# US 2016/0251740 A1 · Method for recycling electrode materials of lithium ion batteries

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0251740 A1
- Document ID: US20160251740A1
- Status: Published application
- Kind: A1
- Application number: 15/054,075
- Filed: 2016-02-25
- Published: 2016-09-01
- Earliest claimed: 2015-02-28
- Assignees: Microvast Power Systems Co., Ltd.
- Applicants: Microvast Power Systems Co., Ltd.
- Inventors: RUI BI; XIAOPING ZHOU
- Web page: https://patentgrep.com/patent/US20160251740A1

## CPC

- B22F 8/00: Manufacture of articles from scrap or waste metal particles
- B22F 1/00: Metallic powder; Treatment of metallic powder, e.g. to facilitate working or to improve properties
- B22F 9/04: starting from solid material, e.g. by crushing, grinding or milling ({C22C1/1084 takes precedence}; crushing, grinding or milling, in general, see the relevant subclasses, e.g. B02C)
- H01M 10/54: Reclaiming serviceable parts of waste accumulators
- B22F 2009/001: {from scrap particles}
- B22F 2998/10: Processes characterised by the sequence of their steps
- Y02P 10/20: Recycling
- Y02W 30/50: Reuse, recycling or recovery technologies
- Y02W 30/84: Recycling of batteries or fuel cells
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS
- Y02W: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATER TREATMENT OR WASTE MANAGEMENT

## Abstract

A method for recycling electrode materials of lithium ion batteries, including the following steps: (1) disassembling the waste lithium ion battery to get positive electrode and negative electrode, immersing the positive electrode and/or the negative electrode into ammonia, then washing by deionized water and drying the positive electrode and/or the negative electrode; (2) sintering the dried positive electrode and/or the negative electrode, and using mechanical method to separate electrode powder material from current collector to get positive electrode powder material and/or negative electrode powder material; (3) supplementing lithium to the positive electrode powder material, then processing the positive electrode powder material by milling, spray drying and sintering to obtain regenerated positive electrode material; or processing the negative electrode powder material by milling, spray drying and sintering to obtain regenerated negative electrode material. The method has advantages of energy saving, simple operation, short processing time and less pollution.

## Claims

### Claim 1

A method for recycling electrode materials of lithium ion batteries, comprising:
(1) disassembling the waste lithium ion battery to get positive electrode and negative electrode, immersing the positive electrode and/or the negative electrode into ammonia, then washing by deionized water and drying the positive electrode and/or the negative electrode;
(2) sintering the dried positive electrode and/or the negative electrode, and using mechanical method to separate electrode powder material from current collector to get positive electrode powder material and/or negative electrode powder material; and
(3) supplementing lithium to the positive electrode powder material, then processing the positive electrode powder material by milling, spray drying and sintering to obtain regenerated positive electrode material; or processing the negative electrode powder material by milling, spray drying and sintering to obtain regenerated negative electrode material.

### Claim 2 (depends on 1)

The method for recycling electrode materials of lithium ion batteries according to claim 1, wherein a concentration of the ammonia in the step (1) is in the range of 1%˜28%, an immersion time in the step (1) is in the range of 5˜300 min.

### Claim 3 (depends on 2)

The method for recycling electrode materials of lithium ion batteries according to claim 2, wherein the concentration of the ammonia in the step (1) is in the range of 3%˜15%, the immersion time in the step (1) is in the range of 20˜120 min.

### Claim 4 (depends on 1)

The method for recycling electrode materials of lithium ion batteries according to claim 1, wherein a sintering temperature in the step (2) is in the range of 250° C.˜650° C., a sintering time in the step (2) is in the range of 1˜6 h.

### Claim 5 (depends on 4)

The method for recycling electrode materials of lithium ion batteries according to claim 4, wherein the sintering temperature in the step (2) is in the range of 300°0 C.˜500° C., the sintering time in the step (2) is in the range of 1.5˜2.5 h.

### Claim 6 (depends on 1)

The method for recycling electrode materials of lithium ion batteries according to claim 1, wherein supplementing lithium to the positive electrode powder material in the step (3) comprises: analyzing the content of elements of the positive electrode powder material firstly, and then adding lithium compound to the positive electrode powder material according to the stoichiometric ratio of the regenerated positive electrode material.

### Claim 7 (depends on 6)

The method for recycling electrode materials of lithium ion batteries according to claim 6, wherein the lithium compound is selected at least one from the group of lithium hydroxide monohydrate, lithium hydroxide, lithium carbonate, lithium acetate and lithium oxide.

### Claim 8 (depends on 1)

The method for recycling electrode materials of lithium ion batteries according to claim 1, wherein a speed of the milling in the step (3) is in the range of 1000˜4000 r/min, a milling time in the step (3) is in the range of 2˜10 h.

### Claim 9 (depends on 1)

The method for recycling electrode materials of lithium ion batteries according to claim 1, wherein a sintering temperature of producing the regenerated positive electrode material in the step (3) is in the range of 600° C.˜1200° C., a sintering time of producing the regenerated positive electrode material in the step (3) is in the range of 5˜20 h.

### Claim 10 (depends on 9)

The method for recycling electrode materials of lithium ion batteries according to claim 9, wherein the sintering temperature of producing the regenerated positive electrode material in the step (3) is in the range of 700° C.˜900° C., the sintering time of producing the regenerated positive electrode material in the step (3) is in the range of 8˜12 h.

### Claim 11 (depends on 1)

The method for recycling electrode materials of lithium ion batteries according to claim 1, wherein a sintering temperature of producing the regenerated negative electrode material in the step (3) is in the range of 500° C.˜1000° C., a sintering time of producing the regenerated negative electrode material in the step (3) is in the range of 3˜15 h.

### Claim 12 (depends on 11)

The method for recycling electrode materials of lithium ion batteries according to claim 11, wherein the sintering temperature of producing the regenerated negative electrode material in the step (3) is in the range of 700° C.˜850° C., the sintering time of producing the regenerated negative electrode material in the step (3) is in the range of 5˜8 h.

### Claim 13 (depends on 1)

The method for recycling electrode materials of lithium ion batteries according to claim 1, wherein the regenerated positive electrode material includes temary material.

### Claim 14 (depends on 13)

The method for recycling electrode materials of lithium ion batteries according to claim 13, wherein the regenerated positive electrode material is lithium nickel-cobalt-manganese oxide or lithium nickel-cobalt-aluminum oxide.

### Claim 15 (depends on 1)

The method for recycling electrode materials of lithium ion batteries according to claim 1, wherein the regenerated negative electrode material is lithium titanate.