# US 2016/0251331 A1 · Metal-conjugated microporous polymers

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0251331 A1
- Document ID: US20160251331A1
- Status: Published application
- Kind: A1
- Application number: 14/980,238
- Filed: 2015-12-28
- Published: 2016-09-01
- Earliest claimed: 2011-12-19
- Assignees: Dalian Institute of Chemical Physics, Chinese Academy of Science
- Applicants: Dalian Institute of Chemical Physics, Chinese Academy of Sciences
- Inventors: Weiqiao DENG; Yong XIE; Xiaohuan LIU
- Web page: https://patentgrep.com/patent/US20160251331A1

## CPC

- C07D 317/36: Alkylene carbonates; Substituted alkylene carbonates
- B01J 31/1691: {Coordination polymers, e.g. metal-organic frameworks [MOF] (preparation of metal complexes containing carboxylic acid moieties C07C51/418; MOF's per se C07F)}
- B01J 31/2243: {At least one oxygen and one nitrogen atom present as complexing atoms in an at least bidentate or bridging ligand}
- B01J 31/2295: {Cyclic compounds, e.g. cyclopentadienyls}
- B01J 2231/341: 1,2-additions, e.g. aldol or Knoevenagel condensations
- B01J 2531/0252: Salen ligands or analogues, e.g. derived from ethylenediamine and salicylaldehyde
- B01J 2531/16: Copper
- B01J 2531/26: Zinc
- B01J 2531/31: Aluminium
- B01J 2531/62: Chromium
- B01J 2531/845: Cobalt
- C07D: HETEROCYCLIC COMPOUNDS (macromolecular compounds C08)
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS

## Abstract

A catalyst which can catalyze ring-addition reaction of CO2 and an alkylene oxide at 0˜180° C. under 0.1˜8.0 MPa to produce a corresponding cyclic carbonate, and the preparation thereof. The catalyst is a conjugated microporous macromolecule polymer complexed with cobalt, chromium, zinc, copper or aluminium, and by using the macromolecule catalyst complexed with different metals to catalyze the reaction of CO2 and alkylene oxide at normal temperature and normal pressure, a yield of the corresponding cyclic carbonate of 35%-90% can be obtained. The catalyst is easy to recover and the re-use of the catalyst has no influence on the yield; additionally, the yield can reach over 90% by controlling the reaction conditions.

## Claims

### Claim 1

A metal-conjugated microporous polymer having the following structure:
wherein, R1═—H, -tBu, -iBu, —NO2, —Cl, —CH2NEt2, —CH2N(Bn)Et2Br, —CH2N(CH3)2CH2Ph,
M is Co, Cr, Zn, Cu, or Al; X═—OAc or —Cl or —Br or —I or -Et or —OMe or —OEt or —OCH2CH2(OCH2CH)2Cl, n represents degree of polymerization of the metal-conjugated microporous polymer and is in the range of 30˜100; when M is Co, R2 is not

### Claim 2 (depends on 1)

The metal-conjugated microporous polymer polymer of claim 1 wherein M is Cr.

### Claim 3 (depends on 1)

The metal-conjugated microporous polymer polymer of claim 1 wherein R2 is

### Claim 4 (depends on 1)

The metal-conjugated microporous polymer polymer of claim 1 wherein M is Co.

### Claim 5 (depends on 1)

A method for preparing the metal-conjugated microporous polymer polymer of claim 1 wherein M is Co, Cr, Zn, or Cu, and the method comprises:
synthesis of the metal-conjugated microporous polymer: with anhydrous toluene and TEA as solvent (volume ratio=3˜4:1), CuI and tetrakis-(triphenylphosphine)palladium(0) as catalyst, a mixture solution of alkynyl benzene A and Salen-M-X or Salen-M (mole ratio=1˜4:1) is stirred under argon for 60˜90 hours at 25˜100° C., affording the metal-conjugated microporous polymer, wherein the mole ratio of CuI and alkynyl benzene A is 1:5˜10 and, and the mole ratio of tetrakis-(triphenylphosphine)palladium(0) and alkynyl benzene A is 1:20˜30 .

### Claim 6 (depends on 1)

A method for preparing the metal-conjugated microporous polymer of claim 1, wherein M is Al, and the method comprises:
1) synthesis of a conjugated microporous polymer (CMP): with anhydrous toluene and TEA as solvent (volume ratio=3˜4:1), tetrakis-(triphenylphosphine)palladium(0) and CuI as catalyst, a mixture solution of alkynyl benzene A and Salen (mole ratio=1:1˜5) is stirred under argon for 60˜90 hours at 20˜150° C., affording the CMP, wherein, the mole ratio of CuI and alkynyl benzene A is 1:10˜40, and the mole ratio of or tetrakis-(triphenylphosphine)palladium(0) and alkynyl benzene A is 1:12˜50;
2) synthesis of the metal -conjugated microporous polymer: with anhydrous toluene as a solvent, a mixture solution of an aluminum compound and CMP (mass ratio=1:1˜6) is stirred for 8˜15 hours at 90˜130° C., affording the metal aluminum-conjugated microporous polymer polymer, wherein, the aluminum compound is AlCl3, AlBr3, AlEt3, Al(OMe)3, Al(OMe)3, or Al(OCH2CH2(OCH2CH)2Cl)3.

### Claim 7 (depends on 5)

The method of claim 5 wherein:
the amount of anhydrous toluene required by each 1 mmol Salen-M-X , or Salen-M is 30˜50 ml.

### Claim 8 (depends on 6)

The method of claim 6 wherein:
the mole ratio of alkynyl benzene A and Salen in step 1) is 1:1˜3; the mole ratio of tetrakis-(triphenylphosphine)palladium(0) or CuI and 1,3,5-triethynylbenzene in step 1) is 1:12˜28, and 1:10˜25 respectively;
the mass ratio of aluminum compound and CMP in step 2) is 1:1˜2.5.

### Claim 9 (depends on 6)

The method of claim 6 wherein:
the amount of anhydrous toluene required by each 1 mmol Salen in step 1) is 20˜25 ml; and
the amount of anhydrous toluene required by each 1 g CMP in step 2) is 15˜20 ml.

### Claim 10 (depends on 5)

The method of claim 5, wherein:
the alkynyl benzene A is 1,3,5-triethynylbenzene, 1,4-diethynylbenzene or tetrakis(4-ethynylphenyl)methane.

### Claim 11 (depends on 6)

The method of claim 6, wherein:
the alkynyl benzene A is 1,3,5-triethynylbenzene, 1,4-diethynylbenzene or tetrakis(4-ethynylphenyl)methane.

### Claim 12 (depends on 1)

A method of making a cyclic carbonate comprising coupling CO2 and an epoxide in the presence of the metal-conjugated microporous polymer of claim 1 as a catalyst at 0˜180° C. and 0.1˜8.0 MPa CO2 pressure.

### Claim 13 (depends on 12)

The method of claim 12, wherein:
general procedure for the catalytic reaction of CO2 and epoxides at ambient pressure and temperature: in the presence of an amine compound, a mixture solution of the metal-conjugated microporous polymer, and the epoxide (mass ratio=1:10˜50) is stirred for 12˜72 hours at ambient pressure and temperature, affording the corresponding cyclic carbonate, wherein, the mole ratio of the amine compound and epoxide is 1:10˜100, and M is not Al.

### Claim 14 (depends on 12)

The method of claim 12, wherein:
general procedure for the catalytic reaction of CO2 and epoxide at a wide range of temperature and pressure: in the presence of a amine compound, a mixture solution of the metal-conjugated microporous polymer polymer and the epoxide (mass ratio=1:10˜50) is stirred for 1˜6 hours at 50˜160° C. and 2˜8 MPa CO2 pressure, affording the corresponding cyclic carbonate, wherein, the mole ratio of the amine compound and epoxide is 1:10˜100, and M is not Al.

### Claim 15 (depends on 12)

The method of claim 12, wherein:
M is Al, general procedure to catalyze reaction of CO2 and the epoxide: in the presence of an amine compound, a mixture solution of the metal-conjugated microporous polymer and epoxide (mass ratio =1:1˜25) is stirred for 3˜80 hours at 0˜160° C., affording the corresponding cyclic carbonate, wherein, the mole ratio of the amine compound and epoxide is 1:5˜1000.

### Claim 16 (depends on 15)

The method of claim 15, wherein, the mole ratio of the amine compound and epoxide is 1:900.

### Claim 17 (depends on 12)

The method of of claim 12, wherein the reaction is conducted in the presence of an amine compound selected from the group consisting of quaternary ammonium salts, triethylamine (TEA), dimethylaminopyridine (DMAP), and mixtures thereof.

### Claim 18 (depends on 12)

The method of claim 12, wherein the epoxide is selected from the group consisting of propylene oxide, epichlorohydrin, 2-ethyloxirane, 2-butyloxirane, 2-phenyloxirane, and mixtures thereof.