# US 2016/0251574 A1 · Composition containing a core-shell aluminate, phosphor obtained from said composition, and preparation methods

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0251574 A1
- Document ID: US20160251574A1
- Status: Published application
- Kind: A1
- Application number: 15/055,502
- Filed: 2016-02-26
- Published: 2016-09-01
- Earliest claimed: 2010-12-14
- Assignees: Rhodia Operations
- Applicants: Rhodia Operations
- Inventors: Valerie BUISSETTE; Thierry LE-MERCIER; Franck AURISSERGUES
- Web page: https://patentgrep.com/patent/US20160251574A1

## CPC

- C09K 11/7774: {Aluminates}
- C04B 35/62897: {Coatings characterised by their thickness}
- C09K 11/02: Use of particular materials as binders, particle coatings or suspension media therefor
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE

## Abstract

A composition comprising an inorganic core and an aluminate shell is described. The aluminate can have the formula (1): (CeaTbb)Mg1+xAl11+y019+x+y (1), where a, b, x and y comply with the relations a+b=1−0.2˜x˜+0.2 and −0.2˜y˜+0.2, wherein the shell uniformly covers the inorganic core over a thickness of no less than 300 nm. A phosphor is also described that can be obtained by calcinating the composition at a temperature of at least 1200° C.

## Claims

### Claim at position 1

1-11. (canceled)

### Claim 12

A process for the preparation of a phosphor, the phosphor comprising:
an inorganic core; and
a shell based on an aluminate of formula (1):
(CeaTbb)Mg1+xAl11+yO19+x+y (1),
wherein:
a+b=1,
−0.2≦x≦+0.2, and
−0.2≦y≦+0.2;
wherein the shell homogeneously covers the inorganic core at a thickness equal to or greater than 300 nm.
wherein the process comprises:
drying a liquid mixture by atomization, the liquid mixture comprising compounds of aluminum, magnesium and one or both of cerium and terbium, and the inorganic core;
calcining the dry product at a temperature of between 700° C. and 950° C. to form a composition; and
calcining the composition at a temperature of at least 1200° C. to form the phosphor.

### Claim 13 (depends on 12)

The process as defined by claim 12, wherein the aluminum compound is in the form of an aluminum sol.

### Claim 14 (depends on 12)

The process as defined by claim 12, wherein the shell covers the inorganic core at a thickness equal to or less than 2000 nm.

### Claim 15 (depends on 14)

The process as defined by claim 14, wherein the shell covers the inorganic core at thickness between 750 nm and 1500 nm.

### Claim 16 (depends on 12)

The process as defined by claim 12, wherein the aluminate corresponds to the formula (1) in which x=y=0.

### Claim 17 (depends on 12)

The process as defined by claim 12, wherein the inorganic core is alumina, zirconia or an alkaline earth metal aluminate.

### Claim 18 (depends on 17)

The process as defined by claim 17, wherein the alumina or zirconia is doped.

### Claim 19 (depends on 17)

The process as defined by claim 17, wherein the alkaline earth metal aluminate is a magnesium aluminate.