
- C30B 29/34: Silicates
- G01T 1/20183: {Arrangements for preventing or correcting crosstalk, e.g. optical or electrical arrangements for correcting crosstalk}
- G01T 1/20185: {Coupling means between the photodiode and the scintillator, e.g. optical couplings using adhesives with wavelength-shifting fibres}
- G01T 1/20189: {Damping or insulation against damage, e.g. caused by heat or pressure}
- G01T: MEASUREMENT OF NUCLEAR OR X-RADIATION (radiation analysis of materials, mass spectrometry G01N23/00; tubes for determining the presence, intensity, density or energy of radiation or particles H01J47/00)
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR

## Abstract

A scintillation crystal can include a rare earth silicate, an activator, and a Group 2 co-dopant. In an embodiment, the Group 2 co-dopant concentration may not exceed 200 ppm atomic in the crystal or 0.25 at % in the melt before the crystal is formed. The ratio of the Group 2 concentration/activator atomic concentration can be in a range of 0.4 to 2.5. In another embodiment, the scintillation crystal may have a decay time no greater than 40 ns, and in another embodiment, have the same or higher light output than another crystal having the same composition except without the Group 2 co-dopant. In a further embodiment, a boule can be grown to a diameter of at least 75 mm and have no spiral or very low spiral and no cracks. The scintillation crystal can be used in a radiation detection apparatus and be coupled to a photosensor.

## Claims

### Claim 1

A scintillation crystal comprising a rare earth silicate, a first dopant, and a second dopant, wherein:
the first dopant is an activator and has a first concentration;
the second dopant includes a Group 2 element and has a second concentration that does not exceed 200 ppm atomic based on a total rare earth content of the scintillation crystal; and
the second atomic concentration divided by the first atomic concentration is in a range of 0.4 to 2.0.

### Claim 2 (depends on 1)

The scintillation crystal of claim 1, wherein the scintillation crystal has a decay time no greater than 40 ns.

### Claim 3 (depends on 1)

The scintillation crystal of claim 1, wherein the scintillation crystal has a formula of Ln2SiO5:Ac,Me or Ln2Si2O7:Ac,Me, wherein:
Ln includes one or more rare earth elements different from the first dopant;
Ac is the first dopant; and
Me is the second dopant.

### Claim 4 (depends on 1)

The scintillation crystal of claim 1, wherein the second dopant is Ca and has a concentration in the scintillation crystal no greater than 160 atomic ppm based on a total rare earth content in the scintillation crystal.

### Claim 5 (depends on 1)

The scintillation crystal of claim 1, wherein the second dopant is Ca, and the second atomic concentration divided by the first atomic concentration in the scintillation crystal is in a range of 0.50 to 2.0.

### Claim 6 (depends on 1)

The scintillation crystal of claim 1, wherein the second dopant is Mg and has a concentration in the scintillation crystal no greater than 0.030 at % based on a total rare earth content in the scintillation crystal.

### Claim 7 (depends on 1)

The scintillation crystal of claim 1, wherein the second dopant is Mg, and the second atomic concentration divided by the first atomic concentration in the scintillation crystal is in a range of 0.35 to 2.5.

### Claim 8 (depends on 1)

The scintillation crystal of claim 1, wherein the first concentration is no greater than 1200 atomic ppm.

### Claim 9 (depends on 1)

The scintillation crystal of claim 1, wherein the first concentration is in a range of 20 atomic ppm to 1200 atomic ppm.

### Claim 10 (depends on 1)

A radiation detection apparatus comprising:
the scintillation crystal of claim 1; and
a photosensor optically coupled to the scintillation crystal.

### Claim 11

A scintillation crystal comprising a rare earth silicate, a first dopant, and a second dopant, wherein:
the first dopant is an activator and has a first concentration;
the second dopant includes a Group 2 element and has a second concentration that does not exceed 200 ppm atomic based on a total rare earth content of the scintillation crystal; and
the scintillation crystal has a decay time no greater than 40 ns.

### Claim 12

A process of forming a scintillation crystal comprising:
charging a crucible with an initial mass of a material for the scintillation crystal that includes a rare earth silicate, a first dopant, and a second dopant, wherein:
the first dopant is an activator and has a first concentration; and
the second dopant is a Group 2 element;
melting the charge to form a melt that includes a rare earth silicate, a first dopant, and a second dopant, wherein:
the first dopant has a first concentration in the melt;
the second dopant has a second concentration in the melt that does not exceed 0.25 at % based on a total rare earth content of the melt; and
the second atomic concentration divided by the first atomic concentration is in a range of 0.4 to 2.5;
growing a boule from the melt; and
cutting the boule to obtain a scintillation crystal.

### Claim 13 (depends on 12)

The process of claim 12, wherein growing the boule is performed such that the boule includes at least 45 wt % of the initial mass and has no spiral or very low spiral.

### Claim 14 (depends on 13)

The process of claim 13, wherein the scintillation crystal has a decay time no greater than 40 ns.

### Claim 15 (depends on 12)

The process of claim 12, wherein the boule has a diameter of at least 75 mm.

### Claim 16 (depends on 12)

The process of claim 12, wherein the second dopant is Ca and has a concentration in the melt no greater than 0.024 at % based on a total rare earth content of the melt.

### Claim 17 (depends on 12)

The process of claim 12, wherein the second dopant is Ca, and the second atomic concentration divided by the first atomic concentration in the melt is in a range of 0.50 to 2.5.

### Claim 18 (depends on 12)

The process of claim 12, wherein the second dopant is Mg and has a concentration in the melt no greater than 0.30 at % based on a total rare earth content of the melt.

### Claim 19 (depends on 12)

The process of claim 12, wherein the second dopant is Mg, and the second atomic concentration divided by the first atomic concentration in the melt is in a range of 0.50 to 2.5.

### Claim 20 (depends on 12)

The process of claim 12, wherein the scintillation crystal has a formula of Ln2SiO5:Ac,Me or Ln2Si2O7:Ac,Me, wherein:
Ln includes one or more rare earth elements different from the first dopant;
Ac is the first dopant; and
Me is the second dopant.