# US 2016/0251265 A1 · Corrosion-resistant member and electrostatic chuck device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0251265 A1
- Document ID: US20160251265A1
- Status: Published application
- Kind: A1
- Application number: 15/027,339
- Filed: 2014-10-15
- Published: 2016-09-01
- Earliest claimed: 2013-10-15
- Assignees: Sumitomo Osaka Cement Co., Ltd.
- Applicants: Sumitomo Osaka Cement Co., Ltd.
- Inventors: Kentaro Takahashi; Yoshiaki Moriya; Megumi Ootomo
- Web page: https://patentgrep.com/patent/US20160251265A1

## CPC

- C04B 35/44: based on aluminates
- C04B 35/6261: {Milling}
- C04B 35/6262: {of calcined, sintered clinker or ceramics}
- C04B 35/62655: {Drying, e.g. freeze-drying, spray-drying, microwave or supercritical drying}
- C04B 35/62675: {characterised by the treatment temperature}
- C04B 35/645: Pressure sintering
- H02N 13/00: Clutches or holding devices using electrostatic attraction, e.g. using Johnson-Rahbek effect
- H05K 7/2039: {characterised by the heat transfer by conduction from the heat generating element to a dissipating body (arrangements for increasing/decreasing heat-transfer, e.g. fins details, F28F13/00)}
- H10P 72/72: using electrostatic chucks
- H10P 72/722: {Details of electrostatic chucks}
- H10P 72/7616: {characterised by a coating, a hardness or a material}
- C04B 2235/3217: Aluminum oxide or oxide forming salts thereof, e.g. bauxite, alpha-alumina
- C04B 2235/3222: Aluminates other than alumino-silicates, e.g. spinel (MgAl2O4)
- C04B 2235/3224: Rare earth oxide or oxide forming salts thereof, e.g. scandium oxide
- C04B 2235/3225: Yttrium oxide or oxide-forming salts thereof
- C04B 2235/3227: Lanthanum oxide or oxide-forming salts thereof
- C04B 2235/5436: micrometer sized, i.e. from 1 to 100 micron
- C04B 2235/5445: submicron sized, i.e. from 0,1 to 1 micron
- C04B 2235/761: Unit-cell parameters, e.g. lattice constants
- C04B 2235/764: Garnet structure A3B2(CO4)3
- C04B 2235/768: Perovskite structure ABO3
- C04B 2235/77: Density
- C04B 2235/9669: Resistance against chemicals, e.g. against molten glass or molten salts
- C04B 2235/9684: Oxidation resistance
- C04B 2235/9692: Acid, alkali or halogen resistance
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- H02N: ELECTRIC MACHINES NOT OTHERWISE PROVIDED FOR
- H05K: PRINTED CIRCUITS; CASINGS OR CONSTRUCTIONAL DETAILS OF ELECTRIC APPARATUS; MANUFACTURE OF ASSEMBLAGES OF ELECTRICAL COMPONENTS
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

Provided are a corrosion-resistant member and an electrostatic chuck device using the same, in which corrosion resistance to halogen corrosive gas such as fluorine corrosive gas or chlorine corrosive gas and plasma thereof is high, dielectric constant and volume resistivity are high, and dielectric loss is low. The corrosion-resistant member is formed of a composite oxide sintered compact containing aluminum, samarium, and a rare earth metal element other than samarium, in which the rare earth metal element other than samarium has an ionic radius of 0.88×10−10 m or more.

## Claims

### Claim 1

A corrosion-resistant member comprising
a composite oxide sintered compact containing aluminum, samarium, and a rare earth metal element other than samarium,
wherein the rare earth metal element other than samarium has an ionic radius of 0.88×10−10 m or more.

### Claim 2 (depends on 1)

The corrosion-resistant member according to claim 1,
wherein a ratio (NRE/(NSM+NRE)) of the number of atoms of the rare earth metal element other than samarium (NRE) to the sum (NSM+NRE) of the number of atoms of samarium (NSM) and the number of atoms of the rare earth metal element other than samarium (NRE) in the composite oxide is 0.01 or higher and 0.5 or lower.

### Claim 3 (depends on 1)

The corrosion-resistant member according to claim 1,
wherein the rare earth metal element other than samarium is one element or two or more elements selected from the group consisting of yttrium, lanthanum, praseodymium, neodymium, europium, gadolinium, terbium, dysprosium, holmium, erbium, and thulium.

### Claim 4 (depends on 1)

The corrosion-resistant member according to claim 1,
wherein a crystal phase of the composite oxide sintered compact is an orthorhombic perovskite phase.

### Claim 5 (depends on 1)

The corrosion-resistant member according to claim 1,
wherein a dielectric constant at a frequency of 1 MHz or lower is 13 or higher,
a dielectric loss at a frequency of 1 MHz or lower is 0.2 or lower, and
volume resistivity is 1×1014 Ω·cm or higher.

### Claim 6 (depends on 1)

An electrostatic chuck device comprising:
a ceramic plate-shaped body that has a first main surface which is a placement surface on which a sample is placed; and
an internal electrode for electrostatic adsorption that is provided on a second main surface of the ceramic plate-shaped body,
wherein the ceramic plate-shaped body is formed of the corrosion-resistant member according to claim 1.

### Claim 7 (depends on 6)

The electrostatic chuck device according to claim 6, further comprising:
a cooling base portion that cools the ceramic plate-shaped body and the internal electrode for electrostatic adsorption; and
a heating member that is provided between the internal electrode for electrostatic adsorption and the cooling base portion.