# US 2016/0252347 A1 · Film thickness sensor and manufacturing method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0252347 A1
- Document ID: US20160252347A1
- Status: Published application
- Kind: A1
- Application number: 14/769,293
- Filed: 2014-12-03
- Published: 2016-09-01
- Earliest claimed: 2014-09-18
- Assignees: Boe Technology Group Co., Ltd.; Ordos Yuansheng Optoelectronics Co., Ltd.
- Applicants: BOE Technology Group Co., Ltd.; Ordos Yuansheng Optoelectronics Co., Ltd.
- Inventors: Ang XIAO
- Web page: https://patentgrep.com/patent/US20160252347A1

## CPC

- G01B 21/08: for measuring thickness
- C23C 14/06: characterised by the coating material ({C23C14/0021} , C23C14/04 take precedence)
- C23C 14/18: on other inorganic substrates
- C23C 14/24: Vacuum evaporation
- C23C 14/546: {using crystal oscillators}
- C23C 14/5853: {Oxidation}
- G01B 1/00: Measuring instruments characterised by the selection of material therefor
- G01B: MEASURING LENGTH, THICKNESS OR SIMILAR LINEAR DIMENSIONS; MEASURING ANGLES; MEASURING AREAS; MEASURING IRREGULARITIES OF SURFACES OR CONTOURS
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

Disclosed is a film thickness sensor, Mg film or Mg/MgO film is coated on a surface of the film thickness sensor, so that Mg material is easy to attach to the film thickness sensor, and then the waste of Mg material is prevented.

## Claims

### Claim 1

A film thickness sensor, wherein Mg film or Mg/MgO film is coated on a surface of the film thickness sensor.

### Claim 2 (depends on 1)

The film thickness sensor according to claim 1, wherein a thickness of the Mg or Mg/MgO film is from 5 nm to 10 nm,

### Claim 3 (depends on 2)

The film thickness sensor according to claim 2, wherein the thickness of the Mg or Mg/MgO film is 8 nm.

### Claim 4 (depends on 1)

The film thickness sensor according to claim 1, wherein a thickness of MgO film in the Mg/MgO film is from 2 nm to 3 nm.

### Claim 5 (depends on 2)

The film thickness sensor according to claim 2, wherein a thickness ratio of Mg film and MgO film in the Mg/MgO film is 1: 0.25-1.5.

### Claim 6 (depends on 5)

The film thickness sensor according to claim 5, wherein the thickness of Mg/MgO film is 5 nm, the thickness ratio of Mg film and MgO film is 1: 0.67-1.5.

### Claim 7 (depends on 5)

The film thickness sensor according to claim 5, wherein the thickness of Mg/MgO film is 8 nm, the thickness ratio of Mg film and MgO film is 1: 0.3-0,6.

### Claim 8 (depends on 5)

The film thickness sensor according to claim 5, wherein the thickness of Mg/MgO film is 10 nm, the thickness ratio of Mg film and MgO film is 1: 0.25-0.45,

### Claim 9

A method for manufacturing a film thickness sensor, comprising:.
at a temperature of 600-700° C. and in an anaerobic condition of high vacuum, evaporating Mg material on the film thickness sensor to form Mg film thickness sensor; or
at a temperature of 600-700° C. and in an anaerobic condition of high vacuum, evaporating Mg material on the film thickness sensor to form Mg film thickness sensor;
exposing the Mg film thickness sensor to an oxygen-containing argon gas at a temperature of 30-45° C. for 60-70 seconds, oxidizing a surface of Mg film partially into MgO to form Mg/MgO film thickness sensor.

### Claim 10 (depends on 9)

The method according to claim 9, wherein a concentration of oxygen gas in the oxygen-containing argon gas is 5-6%.

### Claim 11 (depends on 3)

The film thickness sensor according to claim 3, wherein a thickness ratio of Mg film and MgO film in the Mg/MgO film is 1: 0.25-1.5.

### Claim 12 (depends on 4)

The film thickness sensor according to claim 4, wherein a thickness ratio of Mg film and MgO film in the Mg/MgO film is 1: 0.25-1.5.