# US 2016/0251256 A1 · Ion exchangeable soft glasses for three-dimensional shapes

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0251256 A1
- Document ID: US20160251256A1
- Status: Published application
- Kind: A1
- Application number: 15/052,971
- Filed: 2016-02-25
- Published: 2016-09-01
- Earliest claimed: 2015-02-26
- Assignees: Corning Incorporated
- Applicants: Corning Incorporated
- Inventors: MARIE JACQUELINE MONIQUE COMTE; Robert Michael Morena; Charlene Marie Smith
- Web page: https://patentgrep.com/patent/US20160251256A1

## CPC

- C03C 3/097: containing phosphorus, niobium or tantalum
- B32B 17/00: Layered products essentially comprising sheet glass, or glass, slag, or like fibres
- C03C 3/085: containing an oxide of a divalent metal
- C03C 3/093: containing zinc or zirconium
- C03C 4/18: for ion-sensitive glass
- C03C 21/002: {to perform ion-exchange between alkali ions (C03C21/005 takes precedence)}
- B32B 2250/02: 2 layers
- B32B 2457/20: Displays, e.g. liquid crystal displays, plasma displays
- C03C 2204/00: Glasses, glazes or enamels with special properties
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM

## Abstract

Ion exchangeable alkali aluminosilicate glasses and glass articles having softening points and high temperature coefficients of thermal expansion that permit the glass to be formed into three-dimensional shapes by the vacuum sagging process are provided. These glasses contain significant amounts of at least one of MgO and ZnO and comprise B2O3 and less than 1 mol % Li2O.

## Claims

### Claim 1

An alkali aluminosilicate glass, the alkali aluminosilicate glass comprising from about 0.5 mol % to about 4 mol % B2O3, less than 1 mol % Li2O, and from about 1 mol % to about 7 mol % ZnO, wherein the alkali aluminosilicate glass has a softening point of about 790° C. or less and a high temperature coefficient of thermal expansion of about 35×10−6/K or less, and wherein the alkali aluminosilicate glass is formable into a three-dimensional non-planar shape and is ion exchangeable.

### Claim 2 (depends on 1)

The alkali aluminosilicate glass of claim 1, wherein the alkali aluminosilicate glass is chemically strengthened and has a compressive layer extending to a depth of layer of at least about 40 μm from at least one surface of the alkali aluminosilicate glass into the alkali aluminosilicate glass, the compressive layer having a maximum compressive stress of at least about 600 MPa.

### Claim 3 (depends on 2)

The alkali aluminosilicate glass of claim 2, wherein the depth of layer is at least about 50 μm.

### Claim 4 (depends on 2)

The alkali aluminosilicate glass of claim 2, wherein the maximum compressive stress is at least about 750 MPa.

### Claim 5 (depends on 2)

The alkali aluminosilicate glass of claim 2, wherein the alkali aluminosilicate glass is ion exchanged for ten hours or less in a single ion exchange bath.

### Claim 6 (depends on 2)

The alkali aluminosilicate glass of claim 2, wherein the alkali aluminosilicate glass comprises at least a portion of a cover glass or a housing of a consumer electronic product.

### Claim 7 (depends on 6)

The alkali aluminosilicate glass of claim 6, wherein at least one of the cover glass and the housing has a thickness from about 0.25 mm to about 2.0 mm.

### Claim 8 (depends on 1)

The alkali aluminosilicate glass of claim 1, wherein the alkali aluminosilicate glass comprises: from about 62 mol % to about 70 mol % SiO2; from about 5 mol % to about 11 mol % Al2O3; from about 0.5 mol % to about 4 mol % B2O3; from 0 mol % to about 1 mol % Li2O; from about 13 mol % to about 19 mol % Na2O;
from about 0.3 mol % to about 4 mol % K2O; from 0 mol % to about 6 mol % MgO; and
from about 1 mol % to about 7 mol % ZnO.

### Claim 9 (depends on 8)

The alkali aluminosilicate glass of claim 8, wherein the alkali aluminosilicate glass comprises: from about 64 mol % to about 67 mol % SiO2; from about 5 mol % to about 10 mol % Al2O3; 0 mol % Li2O; from about 13 mol % to about 17 mol % Na2O; and from about 1 mol % to about 4 mol % K2O.

### Claim 10 (depends on 9)

The alkali aluminosilicate glass of claim 9, wherein the alkali aluminosilicate glass comprises from about 4 mol % to about 7 mol % ZnO.

### Claim 11 (depends on 8)

The alkali aluminosilicate glass of claim 8, wherein the alkali aluminosilicate glass comprises from about 0.5 mol % to about 2.5 mol % B2O3 and from about 15 mol % to about 19 mol % Na2O.

### Claim 12 (depends on 8)

The alkali aluminosilicate glass of claim 8, further comprising at least one of from 0 mol % to about 3 mol % P2O5 and from 0 mol % to about 4 mol % ZrO2.

### Claim 13 (depends on 8)

The alkali aluminosilicate glass of claim 8, wherein the alkali aluminosilicate glass further comprises up to about 0.5 mol % of at least one of SnO2 and Sb2O3.

### Claim 14 (depends on 1)

The alkali aluminosilicate glass of claim 1, wherein R2O(mol %)/Al2O3(mol %)≧1.5, where R2O=(Li2O+Na2O+K2O+Rb2O+Cs2O).

### Claim 15 (depends on 1)

The alkali aluminosilicate glass of claim 1, wherein Al2O3(mol %)≧B2O3(mol %).

### Claim 16 (depends on 1)

The alkali aluminosilicate glass of claim 1, wherein the alkali aluminosilicate glass has a 200 poise temperature T200 of 1620° C. or less.

### Claim 17 (depends on 1)

The alkali aluminosilicate glass of claim 1, wherein the alkali aluminosilicate glass has a liquidus viscosity of at least 150 kP.

### Claim 18 (depends on 1)

The alkali aluminosilicate glass of claim 1, wherein the alkali aluminosilicate glass has a zircon breakdown viscosity of less than 30 kP.

### Claim 19

A alkali aluminosilicate alkali aluminosilicate glass, the alkali aluminosilicate glass comprising: from about 62 mol % to about 70 mol % SiO2; from about 5 mol % to about 11 mol % Al2O3; from about 0.5 mol % to about 4 mol % B2O3; from 0 mol % to about 1 mol % Li2O; from about 13 mol % to about 19 mol % Na2O; from about 0.3 mol % to about 4 mol % K2O; from 0 mol % to about 6 mol % MgO; and
from about 1 mol % to about 7 mol % ZnO, the alkali aluminosilicate glass having a softening point of about 790° C. or less and a high temperature coefficient of thermal expansion of about 35×10−6/K or less.

### Claim 20 (depends on 19)

The alkali aluminosilicate glass of claim 19, wherein the alkali aluminosilicate glass comprises: from about 64 mol % to about 67 mol % SiO2; from about 5 mol % to about 10 mol % Al2O3; 0 mol % Li2O; from about 13 mol % to about 17 mol % Na2O; and from about 1 mol % to about 4 mol % K2O.

### Claim 21 (depends on 19)

The alkali aluminosilicate glass of claim 19, wherein the alkali aluminosilicate glass comprises from about 4 mol % to about 7 mol % ZnO.

### Claim 22 (depends on 19)

The alkali aluminosilicate glass of claim 19, wherein the alkali aluminosilicate glass comprises from about 0.5 mol % to about 2.5 mol % B2O3 and from about 15 mol % to about 19 mol % Na2O.

### Claim 23 (depends on 19)

The alkali aluminosilicate glass of claim 19, further comprising at least one of from 0 mol % to about 3 mol % P2O5 and from 0 mol % to about 4 mol % ZrO2.

### Claim 24 (depends on 19)

The alkali aluminosilicate glass of claim 19, wherein the alkali aluminosilicate glass further comprises up to about 0.5 mol % of at least one of SnO2 and Sb2O3.

### Claim 25 (depends on 19)

The alkali aluminosilicate glass of claim 19, wherein R2O(mol %)/Al2O3(mol %)≧1.5, where R2O=(Li2O+Na2O+K2O+Rb2O+Cs2O).

### Claim 26 (depends on 19)

The alkali aluminosilicate glass of claim 19, wherein Al2O3(mol %)≧B2O3(mol %).

### Claim 27 (depends on 19)

The alkali aluminosilicate glass of claim 19, wherein the alkali aluminosilicate glass is chemically strengthened and has a compressive layer extending to a depth of layer of at least about 40 μm from at least one surface of the alkali aluminosilicate glass into the alkali aluminosilicate glass, the compressive layer having a maximum compressive stress of at least about 600 MPa.

### Claim 28 (depends on 27)

The alkali aluminosilicate glass of claim 27, wherein the depth of layer is at least about 50 μm.

### Claim 29 (depends on 27)

The alkali aluminosilicate glass of claim 27, wherein the maximum compressive stress is at least about 750 MPa.

### Claim 30 (depends on 27)

The alkali aluminosilicate glass of claim 27, wherein the alkali aluminosilicate glass is ion exchanged for ten hours or less in a single ion exchange bath.

### Claim 31 (depends on 27)

The alkali aluminosilicate glass of claim 27, wherein the alkali aluminosilicate glass comprises at least a portion of a cover glass or a housing of consumer electronic product.

### Claim 32 (depends on 27)

The alkali aluminosilicate glass of claim 27, wherein at least one of the cover glass and the housing has a thickness from about 0.25 mm to about 1.0 mm.

### Claim 33 (depends on 19)

The alkali aluminosilicate glass of claim 19, wherein the alkali aluminosilicate glass has a 200 poise temperature T200 of 1620° C. or less.

### Claim 34 (depends on 19)

The alkali aluminosilicate glass of claim 19, wherein the alkali aluminosilicate glass has a liquidus viscosity of at least 150 kP.

### Claim 35 (depends on 19)

The alkali aluminosilicate glass of claim 19, wherein the alkali aluminosilicate glass has a zircon breakdown viscosity of less than 30 kP.

### Claim 36 (depends on 19)

The alkali aluminosilicate glass of claim 19, wherein the alkali aluminosilicate glass is formable into a three-dimensional non-planar shape.