# US 2016/0251503 A1 · Additives for rubber compositions

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0251503 A1
- Document ID: US20160251503A1
- Status: Published application
- Kind: A1
- Application number: 14/897,673
- Filed: 2014-12-18
- Published: 2016-09-01
- Earliest claimed: 2013-11-21
- Assignees: Arizona Chemical Company
- Applicants: Arizona Chemical Company, LLC
- Inventors: Jeffery Lin Chenchy; Godefridus J. H. Buisman; Yubin Wu
- Web page: https://patentgrep.com/patent/US20160251503A1

## CPC

- C08L 9/06: Copolymers with styrene
- B60C 1/0016: {Compositions of the tread}
- C08K 3/36: Silica
- C08K 5/09: Carboxylic acids; Metal salts thereof; Anhydrides thereof
- C08K 5/548: containing sulfur {(C08K5/5477 takes precedence)}
- C08L 21/00: Compositions of unspecified rubbers
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- B60C: VEHICLE TYRES; TYRE INFLATION; TYRE CHANGING; CONNECTING VALVES TO INFLATABLE ELASTIC BODIES IN GENERAL; DEVICES OR ARRANGEMENTS RELATED TO TYRES
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)

## Abstract

The instant invention relates to rubber compositions comprising silica, an organomercaptosilane having a bulky group and/or a polyether group bound to the silicon atom and a rosin-containing material. The instant invention also relates to tires comprising such rubber compositions, to methods of preparation of such rubber compositions or tires thereof, and to the use of rosin-containing materials for improving the Mooney viscosity and mechanical properties of rubbers comprising the same (e.g. in a tire).

## Claims

### Claim 1

A rubber composition comprising
(A) a rubber;
(B) silica;
(C) an organomercaptosilane having a bulky group and/or a polyether group bound to the silicon atom and
(D) a rosin-containing material (comprising at least one rosin compound and derivatives thereof) selected from at least one of rosin, dimerized rosin, hydrogenated rosin, disproportionated rosin, decarboxylated rosin and rosin ester,
wherein the bulky group has a total number of carbon atoms and, if any, heteroatoms of at least 20.

### Claim 2 (depends on 1)

The composition of claim 1, wherein the rosin containing-material has an acid number 0.5 to 210 mg KOH/g, in particular from 1 to 205 mg KOH/g, more in particular from 1.5 to 200 mg KOH/g, yet more in particular from 2 to 195 KOH/g; and/or has a softening point from 40 to 170° C., in particular from 45 to 160° C., more in particular from 50 to 150° C., yet more in particular from 55 to 145° C.

### Claim 3 (depends on 1)

The rubber composition of claim 1, wherein the rosin-containing material is a rosin or derivative thereof, in particular selected from tall oil rosin, gum rosin, and wood rosin, and more in particular the rosin-containing material is tall oil rosin.

### Claim 4 (depends on 1)

The rubber composition of claim 1, wherein the organomercaptosilane has both a bulky group and a polyether group bound to the silicon atom.

### Claim 5 (depends on 1)

The rubber composition of claim 1, wherein the bulky group has a total number of carbon atoms and, if any, heteroatoms of at least 22, more in particular at least 24, more in particular at least 28.

### Claim 6 (depends on 1)

The rubber composition of claim 1, wherein the bulky group is a R— group or a RO— group, wherein R is branched or linear monovalent or divalent alkyl, alkenyl, aryl or aralkyl group; and, optionally, R is substituted.

### Claim 7 (depends on 1)

The rubber composition of claim 1, wherein the polyether group is of formula —O(R′—O)m—R″, wherein
R′ is identical or different when m>1 and is a branched or linear, saturated or unsaturated, aliphatic divalent C1-C30 hydrocarbon group;
m is on average 1 to 30; and
R″ is an unsubstituted or substituted branched or linear monovalent alkyl, alkenyl, aryl or aralkyl group having at least 7 carbon atoms, in particular at least 9 carbon atoms and more in particular at least 11 carbon atoms, and more in particular at least 12 atoms.

### Claim 8 (depends on 7)

The rubber composition of claim 7, wherein
R′ is selected from linear aliphatic divalent hydrocarbon group having from 1 to 4 carbon atoms;
m is from 3 to 7; and
R″ is an linear alkyl with 12 to 15 carbon atoms.

### Claim 9 (depends on 1)

The rubber composition of claim 1, wherein the polyether group has a total number of carbon atoms and heteroatoms of at least 20, in particular at least 22, more in particular at least 24, more in particular at least 28.

### Claim 10 (depends on 1, 5, 6, 7, 8, 9)

The rubber composition of claim 1, wherein the organomercaptosilane is an organomercaptosilane of formula (I)
wherein R1 and R2 independently are the same or different and wherein at least one of R1 and R2 is a bulky group and/or a polyether group as defined in any one of claims 1 and 5-9;
R3 is a branched or linear, saturated or unsaturated, aliphatic, aromatic or mixed aliphatic/aromatic divalent C1-C30 hydrocarbon group, in particular a C1-C15 hydrocarbon group, more in particular a C2-C10 hydrocarbon group, and even more in particular a C3-C5 hydrocarbon group; and
R4 is H, CN or (C═O)—R7, where R7 is a branched or linear, saturated or unsaturated, aliphatic, aromatic or mixed aliphatic/aromatic monovalent C1-C30 hydrocarbon group, in particular a C5-C30 hydrocarbon group, more in particular a C5-C20 hydrocarbon group, even more in particular a C7-C15 hydrocarbon group, and yet more in particular a C7-C11 hydrocarbon group.

### Claim 11 (depends on 10)

The rubber composition of claim 10, wherein
R1 is a polyether group; and
each R2 independently is the group R1, a C1-C12 alkyl or a R5O group, where R5 is H, methyl, ethyl, propyl, a C9-C30 branched or linear monovalent alkyl, alkenyl, aryl or aralkyl group or (R6)3Si group where R6 is a C1-C30 branched or linear, alkyl or alkenyl group.

### Claim 12 (depends on 11)

The rubber composition of claim 11, wherein
R2 is the group R1 and/or a R5O group, where R5 is independently selected from methyl, ethyl and propyl;
R3 is a C3-C5 hydrocarbon group; and
R4 is hydrogen.

### Claim 13 (depends on 12)

The rubber composition of claim 12, wherein the organomercaptosilane has a polyether group and an ethoxy group bound to the silicon atom and is an organomercaptosilane of formula
wherein RO— is ethoxy (CH2H5O—) or the polyether group.

### Claim 14 (depends on 1)

The rubber composition of claim 1, wherein the rubber (A) is selected from at least one of styrene/butadiene copolymer (SBR), polybutadiene (BR), natural rubber, polyisoprene, butadiene/isoprene copolymer (IIR), styrene/isoprene/butadiene terpolymer (SIBR), and isoprene/styrene copolymer.

### Claim 15 (depends on 1)

The rubber composition of claim 1, wherein the amount of the organomercaptosilane (C) is from 0.05 to 75 phr, in particular from 0.1 to 60 phr, more in particular from 0.5 to 50 phr, more in particular from 1 to 30 phr, even more in particular from 5 to 15 phr wherein phr is the weight parts of organomercaptosilane per 100 weight parts of rubber component (A).

### Claim 16 (depends on 1)

The rubber composition of claim 1, wherein the amount of rosin-containing material (D) is from 0.001 to 75 phr, in particular from 0.01 to 50 phr, in particular from 0.1 to 25 phr, more in particular from 0.25 to 10 phr, even more in particular from 0.5 to 5.0 phr wherein phr is the weight parts of rosin-containing material per 100 weight parts of rubber component (A).

### Claim 17 (depends on 1)

The rubber composition of claim 1, wherein the amount of silica (B) is from 5 to 150 phr, in particular from 25 to 130 phr, in particular from 40 to 115, wherein phr is the weight parts of silica per 100 weight parts of rubber component (A).

### Claim 18 (depends on 1)

The rubber composition of claim 1 comprising 5-150 phr of silica (B), 0.05-75 phr of the organomercaptosilane (C) and 0.001-75 phr of the rosin-containing material (D), wherein phr is the weight parts of each component (B), (C) or (D) per 100 weight parts of rubber component (A).

### Claim 19 (depends on 1)

The rubber composition of claim 1, having, when the rubber composition is in STAGE 1, a Mooney viscosity from 1 to 75% lower, in particular from 2.5 to 50% lower, more in particular from 5 to 25% lower, even more in particular from 7.5 to 15% lower than the Mooney viscosity of a similar rubber composition without a rosin-containing material.

### Claim 20 (depends on 1)

The rubber composition of claim 1, having, when the rubber composition is not cured, a ratio of the tensile strength measured at 200% elongation over the tensile strength measured at 50% elongation (M200/M50 ratio) from 1 to 50% higher, in particular from 2 to 35% higher, more in particular from 5 to 25% higher than the M200/M50 ratio of a similar rubber compositions without a rosin-containing material.

### Claim 21 (depends on 1)

The rubber composition of claim 1, having an elongation at break from 5 to 75% higher, in particular from 10 to 60% higher, more in particular from 25 to 50% higher than the elongation at break of similar rubber compositions without a rosin-containing material.

### Claim 22 (depends on 1)

The rubber composition of claim 1, having, when the rubber composition is cured, a tan δ at 60° C. less than 10% higher, in particular less than 5% higher, more in particular less than 3% higher, than the tan δ at 60° C. of a similar rubber composition without rosin-containing materials, the tan δ at 60° C. being measured at a frequency of 10 Hz and a strain of 0.1% under shear mode.

### Claim 23 (depends on 1)

A tire comprising the rubber composition of claim 1.

### Claim 24

Use of a rosin-containing material selected from rosin, dimerized rosin, hydrogenated rosin, disproportionated rosin, decarboxylated rosin and rosin ester (component D)
in a rubber composition further comprising
a rubber (component A);
silica (component B); and
an organomercaptosilane having a bulky group and/or a polyether group bound to the silicon atom (component C), wherein the bulky group has a total number of carbon atoms and, if any, heteroatoms of at least 20
to obtain a rubber composition having, when the rubber composition is not cured, a reduced Mooney viscosity and/or improved mechanical properties when compared to a similar uncured rubber composition without component D; and/or
to obtain a rubber composition having, when the rubber composition is cured, improved tensile strength when compared to a similar cured rubber composition without component D.

### Claim 25 (depends on 1)

A method for preparing a rubber composition according to claim 1 comprising mixing:
(A) a rubber;
(B) silica;
(C) an organomercaptosilane having a bulky group and/or a polyether group, wherein the bulky group has a total number of carbon atoms and, if any, heteroatoms of at least 20; and
(D) of a rosin-containing material selected from rosin, dimerized rosin, hydrogenated rosin, disproportionated rosin, decarboxylated rosin and rosin ester.