# US 2016/0250867 A1 · Recording method, recorded matter, recorded matter processing method, and method for improving fold-crack resistance of recorded matter

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0250867 A1
- Document ID: US20160250867A1
- Status: Published application
- Kind: A1
- Application number: 15/052,589
- Filed: 2016-02-24
- Published: 2016-09-01
- Earliest claimed: 2015-02-26
- Assignees: Canon Kabushiki Kaisha
- Applicants: Canon Kabushiki Kaisha
- Inventors: Masaya Asao; Tatsuo Senba
- Web page: https://patentgrep.com/patent/US20160250867A1

## CPC

- B41J 11/0015: {for treating before, during or after printing or for uniform coating or laminating the copy material before or after printing (selective coating B41J2/2114)}
- B41M 7/0036: {using protective coatings or layers dried without curing}
- B41J: TYPEWRITERS; SELECTIVE PRINTING MECHANISMS, i.e. MECHANISMS PRINTING OTHERWISE THAN FROM A FORME; CORRECTION OF TYPOGRAPHICAL ERRORS
- B41M: PRINTING, DUPLICATING, MARKING, OR COPYING PROCESSES; COLOUR PRINTING, (correction of typographical errors B41J; processes for applying transfer pictures or the like B44C1/16; fluid media for correction of typographical errors by coating C09D10/00; printing textiles D06P)

## Abstract

A recording method includes an ink application process of applying ink to a record medium and a cover layer formation process of forming a cover layer by applying a liquid composition containing polyurethane resin particles to the record medium to which the ink is applied in such a manner as to be at least partially overlapped with a region to which the ink is applied, in which the breaking strength of the cover layer is 0.1 N or more and the breaking elongation of the cover layer is 200% or more.

## Claims

### Claim 1

A recording method, comprising:
applying ink to a record medium; and
forming a cover layer by applying a liquid composition containing polyurethane resin particles to the record medium to which the ink is applied in such a manner as to be at least partially overlapped with a region to which the ink is applied, wherein breaking strength of the cover layer is 0.1 N or more and breaking elongation of the cover layer is 200% or more.

### Claim 2 (depends on 1)

The recording method according to claim 1, wherein, in the formation of the cover layer, a roll type coating device having a pan storing the liquid composition and a roll applying the liquid composition pumped up from inside of the pan to the record medium is used.

### Claim 3 (depends on 1)

The recording method according to claim 1, comprising, after the formation of the cover layer, performing drying at a temperature of 70° C. or more.

### Claim 4 (depends on 1)

The recording method according to claim 1, comprising, after the formation of the cover layer, folding the recorded matter.

### Claim 5

Recorded matter comprising:
a substrate;
and an ink receiving layer containing a coloring material, wherein
a cover layer containing polyurethane resin is provided in such a manner as to be at least partially overlapped with a region containing the coloring material of the ink receiving layer,
breaking strength of the cover layer is 0.1 N or more, and
breaking elongation of the cover layer is 200% or more.

### Claim 6

A recorded matter processing method comprising:
folding recorded matter obtained by applying ink to a record medium,
the method including forming a cover layer by applying a liquid composition containing polyurethane resin particles before the folding, wherein
breaking strength of the cover layer is 0.1 N or more and
breaking elongation of the cover layer is 200% or more.

### Claim 7

A method for improving fold-crack resistance of recorded matter obtained by applying ink to a record medium, the method comprising:
forming a cover layer by applying a liquid composition containing polyurethane resin particles to at least one part of the recorded matter, wherein
breaking strength of the cover layer is 0.1 N or more and
breaking elongation of the cover layer is 200% or more.