# US 2016/0251737 A1 · Corrosion pitting resistant martensitic stainless steel

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0251737 A1
- Document ID: US20160251737A1
- Status: Published application
- Kind: A1
- Application number: 14/632,159
- Filed: 2015-02-26
- Published: 2016-09-01
- Earliest claimed: 2015-02-26
- Assignees: General Electric Company
- Applicants: General Electric Company
- Inventors: Theodore Francis Majka
- Web page: https://patentgrep.com/patent/US20160251737A1

## CPC

- C21D 8/00: Modifying the physical properties of ferrous metals or ferrous alloys by deformation combined with, or followed by, heat treatment (hardening articles or materials formed by forging or rolling with no further heating beyond that required for the formation C21D1/02)
- C21D 6/004: {containing Cr and Ni}
- C21D 6/007: {containing Co}
- C22C 38/44: with molybdenum or tungsten
- C22C 38/52: with cobalt
- C21D 2211/001: Austenite
- C21D 2211/004: Dispersions; Precipitations
- C21D 2211/008: Martensite
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

A forged, martensitic, stainless steel alloy is disclosed. The alloy comprises, by weight: about 12.0 to about 16.0 percent chromium; greater than 16.0 to about 20.0 percent cobalt, about 6.0 to about 8.0 percent molybdenum, about 1.0 to about 3.0 percent nickel, about 0.020 to about 0.040 percent carbon; and the balance iron and incidental impurities. The forged, martensitic, stainless steel alloys are highly resistant to pitting corrosion and provide a combination of tensile strength, ductility, and fracture toughness suitable for use as turbine compressor airfoils.

## Claims

### Claim 1

A forged, martensitic, stainless steel alloy comprising, by weight: about 12.0 to about 16.0 percent chromium; greater than 16.0 to about 20.0 percent cobalt, about 6.0 to about 8.0 percent molybdenum, about 1.0 to about 3.0 percent nickel, about 0.020 to about 0.040 percent carbon; and the balance iron and incidental impurities.

### Claim 2 (depends on 1)

The alloy of claim 1, wherein the alloy comprises about 16.5 to about 20.0 percent cobalt.

### Claim 3 (depends on 1)

The alloy of claim 1, wherein the alloy has a microstructure that contains substantially no laves phase.

### Claim 4 (depends on 1)

The alloy of claim 1, wherein the alloy has a microstructure that comprises substantially no chi phase.

### Claim 5 (depends on 1)

The alloy of claim 1, wherein the alloy has a microstructure that comprises substantially no delta ferrite phase.

### Claim 6 (depends on 1)

The alloy of claim 1, wherein the alloy has a microstructure that comprises substantially no laves phase, chi phase and delta ferrite phase.

### Claim 7 (depends on 1)

The alloy of claim 1, wherein the alloy has a microstructure that comprises a retained austenite phase.

### Claim 8 (depends on 7)

The alloy of claim 7, wherein the retained austenite phase comprises at least about 15 percent by volume of the microstructure.

### Claim 9 (depends on 8)

The alloy of claim 8, wherein the retained austenite phase comprises about 15 percent to about 25 percent by volume of the microstructure.

### Claim 10 (depends on 1)

The alloy of claim 1, wherein the alloy is configured to provide a tensile elongation of at least about 14 percent.

### Claim 11 (depends on 10)

The alloy of claim 10, wherein the elongation is about 14 to about 24 percent.

### Claim 12 (depends on 1)

The alloy of claim 1, wherein the alloy is configured to provide a tensile reduction in area of at least about 41 percent.

### Claim 13 (depends on 12)

The alloy of claim 12, wherein the reduction in area is about 41 to about 49 percent.

### Claim 14 (depends on 1)

The alloy of claim 1, wherein the alloy has a pitting resistance equivalence number of about 31.8 or more.

### Claim 15 (depends on 1)

The alloy of claim 1, wherein the alloy has an ultimate tensile strength of about 150 ksi or more.

### Claim 16 (depends on 1)

The alloy of claim 1, wherein the alloy comprises a turbine compressor airfoil.

### Claim 17

A method of making a forged, martensitic, stainless steel alloy, comprising:
providing a forged preform of martensitic, pitting corrosion resistant stainless steel alloy comprising, by weight: about 12.0 to about 16.0 percent chromium; greater than 16.0 to about 20.0 percent cobalt, about 6.0 to about 8.0 percent molybdenum, about 1.0 to about 3.0 percent nickel, about 0.020 to about 0.040 percent carbon; and the balance iron and incidental impurities;
heating the forged preform to a solutionizing temperature for a time sufficient to form a solutionized microstructure;
cooling the forged preform and solutionized microstructure to room temperature to form a martensitic microstructure;
heating the forged preform to a tempering temperature of about 600° F. for a tempering time sufficient to form a tempered forged preform comprising a tempered martensitic microstructure; and
cooling the tempered forged preform to room temperature.

### Claim 18 (depends on 17)

The method of claim 17, wherein the solutionizing temperature comprises about 2,000 to about 2,100° F. and the time comprises about 1 to about 3 hours.

### Claim 19 (depends on 17)

The method of claim 17, wherein the tempering time is about 3 to about 6 hours.

### Claim 20 (depends on 17)

The method of claim 17, wherein the tempered forged preform comprises a turbine airfoil preform.