# US 2016/0251736 A1 · Selective laser sintering method, heat treatment method, metal powder, and shaped product

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0251736 A1
- Document ID: US20160251736A1
- Status: Published application
- Kind: A1
- Application number: 15/051,293
- Filed: 2016-02-23
- Published: 2016-09-01
- Earliest claimed: 2015-02-27
- Assignees: Japan Silicolloy Industry Co., Ltd.
- Applicants: Japan Silicolloy Industry Co., Ltd.
- Inventors: Takayasu Shimizu
- Web page: https://patentgrep.com/patent/US20160251736A1

## CPC

- C21D 1/18: Hardening (C21D1/02 takes precedence); Quenching with or without subsequent tempering (quenching devices C21D1/62)
- B22F 10/28: Powder bed fusion, e.g. selective laser melting [SLM] or electron beam melting [EBM]
- B22F 10/34: of powder characteristics, e.g. density, oxidation or flowability
- B22F 10/366: Scanning parameters, e.g. hatch distance or scanning strategy
- C21D 6/004: {containing Cr and Ni}
- C21D 6/005: {containing Mn}
- C21D 6/008: {containing Si}
- C21D 9/0068: {for particular articles not mentioned below}
- C22C 38/04: containing manganese
- C22C 38/34: with more than 1.5% by weight of silicon
- C22C 38/42: with copper
- C22C 38/44: with molybdenum or tungsten
- C22C 38/48: with niobium or tantalum
- B22F 10/36: of energy beam parameters
- B22F 10/50: Treatment of workpieces or articles during build-up, e.g. treatments applied to fused layers during build-up
- B22F 10/64: by thermal means (control of energy beam parameters for post heating B22F10/364)
- B22F 2003/248: {Thermal after-treatment}
- B22F 2998/10: Processes characterised by the sequence of their steps
- B22F 2999/00: Aspects linked to processes or compositions used in powder metallurgy
- C22C 33/0285: {with Cr, Co, or Ni having a minimum content higher than 5%}
- Y02P 10/25: Process efficiency
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A selective laser sintering method alternately repeats a step of forming silicon alloy A2 powder (metal powder) in layers, the silicon alloy A2 powder made of high silicon stainless steel containing C:less than 0.10, Si:2.0˜9.0, Mn:0.05˜6.0, Cu:0.5˜4.0, Ni:1.0˜24.0, Cr:6.0˜28.0, Mo:0.2˜4.0, Nb:0.03˜2.0 in wt % and the balance of Fe and inevitable impurities, and a step of selectively applying a laser to the silicon alloy A2 powder formed in layers to melt and sinter the silicon alloy A2 powder.

## Claims

### Claim 1

A selective laser sintering method comprising:
alternately repeating
a step of forming metal powder in layers, the metal powder being made of high silicon stainless steel containing C:less than 0.10, Si:2.0˜9.0, Mn:0.05˜6.0, Cu:0.5˜4.0, Ni:1.0˜24.0, Cr:6.0˜28.0, Mo:0.2˜4.0, Nb:0.03˜2.0 in wt %, and a balance of Fe and inevitable impurities; and
a step of selectively applying a laser to the metal powder formed in layers to melt and sinter the metal powder.

### Claim 2 (depends on 1)

The selective laser sintering method according to claim 1, wherein a particle size of the metal powder is 32 to 62 micrometers.

### Claim 3 (depends on 1)

The selective laser sintering method according to claim 1, wherein
energy density E calculated by following equation is 31 to 124 [J/mm3]
E
=
P
v
×
s
×
t
where P is an output of the laser, v is a scanning speed of the laser, s is a scanning pitch of the laser, and t is a lamination thickness of one layer of the metal powder.

### Claim 4 (depends on 3)

The selective laser sintering method according to claim 3, wherein the energy density E is 36 to 124 [J/mm3].

### Claim 5 (depends on 3)

The selective laser sintering method according to claim 3, wherein the energy density E is 50 to 124 [J/mm3].

### Claim 6 (depends on 3)

The selective laser sintering method according to claim 3, wherein the energy density E is 50 to 118 [J/mm3].

### Claim 7 (depends on 1)

A heat treatment method comprising:
a step of performing solution treatment on a shaped product shaped by the selective laser sintering method according to claim 1; and
a step of performing ageing treatment on the shaped product after the solution treatment.

### Claim 8

Metal powder used in a selective laser sintering method that selectively applies a laser to metal powder to melt and sinter the metal powder for lamination, wherein
the metal powder is made of high silicon stainless steel containing C:less than 0.10, Si:2.0˜9.0, Mn:0.05˜6.0, Cu:0.5˜4.0, Ni:1.0˜24.0, Cr:6.0˜28.0, Mo:0.2˜4.0, Nb:0.03˜2.0 in wt %, and a balance of Fe and inevitable impurities.

### Claim 9 (depends on 8)

The metal powder according to claim 8, wherein a particle size of the metal powder is 32 to 62 micrometers.

### Claim 10 (depends on 1)

A shaped product shaped by the selective laser sintering method according to claim 1.

### Claim 11 (depends on 7)

A shaped product heat-treated by the heat treatment method according to claim 7.