# US 2016/0249674 A1 · Tobacco material and treatment thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0249674 A1
- Document ID: US20160249674A1
- Status: Published application
- Kind: A1
- Application number: 15/033,199
- Filed: 2014-10-30
- Published: 2016-09-01
- Earliest claimed: 2013-10-31
- Assignees: British American Tobacco (Investments) Limited
- Applicants: British American Tobacco (Investments) Limited
- Inventors: Denis BENJAK; Pedro FIELD; Alcindo GLESSE; Matthias LINK
- Web page: https://patentgrep.com/patent/US20160249674A1

## CPC

- A24B 13/00: Tobacco for pipes, for cigars, e.g. cigar inserts, or for cigarettes; Chewing tobacco; Snuff (reconstituted tobacco products A24B3/14)
- A24B 3/04: Humidifying or drying tobacco bunches or cut tobacco (A24B3/12 takes precedence)
- A24B 15/18: Treatment of tobacco products or tobacco substitutes
- A24B 15/24: by extraction; Tobacco extracts
- A24B 15/245: {Nitrosamines}
- A24B: MANUFACTURE OR PREPARATION OF TOBACCO FOR SMOKING OR CHEWING; TOBACCO; SNUFF

## Abstract

A tobacco material and a process for the treatment of tobacco are provided. The process comprises securing the tobacco within a moisture-retaining material and exposing the tobacco material to an ambient processing temperature of at least about 45° C., with the tobacco having a packing density of at least 200 kg/m3 on a dry matter weight base at the start of the process and a moisture content of between about 10% and 23%. The TSNA content of the tobacco material is maintained at a relatively constant level during the process.

## Claims

### Claim at position 1

1: A process for treating tobacco material wherein the tobacco material has a relatively constant TSNA content during the process, the process comprising securing tobacco material within a moisture-retaining material and exposing the tobacco material to an ambient processing temperature of at least about 45° C., wherein the tobacco material has a packing density on a dry matter weight base of at least 200 kg/m3 at the start of the process and has a moisture content of between about 10% and 23% before and during treatment.

### Claim at position 2 (depends on 1)

2: The process according to claim 1, wherein the TSNA content of the treated tobacco material has not increased by more than about 0.25 μg/g from the TSNA content of untreated tobacco material.

### Claim at position 3 (depends on 1)

3: The process according to either claim 1, wherein the tobacco material has a packing density on a dry matter weight base of between about 200 kg/m3 and 500 kg/m3.

### Claim at position 4 (depends on 1)

4: The process according to claim 1, wherein the tobacco material has a moisture content of between about 10% and 18% before and during the treatment.

### Claim at position 5 (depends on 1)

5: The process according to claim 1, wherein the tobacco material is secured within the moisture-retaining material for between about 5 and 65 days.

### Claim at position 6 (depends on 1)

6: The process according to claim 1, wherein the tobacco material is exposed to an ambient processing temperature of above 55° C.

### Claim at position 7 (depends on 1)

7: The process according to claim 1, wherein the tobacco material has been exposed to an ambient processing temperature of at least about 45° C. or above 55° C. for at least 10 days.

### Claim at position 8 (depends on 7)

8: The process according to claim 7, wherein the tobacco material has been exposed to an ambient processing temperature of at least about 45° C. or above 55° C. for between about 10 and 40 days.

### Claim at position 9 (depends on 1)

9: The process according to claim 1, wherein the temperature of the tobacco material reaches the ambient processing temperature within about 4 to 10 days.

### Claim at position 10 (depends on 1)

10: The process according to claim 1, wherein the temperature of the tobacco material reaches a second temperature that is higher than the ambient processing temperature.

### Claim at position 11 (depends on 10)

11: The process according to claim 10, wherein the second temperature is at least 2° C. above the ambient processing temperature

### Claim at position 12 (depends on 10)

12: The process according to claim 10, wherein the second temperature is reached within about 7 to 13 days.

### Claim at position 13 (depends on 1)

13: The process according to claim 1, wherein the ambient processing humidity is between about 50-500 g water/m3 for ambient processing temperatures around or above 100° C., about 50-340 g water/m3 for ambient processing temperatures around 90° C., about 50-230 g water/m3 for ambient processing temperatures around 80° C., about 50-160 g water/m3 for ambient processing temperatures around 70° C., about 50-110 g water/m3 for ambient processing temperatures around 60° C., about 40-80 g water/m3 for ambient processing temperatures around 55° C. or about 30-70 g water/m3 for ambient processing temperatures around 45° C.

### Claim at position 14 (depends on 1)

14: The process according to claim 1, wherein the moisture-retaining material is wrapped around the tobacco material.

### Claim at position 15 (depends on 14)

15: The process according to claim 14, wherein the moisture-retaining material comprises flexible polymeric material.

### Claim at position 16 (depends on 15)

16: The process according to claim 15, wherein the flexible polymeric material comprises polyethylene.

### Claim at position 17 (depends on 1)

17: The process according to claim 1, wherein the tobacco material is placed in a chamber to control the ambient processing temperature and/or ambient processing humidity.

### Claim at position 18 (depends on 1)

18: The process according to claim 1, wherein the total TSNA content of the tobacco material is between about 0.4 and 0.95 μg/g.

### Claim at position 19 (depends on 1)

19: The process according to claim 1, wherein the tobacco material comprises whole leaf tobacco.

### Claim at position 20 (depends on 1)

20: The process according to claim 1, wherein the tobacco material does not comprise cut rag tobacco.

### Claim at position 21 (depends on 1)

21: The process according to claim 1, wherein the tobacco material is post-curing tobacco.

### Claim at position 22 (depends on 1)

22: The process according to claim 1, wherein the microbial content of the treated tobacco material is lower than the microbial content of the untreated tobacco material, and/or wherein the tobacco material at the end of the process is further processed for incorporation into a smoking article.

### Claim 23

(canceled)

### Claim at position 24 (depends on 1)

24: The process according to claim 1, wherein the tobacco material at the end of the process is suitable for incorporation into a smoking article.

### Claim 25

(canceled)

### Claim at position 26

26: A tobacco material secured within a moisture-retaining material, wherein the tobacco material has been exposed to an ambient processing temperature of at least about 45° C., has a packing density on a dry matter weight base of at least 200 kg/m3 and a moisture content of between about 10% and 23%, and wherein the TSNA content of the tobacco material has not increased from the TSNA content of tobacco material prior to being secured within a moisture-retaining material and exposed to an ambient processing temperature of at least about 45° C.

### Claim at position 27 (depends on 26)

27: A smoking article or a smokeless tobacco product, which comprises the tobacco material of claim 26.

### Claim 28

(canceled)

### Claim at position 29 (depends on 26)

29: A tobacco extract manufactured from the tobacco material of claim 26.

### Claim at position 30 (depends on 29)

30: A nicotine-delivery system comprising an extract according to claim 29.