# US 2016/0251504 A1 · Polyethylene molding composition for producing blown films having improved processability

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0251504 A1
- Document ID: US20160251504A1
- Status: Published application
- Kind: A1
- Application number: 15/154,800
- Filed: 2016-05-13
- Published: 2016-09-01
- Earliest claimed: 2005-03-01
- Assignees: Basell Polyolefine GmbH
- Applicants: Basell Polyolefine GmbH
- Inventors: Joachim Berthold; Lutz-Gerd Heinicke; Gerhardus Meier
- Web page: https://patentgrep.com/patent/US20160251504A1

## CPC

- C08L 23/06: Polyethylene
- C08J 5/18: Manufacture of films or sheets
- C08L 23/04: Homopolymers or copolymers of ethene
- C08L 23/0807: with unsaturated hydrocarbons only containing four or more carbon atoms
- C08L 23/0815: {with aliphatic 1-olefins containing one carbon-to-carbon double bond}
- C08J 2323/04: Homopolymers or copolymers of ethene
- C08J 2323/06: Polyethene
- C08J 2423/08: Copolymers of ethene (C08J2423/16 takes precedence)
- C08L 23/08: Copolymers of ethene (C08L23/16 takes precedence)
- C08L 2203/16: used for films
- C08L 2205/025: containing two or more polymers of the same hierarchy C08L, and differing only in parameters such as density, comonomer content, molecular weight, structure
- C08L 2205/03: containing three or more polymers in a blend
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)

## Abstract

The invention relates to a polyethylene molding composition having a multimodal molar mass distribution particularly suitable for blow molding films having a thickness in the range from 8 to 200 μm. The molding composition has a density at a temperature of 23° C. in the range from 0.953 to 0.960 g/cm3 and an MFR190/5 of the final product after extrusion in the range from 0.10 to 0.50 dg/min. The composition comprises from 30 to 60% by weight of a first ethylene polymer fraction made of a homopolymer A having a first molecular weight, from 22 to 40% by weight of a second ethylene polymer fraction made of a further homopolymer or first copolymer B of ethylene and at least one first comonomer from the group of olefins having from 4 to 8 carbon atoms, the first copolymer B having a second molecular weight higher than the first molecular weight, and from 10 to 30% by weight of a third ethylene polymer fraction made of a second copolymer C having a third molecular weight higher than the second molecular weight. The molding composition of the invention allows to produce thin films having improved processability without impairing the mechanical properties.

## Claims

### Claim 1

A polyethylene molding composition having a multimodal molar mass distribution, a density at a temperature of 23° C. in the range from 0.953 to 0.960 g/cm3 and a MFR190/5 of the final product after extrusion in the range from 0.10 to 0.50 dg/min, said polyethylene molding composition comprising:
from 30 to 60% by weight of a first ethylene polymer fraction made of an ethylene homopolymer A having a first molecular weight,
from 22 to 40% by weight of a second ethylene polymer fraction made of a further homopolymer or first copolymer B of ethylene and at least one first comonomer from the group of olefins having from 4 to 8 carbon atoms, said first copolymer B having a second molecular weight higher than said first molecular weight, and
from 10 to 30% by weight of a third ethylene polymer fraction made of a second copolymer C of ethylene and at least one second comonomer, said second copolymer C having a third molecular weight higher than said second molecular weight,
all percentages being based on the total weight of the molding composition.

### Claim 2 (depends on 1)

The polyethylene molding composition according to claim 1, comprising:
from 42 to 52% by weight of the first ethylene polymer fraction,
from 27 to 38% by weight of the second ethylene polymer fraction, the first copolymer B containing from 0.1 to 1.0% by weight, based on the weight of copolymer B, of said at least one first comonomer, and
from 15 to 25% by weight of the third ethylene polymer fraction, the second copolymer C containing from 1 to 15% by weight, based on the weight of the second copolymer C, of said at least one second comonomer.

### Claim 3 (depends on 1)

The polyethylene molding composition of claim 1, wherein said first comonomer and said second comonomer are independently selected from the group comprising 1-butene, 1-pentene, 1-hexene, 1-octene, 4-methyl-1-pentene and mixtures thereof.

### Claim 4 (depends on 1)

The polyethylene molding composition of claim 1, wherein the density is from 0.955 to 0.959 g/cm3 and the MFR190/5 of the final product after extrusion is in the range from 0.32 to 0.42 g/10 min.

### Claim 5 (depends on 4)

The polyethylene molding composition according to claim 4, having a viscosity number VN3, measured in accordance with ISO/R 1191 in decalin at a temperature of 135° C., in the range from 270 to 400 cm3/g.

### Claim 6 (depends on 1)

A process for preparing the polyethylene molding composition of claim 1, comprising the step of polymerizing ethylene, said at least one first comonomer and said at least one second comonomer in suspension at temperatures in the range from 20 to 120° C., at a pressure in the range from 2 to 10 bar and in the presence of a Ziegler catalyst comprising a transition metal compound and an organo-aluminum compound.

### Claim 7 (depends on 6)

The process according to claim 6, wherein said polymerization step is carried out in multiple successive polymerization stages comprising a first stage, a second stage, and a third stage performed in corresponding multiple reactors comprising a first reactor, a second reactor and a third reactor arranged in series, the molar mass of the polyethylene composition prepared in each stage being adjusted in each case by means of hydrogen.

### Claim 8 (depends on 7)

The process according to claim 7, wherein the hydrogen concentration in the first polymerization stage is set in such a manner that the homopolymer A has a viscosity number VN1 in the range from 70 to 110 cm3/g.

### Claim 9 (depends on 7)

The process according to claim 7, wherein the hydrogen concentration in the second polymerization stage is set in such a manner that the mixture of homopolymer A plus homopolymer or copolymer B has a viscosity number VN2 in the range from 250 to 400 cm3/g.

### Claim 10 (depends on 7)

The process according to claim 7, wherein the hydrogen concentration in the third polymerization stage is set in such a manner that the mixture of homopolymer A plus first homopolymer or copolymer B plus second copolymer C has a viscosity number VN3 in the range from 280 to 400 cm3/g.

### Claim 11 (depends on 1)

Use of a polyethylene molding composition according to claim 1, for producing blown films having a thickness in the range from 8 to 200 μm.

### Claim 12 (depends on 11)

The use of a polyethylene molding composition according to claim 11, wherein the blown film is produced via a blown film process comprising the step of melting the polyethylene molding composition so as to obtain a polyethylene melt, extruding the polyethylene melt by forcing the same through an annular die so as to form a bubble having a frost line oscillating at a maximum of ±2 cm in axial direction during the shock test at a maximal take-off speed.

### Claim 13 (depends on 1)

A blown film comprising a polyethylene molding composition according to claim 1, having a thickness in the range from 8 to 200 μm, and a DDI of more than 280 g, measured on a film having a thickness of 20 μm.