# US 2016/0251464 A1 · Ethylene-based quaterpolymer having low glass transition temperature and preparation method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0251464 A1
- Document ID: US20160251464A1
- Status: Published application
- Kind: A1
- Application number: 14/769,014
- Filed: 2015-04-08
- Published: 2016-09-01
- Earliest claimed: 2014-04-08
- Assignees: Korea Institute of Industrial Technology
- Applicants: Korea Institute of Industrial Technology
- Inventors: Dong Hyun Kim; Jung Soo Kim; Dong Gyu Jeon; Ji Hoon Jang
- Web page: https://patentgrep.com/patent/US20160251464A1

## CPC

- C08F 210/16: Copolymers of ethene with alpha-alkenes, e.g. EP rubbers
- C08F 210/18: with non-conjugated dienes, e.g. EPT rubbers
- C08F 212/08: Styrene
- C08F 212/36: Divinylbenzene
- C08F 4/6592: containing at least one cyclopentadienyl ring, condensed or not, e.g. an indenyl or a fluorenyl ring
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS

## Abstract

The present invention relates to a highly elastic, ethylene-based quaterpolymer and a preparation method thereof. More particularly, the present invention relates to a highly elastic, ethylene-based quaterpolymer which comprises a specific molar ratio of an ethylene unit, a C4-6 α-olefin unit, a C8-12 α-olefin unit and at least one functional unit derived from a styrene-based monomer and to a method for preparing the ethylene-based quaterpolymer using a metallocene catalyst.

## Claims

### Claim 1

A highly elastic, ethylene-based quaterpolymer comprising:
55-93.9 mol % of an ethylene unit;
3-40 mol % of a C4-6 α-olefin unit;
3-40 mol % of a C8-12 α-olefin unit; and
0.1-5 mol % of a functional unit derived from at least one styrene-based monomer,
the ethylene-based quaterpolymer having a weight-average molecular weight of 50,000-300,000 and a glass transition temperature between −40° C. and −80° C.

### Claim 2 (depends on 1)

The highly elastic, ethylene-based quaterpolymer according to claim 1, wherein the copolymer comprises:
65-85 mol % of an ethylene unit;
3-25 mol % of a C4-6 α-olefin unit;
5-25 mol % of a C8-12 α-olefin unit; and
0.3-2 mol % of a functional unit derived from at least one styrene-based monomer.

### Claim 3 (depends on 1)

The highly elastic, ethylene-based quaterpolymer according to claim 1, wherein the styrene-based monomer is styrene, divinylbenzene, p-methylstyrene, α-methylstyrene, butylstyrene, methoxystyrene, isopropylstyrene or butenylstyrene.

### Claim 4 (depends on 1)

The highly elastic, ethylene-based quaterpolymer according to claim 1, wherein the copolymer has a molecular weight distribution of 1-3.

### Claim 5 (depends on 1)

The highly elastic, ethylene-based quaterpolymer according to claim 1, wherein the copolymer has a Tanδ of 0.3 or greater.

### Claim 6

A method for preparing an ethylene-based quaterpolymer, comprising polymerizing 55-93.9 mol % of an ethylene monomer, 3-40 mol % of a C4-6 α-olefin monomer, 3-40 mol % of a C8-12 α-olefin monomer and 0.1-5 mol % of at least one styrene-based monomer using a metallocene catalyst.

### Claim 7 (depends on 6)

The method for preparing an ethylene-based quaterpolymer according to claim 6, wherein the metallocene catalyst comprises a group 4 transition metal as a metal center; cyclopentadienyl or a derivative thereof, fluorenyl or a derivative thereof, or indenyl or a derivative thereof as a ligand; and has a bridged (ansa) structure or a non-bridged structure.

### Claim 8 (depends on 7)

The method for preparing an ethylene-based quaterpolymer according to claim 7, wherein the metallocene catalyst is ethyl bis(indenyl)zirconium dichloride.

### Claim 9 (depends on 6)

The method for preparing an ethylene-based quaterpolymer according to claim 6, wherein the catalytic activity in the polymerization is 5,000 or higher.

### Claim 10 (depends on 6)

The method for preparing an ethylene-based quaterpolymer according to claim 6, wherein the metallocene catalyst is used together with a metallocene cocatalyst selected from the group consisting of an alkylaluminoxane cocatalyst, an organic alkylaluminum cocatalyst, a boron compound cocatalyst and a mixture thereof.

### Claim 11 (depends on 10)

The method for preparing an ethylene-based quaterpolymer according to claim 10, wherein
the alkylaluminoxane cocatalyst is selected from the group consisting of methylaluminoxane, ethylaluminoxane, propylaluminoxane, butylaluminoxane and isobutylaluminoxane;
the organic alkylaluminum cocatalyst is selected from the group consisting of trimethylaluminum, triethylaluminum, diisobutylaluminum, triisobutylaluminum and tri-n-octylaluminum; and
the boron compound cocatalyst is selected from the group consisting of tris(pentafluorophenyl)borane, trityl tetrakis(pentafluorophenyl)borate, dimethylanilinium tetrakis(pentafluorophenyl)borate and triphenylmethylinium tetrakis(pentafluorophenyl)borate.

### Claim 12 (depends on 6)

The method for preparing an ethylene-based quaterpolymer according to claim 6, wherein the polymerization is performed at 20-70° C.

### Claim 13 (depends on 6)

The method for preparing an ethylene-based quaterpolymer according to claim 6, wherein the polymerization is performed for from 20 minutes to 1 hour.