# US 2016/0251303 A1 · Crystalline organic-inorganic halide perovskite thin films and methods of preparation

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0251303 A1
- Document ID: US20160251303A1
- Status: Published application
- Kind: A1
- Application number: 15/054,988
- Filed: 2016-02-26
- Published: 2016-09-01
- Earliest claimed: 2015-02-27
- Assignees: Cornell University
- Applicants: Cornell University
- Inventors: David T. MOORE; Hiroaki SAI; Kwan Wee TAN; Lara A. Estroff; Ulrich B. Wiesner
- Web page: https://patentgrep.com/patent/US20160251303A1

## CPC

- B05D 1/005: {Spin coating}
- B05D 3/007: {After-treatment}
- C23C 18/1204: {inorganic material, e.g. non-oxide and non-metallic such as sulfides, nitrides based compounds}
- C23C 18/1245: {Inorganic substrates other than metallic}
- C23C 18/1291: {by heating of the substrate}
- H10K 30/10: comprising heterojunctions between organic semiconductors and inorganic semiconductors
- H10K 85/50: Organic perovskites; Hybrid organic-inorganic perovskites [HOIP], e.g. CH3NH3PbI3
- B05D 3/0254: {After-treatment}
- H10K 30/50: Photovoltaic [PV] devices
- Y02P 20/54: using solvents, e.g. supercritical solvents or ionic liquids
- B05D: PROCESSES FOR APPLYING FLUENT MATERIALS TO SURFACES, IN GENERAL (conveying articles or workpieces through baths of liquid B65G, e.g. B65G49/02)
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H10K: ORGANIC ELECTRIC SOLID-STATE DEVICES
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A film comprising a crystalline halide perovskite composition having the following formula: AMX3 (1) wherein: A is an organic cation selected from the group consisting of methylammonium, tetramethylammonium, formamidinium, and guanidinium; M is at least one divalent metal; and X is independently selected from halide atoms; wherein the crystalline film of the halide perovskite composition possesses at least one of an average grain size of at least 30 microns, substantial crystal orientation evidenced in an ordering parameter of at least 0.6, and a level of crystallinity of at least 90%. Methods for producing films of these halide perovskite compositions using ionic liquids instead of volatile organic solvents are also described herein.

## Claims

### Claim 1

A film comprising a crystalline halide perovskite composition having the following formula:
AMX3 (1)
wherein:
A is an organic cation selected from the group consisting of methylammonium, tetramethylammonium, formamidinium, and guanidinium;
M is at least one divalent metal; and
X is independently selected from halide atoms;
wherein the crystalline film of the halide perovskite composition possesses at least one of an average grain size of at least 30 microns, substantial crystal orientation evidenced in an ordering parameter of at least 0.6, and a level of crystallinity of at least 90%.

### Claim 2 (depends on 1)

The film of claim 1, wherein the film of the crystalline halide perovskite composition possesses an average grain size of at least 30 microns.

### Claim 3 (depends on 1)

The film of claim 1, wherein the film of the crystalline halide perovskite composition possesses an average grain size of at least 50 microns.

### Claim 4 (depends on 1)

The film of claim 1, wherein the film of the crystalline halide perovskite composition possesses an average grain size of at least 100 microns.

### Claim 5 (depends on 1)

The film of claim 1, wherein the at least one divalent metal is selected from lead, tin, and germanium.

### Claim 6 (depends on 1)

The film of claim 1, wherein the film has a thickness of at least 200 nm.

### Claim 7

A method for producing a film of a crystalline halide perovskite composition, the method comprising:
i) forming a film of a perovskite precursor solution onto a substrate, the perovskite precursor solution comprising a) a metal-containing compound of the formula MX′2, where M is at least one divalent metal and X′ is a monovalent anion; b) an organic salt of the formula AX, wherein A is selected from methylammonium, tetramethylammonium, formamidinium, and guanidinium, and X is independently selected from halide atoms; and c) an ionic liquid; wherein components a) and b) are dissolved in component c); and
ii) annealing the film of the perovskite precursor solution at a temperature of at least 30° C. for a time period effective to convert perovskite precursor components in the perovskite precursor solution to a film of a crystalline halide perovskite composition having the following formula:
AMX3 (1)
wherein A, M, and X are as defined above.

### Claim 8 (depends on 7)

The method of claim 7, wherein the at least one divalent metal (M) is selected from lead, tin, and germanium.

### Claim 9 (depends on 7)

The method of claim 7, wherein the film of the crystalline halide perovskite composition has a thickness of at least 200 nm.

### Claim 10 (depends on 7)

The method of claim 7, wherein the ionic liquid is selected from the group consisting of an alkylammonium ionic liquid, formamidinium ionic liquid, and guanidinium ionic liquid.

### Claim 11 (depends on 7)

The method of claim 7, wherein the ionic liquid possesses a cation that is equivalent to the cation A in the organic salt.

### Claim 12 (depends on 7)

The method of claim 7, wherein the ionic liquid possesses an anion other than halide.

### Claim 13 (depends on 7)

The method of claim 7, wherein the ionic liquid possesses a carbon-containing anion.

### Claim 14 (depends on 7)

The method of claim 7, wherein MX′2 and AX in the precursor are present in a relative amount such that the ratio of M:X is about 1:3.

### Claim 15 (depends on 7)

The method of claim 7, wherein a temperature of at least 30° C. and up to 150° C. is used in the annealing step (ii).

### Claim 16 (depends on 7)

The method of claim 7, wherein the crystalline film of the halide perovskite composition possesses at least one of an average grain size of at least 30 microns, substantial crystal orientation evidenced in an ordering parameter of at least 0.6, and a level of crystallinity of at least 90%.

### Claim 17 (depends on 7)

The method of claim 7, wherein the film of the crystalline halide perovskite composition possesses an average grain size of at least 30 microns.

### Claim 18 (depends on 7)

The method of claim 7, wherein the film of the crystalline halide perovskite composition possesses an average grain size of at least 50 microns.

### Claim 19 (depends on 7)

The method of claim 7, wherein the film of the crystalline halide perovskite composition possesses an average grain size of at least 100 microns.

### Claim 20 (depends on 7)

The method of claim 7, further comprising removing the ionic liquid by rinsing said film of the crystalline halide perovskite composition with a solvent in which the ionic liquid is soluble.