# US 2016/0251497 A1 · Method for producing stabilized polymer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0251497 A1
- Document ID: US20160251497A1
- Status: Published application
- Kind: A1
- Application number: 15/030,715
- Filed: 2014-10-20
- Published: 2016-09-01
- Earliest claimed: 2013-10-21
- Assignees: Adeka Corporation
- Applicants: Adeka Corporation
- Inventors: Naoshi KAWAMOTO; Atsushi SAKAI; Tetsuya SEGUCHI; Kenji YAMAZAKI
- Web page: https://patentgrep.com/patent/US20160251497A1

## CPC

- C08K 5/524: Esters of phosphorous acids, e.g. of H3PO3
- C08F 2/44: Polymerisation in the presence of compounding ingredients, e.g. plasticisers, dyestuffs, fillers
- C08K 5/134: Phenols containing ester groups
- C08K 5/005: {Stabilisers against oxidation, heat, light, ozone}
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS

## Abstract

Provided is a method of producing a stabilized polymer by which, while imparting sufficient stabilizing effect to the polymer of a monomer having an ethylenically unsaturated bond, the amount of residual solvent in the polymer can be reduced and the occurrence of foaming can be inhibited. The method of producing a stabilized polymer comprises the step of adding an antioxidant having a melting point of 70° C. or lower to a catalyst system or a polymerization system before or during polymerization of a monomer having an ethylenically unsaturated bond such that 0.005 to 0.5 parts by mass of the antioxidant is incorporated with respect to 100 parts by mass of a polymer obtained by the polymerization of the monomer having an ethylenically unsaturated bond.

## Claims

### Claim 1

A method of producing a stabilized polymer, said method comprising the step of adding an antioxidant having a melting point of 70° C. or lower to a catalyst system or a polymerization system before or during polymerization of a monomer having an ethylenically unsaturated bond such that 0.005 to 0.5 parts by mass of said antioxidant is incorporated with respect to 100 parts by mass of a polymer obtained by said polymerization of said monomer having an ethylenically unsaturated bond.

### Claim 2

A method of producing a stabilized polymer, said method comprising the step of adding a mixture of an antioxidant having a melting point of 70° C. or lower and a solvent to a catalyst system or a polymerization system before or during polymerization of a monomer having an ethylenically unsaturated bond such that 0.005 to 0.5 parts by mass of said antioxidant and 5 parts by mass or less of said solvent are incorporated with respect to 100 parts by mass of a polymer obtained by said polymerization of said monomer having an ethylenically unsaturated bond.

### Claim 3 (depends on 1)

The method of producing a stabilized polymer according to claim 1, wherein said monomer having an ethylenically unsaturated bond comprises an α-olefin.

### Claim 4 (depends on 2)

The method of producing a stabilized polymer according to claim 2, wherein said solvent is selected from mineral oils, aliphatic solvents, aromatic solvents and mixtures thereof.

### Claim 5 (depends on 1)

The method of producing a stabilized polymer according to claim 1, wherein said polymerization is vapor-phase polymerization or bulk polymerization.

### Claim 6 (depends on 1)

The method of producing a stabilized polymer according to claim 1, wherein said antioxidant having a melting point of 70° C. or lower contains at least one compound represented by the following Formula (1) or (2):
(wherein, R1 and R2 each independently represent any of an alkyl group having 1 to 40 carbon atoms, an aryl group having 6 to 40 carbon atoms, an arylalkyl group having 7 to 40 carbon atoms, a heterocycle-containing group having 3 to 25 carbon atoms and a combination thereof, which R1 and R2 are optionally bound together to form 5,5-dialkyl-1,3,2-dioxaphosphorinane;
R3 represents a direct bond, an alkylidene group having 1 to 40 carbon atoms or an arylene group having 6 to 40 carbon atoms;
b represents an integer of 1 to 4;
when b is 1, T represents a hydrogen atom, an alkyl group having 1 to 40 carbon atoms or an aryl group having 6 to 40 carbon atoms;
when b is 2, T represents an alkylidene group having 1 to 40 carbon atoms, an arylene group having 6 to 40 carbon atoms or —O—;
when b is 3, T represents an alkanetriyl group having 1 to 40 carbon atoms;
when b is 4, T represents an alkanetetrayl group having 1 to 40 carbon atoms;
a methylene group in said alkyl group, said alkylidene group, said alkanetriyl group and said alkanetetrayl group are optionally substituted with >C═O, —O—, —S—, —CO—O—, —O—CO—, —O—CO—O—, —NR4—, a phosphine, a phosphinite, a phosphonite, a phosphite, a phosphorane, a phosphonate or a combination thereof and also branched; and
R4 represents a hydrogen atom or an alkyl group having 1 to 4 carbon atoms); or
(wherein, R5 and R6 each independently represent an alkyl group having 1 to 40 carbon atoms or an aryl group having 6 to 40 carbon atoms).

### Claim 7 (depends on 2)

The method of producing a stabilized polymer according to claim 2, wherein said monomer having an ethylenically unsaturated bond comprises an α-olefin.

### Claim 8 (depends on 2)

The method of producing a stabilized polymer according to claim 2, wherein said polymerization is vapor-phase polymerization or bulk polymerization.

### Claim 9 (depends on 2)

The method of producing a stabilized polymer according to claim 2, wherein said antioxidant having a melting point of 70° C. or lower contains at least one compound represented by the following Formula (1) or (2):
(wherein, R1 and R2 each independently represent any of an alkyl group having 1 to 40 carbon atoms, an aryl group having 6 to 40 carbon atoms, an arylalkyl group having 7 to 40 carbon atoms, a heterocycle-containing group having 3 to 25 carbon atoms and a combination thereof, which R1 and R2 are optionally bound together to form 5,5-dialkyl-1,3,2-dioxaphosphorinane;
R3 represents a direct bond, an alkylidene group having 1 to 40 carbon atoms or an arylene group having 6 to 40 carbon atoms;
b represents an integer of 1 to 4;
when b is 1, T represents a hydrogen atom, an alkyl group having 1 to 40 carbon atoms or an aryl group having 6 to 40 carbon atoms;
when b is 2, T represents an alkylidene group having 1 to 40 carbon atoms, an arylene group having 6 to 40 carbon atoms or —O—;
when b is 3, T represents an alkanetriyl group having 1 to 40 carbon atoms;
when b is 4, T represents an alkanetetrayl group having 1 to 40 carbon atoms;
a methylene group in said alkyl group, said alkylidene group, said alkanetriyl group and said alkanetetrayl group are optionally substituted with >C═O, —O—, —S—, —CO—O—, —O—CO—, —O—CO—O—, —NR4—, a phosphine, a phosphinite, a phosphonite, a phosphite, a phosphorane, a phosphonate or a combination thereof and also branched; and
R4 represents a hydrogen atom or an alkyl group having 1 to 4 carbon atoms); or
(wherein, R5 and R6 each independently represent an alkyl group having 1 to 40 carbon atoms or an aryl group having 6 to 40 carbon atoms).