# US 2016/0251252 A1 · Nanoparticle additives for silica soot compacts and methods for strengthening silica soot compacts

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0251252 A1
- Document ID: US20160251252A1
- Status: Published application
- Kind: A1
- Application number: 15/052,309
- Filed: 2016-02-24
- Published: 2016-09-01
- Earliest claimed: 2015-02-27
- Assignees: Corning Incorporated
- Applicants: Corning Incorporated
- Inventors: Joel Edward Clinton; Yunfeng Gu; Ji Wang
- Web page: https://patentgrep.com/patent/US20160251252A1

## CPC

- C03B 37/01282: {by pressing or sintering, e.g. hot-pressing}
- C03B 19/066: {for the production of quartz or fused silica articles (other processes specially adapted for the production of quartz or fused silica articles C03B20/00)}
- C03B: MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES

## Abstract

A method of strengthening a silica soot compact is provided. The method includes forming a mixture of silica soot particles and nanoparticles, and forming a silica soot compact from the mixture.

## Claims

### Claim 1

A method of strengthening a silica soot compact, the method comprising:
forming a mixture of silica soot particles and nanoparticles; and
forming a silica soot compact from the mixture.

### Claim 2 (depends on 1)

The method of claim 1, comprising forming a mixture of silica soot particles and nanoparticles in the absence of a solvent.

### Claim 3 (depends on 1)

The method of claim 1, further comprising humidifying at least one of the nanoparticles, the silica soot particles, and the mixture of silica soot particles and nanoparticles.

### Claim 4 (depends on 1)

The method of claim 1, further comprising sintering the silica soot compact.

### Claim 5 (depends on 1)

The method of claim 1, wherein the nanoparticles are hydrophilic.

### Claim 6 (depends on 1)

The method of claim 1, wherein the nanoparticles are selected from the group consisting of silica, germanium oxide, gallium oxide, antimony oxide, arsenic oxide, bismuth oxide, indium oxide, lead oxide, phosphorus oxide, tantalum oxide, tellurium oxide, tin oxide, titanium oxide, selenium oxide, and mixtures thereof.

### Claim 7 (depends on 1)

The method of claim 1, wherein the nanoparticles have a particle size of between about 1.0 nm and about 100 nm.

### Claim 8 (depends on 1)

The method of claim 1, wherein the soot particles have a particle size of between about 0.05 micron and about 0.4 micron with an average particle size of about 0.2 micron.

### Claim 9 (depends on 1)

The method of claim 1, wherein the soot particles have a particulate surface area of greater than about 15 m2/g.

### Claim 10 (depends on 1)

The method of claim 1, wherein the mixture of silica soot particles and nanoparticles has a bulk density of less than about 0.30 g/cm3.

### Claim 11 (depends on 1)

The method of claim 1, wherein the silica soot compact has a density of less than about 1.20 g/cm3.

### Claim 12 (depends on 1)

The method of claim 1, wherein forming a silica soot compact comprises pressing the silica soot particles over an outer layer of a substrate to form at least a portion of an optical fiber preform.

### Claim 13

A method of forming a cladding portion of an optical fiber preform, the method comprising:
positioning a partially manufactured optical fiber preform in an inner cavity of a mold body;
contacting silica soot particles with nanoparticles;
after contacting the silica soot particles with the nanoparticles, loading the mold body with the silica soot particles; and
compressing the silica soot particles in a radial direction to form a silica soot compact.

### Claim 14 (depends on 13)

The method of claim 13, comprising contacting silica soot particles with nanoparticles in the absence of a solvent.

### Claim 15 (depends on 13)

The method of claim 13, further comprising humidifying at least one of the nanoparticles, the silica soot particles, and the mixture of silica soot particles and nanoparticles.

### Claim 16 (depends on 13)

The method of claim 13, wherein the nanoparticles are hydrophilic.

### Claim 17 (depends on 13)

The method of claim 13, wherein the nanoparticles are selected from a group consisting of silica, germanium oxide, gallium oxide, antimony oxide, arsenic oxide, bismuth oxide, indium oxide, lead oxide, phosphorus oxide, tantalum oxide, tellurium oxide, tin oxide, titanium oxide, selenium oxide, and mixtures thereof.

### Claim 18 (depends on 13)

The method of claim 13, wherein the nanoparticles have a particle size of between about 1.0 nm and about 100 nm.

### Claim 19 (depends on 13)

The method of claim 13, wherein the soot particles have a particle size of between about 0.05 micron and about 0.4 micron with an average particle size of about 0.2 micron.

### Claim 20 (depends on 13)

The method of claim 13, wherein the soot particles have a particulate surface area of greater than about 15 m2/g.