- Inventors: Kazumi TANABE; Takashi YOKOYAMA; Tegi KIM
- Web page: https://patentgrep.com/patent/US20160251774A1

## CPC

- C30B 15/20: Controlling or regulating (controlling or regulating in general G05)
- C30B 15/04: adding doping materials, e.g. for n-p-junction
- C30B 15/14: Heating of the melt or the crystallised materials
- C30B 27/02: by pulling from a melt
- C30B 29/06: Silicon
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR

## Abstract

There is provided a silicon single crystal producing method in producing a silicon single crystal by the Czochralski method using a pulling apparatus including a heat shield, wherein an oxygen concentration in the crystal is controlled through the adjustment of a flow velocity of inert gas introduced into the apparatus at the gap portion between an exterior surface of the single crystal and a lower-end opening edge of the heat shield, in accordance with a gap-to-crystal-diameter ratio (“the area of the gap portion”/“the area of a cross-sectional of the single crystal”). By this producing method, it is possible to appropriately control the oxygen concentration in the pulled single crystal.

## Claims

### Claim 1

A method for producing a silicon single crystal by the Czochralski method using a single crystal pulling apparatus in which a heat shield is disposed around a silicon single crystal, which is being pulled, so as to be concentric with a pulling axis, wherein
an oxygen concentration in the crystal is controlled through adjustment, in accordance with a gap-to-crystal-diameter ratio, of a flow velocity of inert gas introduced into the single crystal pulling apparatus at a gap portion between an exterior surface of the single crystal and a lower-end opening edge of the heat shield, the gap-to-crystal-diameter ratio being obtained by dividing an area of the gap portion by an area of a cross section perpendicular to the pulling axis of the single crystal.

### Claim 2 (depends on 1)

The silicon single crystal producing method according to claim 1, wherein
the oxygen concentration in the crystal is controlled through flow velocity adjustment of the inert gas, on the basis that
when the gap-to-crystal-diameter ratio is 0.27 to 0.45, an inert gas flow velocity at the gap portion between the single crystal and the heat shield, and the oxygen concentration in the crystal have a negative correlation, and
when the gap-to-crystal-diameter ratio is 0.72 to 0.92, the inert gas flow velocity at the gap portion and the oxygen concentration in the crystal have a positive correlation.

### Claim 3 (depends on 1)

The silicon single crystal producing method according to claim 1, wherein
when the single crystal is pulled,
the oxygen concentration in the crystal is controlled through adjustment of a flow velocity of inert gas at the gap portion performed in stages in the pulling on the basis of a relation between the inert gas flow velocity at the gap portion that is calculated in advance in accordance with the gap-to-crystal-diameter ratio, and the oxygen concentration in the crystal.

### Claim 4 (depends on 2)

The silicon single crystal producing method according to claim 2, wherein
the oxygen concentration in the crystal is controlled through adjustment of the flow velocity of inert gas introduced into the single crystal pulling apparatus in accordance with a diameter fluctuation of the crystal.

### Claim 5 (depends on 1)

The silicon single crystal producing method according to claim 1, wherein
the silicon single crystal to be grown has such a diameter that enables a silicon wafer having a diameter of 300 mm or more to be cut.

### Claim 6 (depends on 3)

The silicon single crystal producing method according to claim 3, wherein
the oxygen concentration in the crystal is controlled through adjustment of the flow velocity of inert gas introduced into the single crystal pulling apparatus in accordance with a diameter fluctuation of the crystal.