# US 2016/0251789 A1 · Fibrous network structure having excellent compression durability

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0251789 A1
- Document ID: US20160251789A1
- Status: Published application
- Kind: A1
- Application number: 15/032,924
- Filed: 2014-10-28
- Published: 2016-09-01
- Earliest claimed: 2013-10-29
- Assignees: Toyobo Co., Ltd.
- Applicants: Toyobo Co., Ltd.
- Inventors: Teruyuki Taninaka; Shinichi Kobuchi; Hiroyuki Wakui
- Web page: https://patentgrep.com/patent/US20160251789A1

## CPC

- D04H 3/16: with bonds between thermoplastic filaments produced in association with filament formation, e.g. immediately following extrusion
- D04H 3/007: Addition polymers
- D04H 3/011: Polyesters
- D04H: MAKING TEXTILE FABRICS, e.g. FROM FIBRES OR FILAMENTARY MATERIAL (weaving D03; knitting D04B; braiding D04C; net-making D04G; sewing D05B; tufting D05C; finishing non-woven fabrics D06); FABRICS MADE BY SUCH PROCESSES OR APPARATUS, e.g. FELTS, NON-WOVEN FABRICS; COTTON-WOOL; WADDING {; NON-WOVEN FABRICS FROM STAPLE FIBRES, FILAMENTS OR YARNS, BONDED WITH AT LEAST ONE WEB-LIKE MATERIAL DURING THEIR CONSOLIDATION}(non-woven fabrics having an intermediate or external layer of a different kind, e.g. of woven fabric, B32B)

## Abstract

A network structure is disclosed including a three-dimensional random loop bonded structure obtained by forming random loops with curling treatment of a continuous linear structure including at least one thermoplastic elastomer selected from a polyester-based thermoplastic elastomer, a polyolefin-based thermoplastic elastomer, and an ethylene-vinyl acetate copolymer, and by making each loop mutually contact in a molten state, wherein a fiber diameter of the continuous linear structure is not less than 0.1 mm and not more than 3.0 mm, a fiber diameter of a surface layer portion of the network structure is not less than 1.05 times of a fiber diameter of an inner layer portion thereof, an apparent density is not less than 0.01 g/cm3 and not more than 0.20 g/cm3, 750 N-constant load repeated compression residual strain is not more than 15%, and 40%-compression hardness retention after 750 N-constant load repeated compression is not less than 55%.

## Claims

### Claim 1

A network structure comprising a three-dimensional random loop bonded structure obtained by forming random loops with curling treatment of a continuous linear structure including at least one thermoplastic elastomer selected from the group consisting of a polyester-based thermoplastic elastomer, a polyolefin-based thermoplastic elastomer, and an ethylene-vinyl acetate copolymer, and by making each loop mutually contact in a molten state, wherein
a fiber diameter of the continuous linear structure is not less than 0.1 mm and not more than 3.0 mm,
a fiber diameter of a surface layer portion of the network structure is not less than 1.05 times of a fiber diameter of an inner layer portion thereof,
an apparent density is not less than 0.01 g/cm3 and not more than 0.20 g/cm3,
750 N-constant load repeated compression residual strain is not more than 15%, and
40%-compression hardness retention after 750 N-constant load repeated compression is not less than 55%.

### Claim 2 (depends on 1)

The network structure according to claim 1, wherein 65%-compression hardness retention after 750 N-constant load repeated compression is not less than 70%.

### Claim 3 (depends on 1)

The network structure according to claim 1, wherein a compression-deflection coefficient is not less than 2.5.

### Claim 4 (depends on 1)

The network structure according to claim 1, wherein the network structure has a thickness of not less than 10 mm and not more than 300 mm.

### Claim 5 (depends on 1)

The network structure according to claim 1, wherein 40%-compression hardness retention after 750 N-constant load repeated compression is not less than 60%.

### Claim 6 (depends on 1)

The network structure according to claim 1, wherein 40%-compression hardness retention after 750 N-constant load repeated compression is not less than 65%.

### Claim 7 (depends on 1)

The network structure according to claim 1, wherein 65%-compression hardness retention after 750 N-constant load repeated compression is not less than 73%.