# US 2016/0251255 A1 · Fast ion-exchangeable boron-free glasses with low softening point

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0251255 A1
- Document ID: US20160251255A1
- Status: Published application
- Kind: A1
- Application number: 15/040,502
- Filed: 2016-02-10
- Published: 2016-09-01
- Earliest claimed: 2015-02-26
- Assignees: Corning Incorporated
- Applicants: Corning Incorporated
- Inventors: Timothy Michael Gross; John Christopher Mauro; Yihong Mauro; Rohit Rai; Adama Tandia; Zhongzhi Tang
- Web page: https://patentgrep.com/patent/US20160251255A1

## CPC

- C03C 3/097: containing phosphorus, niobium or tantalum
- B32B 17/06: comprising glass as the main or only constituent of a layer, next to another layer of a specific {material}
- C03C 21/002: {to perform ion-exchange between alkali ions (C03C21/005 takes precedence)}
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM

## Abstract

Alkali aluminosilicate glasses that exhibit fast ion exchange performance and having low softening points that enable the glasses to be formed into non-planar, three-dimensional shapes. The glasses contain less than about 1 mol % of boron oxide and, in some embodiments, are substantially free of B2O3. Furthermore, these glasses have excess amounts of alkali oxides relative to both Al2O3 and P2O5, in order to improve melting behavior and ion exchange performance while still achieving sufficiently low softening points to allow for formability.

## Claims

### Claim 1

An alkali aluminosilicate glass, the alkali aluminosilicate glass comprising: from 0 mol % to about 1 mol % B2O3, and Na2O, the alkali aluminosilicate glass having a softening point of about 900° C. or less, wherein 1.3≦R2O(mol %)/Al2O3(mol %)≦2.2, where R2O=(Li2O(mol %)+Na2O(mol %)+K2O(mol %)+Rb2O(mol %)+Cs2O(mol %)).

### Claim 2 (depends on 1)

The alkali aluminosilicate glass of claim 1, wherein the alkali aluminosilicate glass is boron-free.

### Claim 3 (depends on 1)

The alkali aluminosilicate glass of claim 1, wherein 5 mol %≦R2O(mol %)−Al2O3(mol %)≦12 mol %.

### Claim 4 (depends on 3)

The alkali aluminosilicate glass of claim 3, wherein 5 mol %≦Na2O(mol %)+K2O(mol %)−Al2O3(mol %)≦12 mol %.

### Claim 5 (depends on 1)

The alkali aluminosilicate glass of claim 1, wherein the alkali aluminosilicate glass comprises: from about 50 mol % to about 70 mol % SiO2; from about 10 mol % to about 15 mol % Al2O3; from 0 mol % to about 1 mol % B2O3; from 0 mol % to about 5 mol % P2O5; from about 18 mol % to about 22 mol % Na2O; from 0 mol % to about 3 mol % K2O; from 0 mol % to about 4 mol % MgO; from 0 mol % to about 1 mol % CaO;
and from 0 mol % to about 8 mol % ZnO.

### Claim 6 (depends on 5)

The alkali aluminosilicate glass of claim 5, wherein the alkali aluminosilicate glass comprises: from about 55 mol % to about 66 mol % SiO2; from about 10 mol % to about 14 mol % Al2O3; from 0 mol % to about 0.5 mol % B2O3; from 0 mol % to about 5 mol % P2O5; from about 19 mol % to about 21 mol % Na2O; from 0 mol % to about 2 mol % K2O; from 0 mol % to about 2 mol % MgO; from 0 mol % to about 0.5 mol % CaO; and from about 1 mol % to about 7 mol % ZnO.

### Claim 7 (depends on 6)

The alkali aluminosilicate glass of claim 6, wherein 5 mol % Na2O(mol %)+K2O(mol %)−Al2O3(mol %)≦10 mol %.

### Claim 8 (depends on 6)

The alkali aluminosilicate glass of claim 6, wherein K2O(mol %)≦0.5(Na2O(mol %)+K2O(mol %)).

### Claim 9 (depends on 6)

The alkali aluminosilicate glass of claim 6, wherein 1.3≦(Na2O(mol %)+K2O(mol %))/Al2O3(mol %)≦2.0.

### Claim 10 (depends on 6)

The alkali aluminosilicate glass of claim 6, wherein the alkali aluminosilicate glass comprises: from about 56 mol % to about 62 mol % SiO2; from about 11 mol % to about 14 mol % Al2O3; from about 1 mol % to about 5 mol % P2O5; from about 19 mol % to about 20 mol % Na2O; from 0 mol % to about 2 mol % K2O; from 0 mol % to about 4 mol % MgO; from 0 mol % to about 0.2 mol % CaO; and from about 2 mol % to about 7 mol % ZnO, wherein 5 mol % Na2O(mol %)+K2O(mol %)−Al2O3(mol %)≦9 mol %.

### Claim 11 (depends on 12)

The alkali aluminosilicate glass of claim 12, wherein 1.4≦(Na2O(mol %)+K2O(mol %))/Al2O3(mol %)≦1.8.

### Claim 12 (depends on 1)

The alkali aluminosilicate glass of claim 1, wherein the alkali aluminosilicate glass is ion exchanged and has a compressive layer extending to a depth of layer of at least about 40 μm from at least one surface of the alkali aluminosilicate glass into the alkali aluminosilicate glass and having a maximum compressive stress of at least about 600 MPa.

### Claim 13 (depends on 12)

The alkali aluminosilicate glass of claim 12, wherein the alkali aluminosilicate glass is ion exchanged for seven hours or less in a single ion exchange bath.

### Claim 14 (depends on 13)

The alkali aluminosilicate glass of claim 13, wherein, after being ion exchanged in the first ion exchange bath, the first ion exchange bath having a first composition, the alkali aluminosilicate glass is ion exchanged in a second ion exchange bath, the second ion exchange bath having a second composition that is different from the first composition.

### Claim 15 (depends on 14)

The alkali aluminosilicate glass of claim 14, wherein the maximum compressive stress is at least about 600 MPa after the alkali aluminosilicate glass is ion exchanged in the second ion exchange bath.

### Claim 16 (depends on 1)

The alkali aluminosilicate glass of claim 1, wherein the alkali aluminosilicate glass comprises at least a portion of a cover glass or a housing of a consumer electronic product.

### Claim 17 (depends on 16)

The alkali aluminosilicate glass of claim 16, wherein at least one of the cover glass and the housing has a thickness from about 0.25 mm to about 1.0 mm.

### Claim 18 (depends on 1)

The alkali aluminosilicate glass of claim 1, wherein the alkali aluminosilicate glass is formable into a three-dimensional non-planar article.

### Claim 19

An alkali aluminosilicate glass comprising: from about 50 mol % to about 70 mol % SiO2; from about 10 mol % to about 15 mol % Al2O3; from 0 mol % to about 1 mol % B2O3; from 0 mol % to about 5 mol % P2O5; from about 18 mol % to about 22 mol % Na2O; from 0 mol % to about 3 mol % K2O; from 0 mol % to about 4 mol % MgO; from 0 mol % to about 1 mol % CaO; and from 0 mol % to about 8 mol % ZnO, wherein 1.3≦(Na2O(mol %)+K2O(mol %))/Al2O3(mol %)≦2.0, wherein the alkali aluminosilicate glass has a softening point of about 900° C. or less, and wherein 1.3≦R2O(mol %)/Al2O3(mol %)≦2.2, where R2O=(Li2O(mol %)+Na2O(mol %)+K2O(mol %)+Rb2O(mol %)+Cs2O(mol %)).

### Claim 20 (depends on 19)

The alkali aluminosilicate glass of claim 19, wherein the alkali aluminosilicate glass is boron-free.

### Claim 21 (depends on 19)

The alkali aluminosilicate glass of claim 19, wherein 5 mol %≦R2O(mol %)−Al2O3(mol %)≦12 mol %.

### Claim 22 (depends on 19)

The alkali aluminosilicate glass of claim 19, wherein the alkali aluminosilicate glass comprises: from about 55 mol % to about 66 mol % SiO2; from about 10 mol % to about 14 mol % Al2O3; from 0 mol % to about 0.5 mol % B2O3; from 0 mol % to about 5 mol % P2O5; from about 19 mol % to about 21 mol % Na2O; from 0 mol % to about 2 mol % K2O; from 0 mol % to about 2 mol % MgO; from 0 mol % to about 0.5 mol % CaO; and from about 1 mol % to about 7 mol % ZnO, wherein the alkali aluminosilicate glass has a softening point of about 900° C. or less.

### Claim 23 (depends on 19)

The alkali aluminosilicate glass of claim 19, wherein 5 mol %≦Na2O(mol %)+K2O(mol %)−Al2O3(mol %)≦10 mol %.

### Claim 24 (depends on 19)

The alkali aluminosilicate glass of claim 19, wherein K2O(mol %)≦0.5(Na2O(mol %)+K2O(mol %)).

### Claim 25 (depends on 19)

The alkali aluminosilicate glass of claim 19, wherein 1.3≦(Na2O(mol %)+K2O(mol %))/Al2O3(mol %)≦2.0.

### Claim 26 (depends on 19)

The alkali aluminosilicate glass of claim 19, wherein the alkali aluminosilicate glass comprises: from about 56 mol % to about 62 mol % SiO2; from about 11 mol % to about 14 mol % Al2O3; from about 1 mol % to about 5 mol % P2O5; from about 19 mol % to about 20 mol % Na2O; from 0 mol % to about 2 mol % K2O; from 0 mol % to about 4 mol % MgO; from 0 mol % to about 0.2 mol % CaO; and from about 2 mol % to about 7 mol % ZnO, wherein 5 mol %≦Na2O(mol %)+K2O(mol %)−Al2O3(mol %)≦9 mol %.

### Claim 27 (depends on 26)

The alkali aluminosilicate glass of claim 26, wherein 1.4≦(Na2O(mol %)+K2O(mol %))/Al2O3(mol %)≦1.8.

### Claim 28 (depends on 19)

The alkali aluminosilicate glass of claim 19, wherein the alkali aluminosilicate glass is ion exchanged and has a compressive layer extending to a depth of layer of at least about 40 μm from at least one surface of the alkali aluminosilicate glass into the alkali aluminosilicate glass and having a maximum compressive stress of at least about 600 MPa.

### Claim 29 (depends on 28)

The alkali aluminosilicate glass of claim 28, wherein the alkali aluminosilicate glass is ion exchanged for seven hours or less in a single ion exchange bath.

### Claim 30 (depends on 28)

The alkali aluminosilicate glass of claim 28, wherein, after being ion exchanged in the first ion exchange bath, the first ion exchange bath having a first composition, the alkali aluminosilicate glass is ion exchanged in a second ion exchange bath, wherein the second ion exchange bath having a second composition that is different from the first composition.

### Claim 31 (depends on 30)

The alkali aluminosilicate glass of claim 30, wherein the maximum compressive stress is at least about 600 MPa after the alkali aluminosilicate glass is ion exchanged in the second ion exchange bath.

### Claim 32 (depends on 19)

The alkali aluminosilicate glass of claim 19, wherein the alkali aluminosilicate glass comprises at least a portion of a cover glass or a housing of a consumer electronic product.

### Claim 33 (depends on 19)

The alkali aluminosilicate glass of claim 19, wherein at least one of the cover glass and the housing has a thickness from about 0.25 mm to about 1.0 mm.

### Claim 34 (depends on 19)

The alkali aluminosilicate glass of claim 19, wherein the alkali aluminosilicate glass is formable into a three-dimensional non-planar article.