# US 2016/0245132 A1 · Iron-Based Alloys and Methods of Making and Use Thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0245132 A1
- Document ID: US20160245132A1
- Status: Published application
- Kind: A1
- Application number: 15/147,087
- Filed: 2016-05-05
- Published: 2016-08-25
- Earliest claimed: 2013-09-19
- Assignees: L.E. Jones Company
- Applicants: L.E. Jones Company
- Inventors: Cong Yue Qiao; David Doll; Todd Trudeau; Peter Vennema
- Web page: https://patentgrep.com/patent/US20160245132A1

## CPC

- F01L 3/02: Selecting particular materials for valve-members or valve-seats; Valve-members or valve-seats composed of two or more materials
- C21D 1/18: Hardening (C21D1/02 takes precedence); Quenching with or without subsequent tempering (quenching devices C21D1/62)
- C21D 1/25: Hardening, combined with annealing between 300 degrees Celsius and 600 degrees Celsius, i.e. heat refining ("Vergüten")
- C21D 6/002: {containing Cr (C21D6/004 takes precedence)}
- C21D 6/004: {containing Cr and Ni}
- C21D 6/007: {containing Co}
- C21D 6/02: Hardening by precipitation
- C21D 9/0068: {for particular articles not mentioned below}
- C22C 37/08: with nickel
- C22C 37/10: containing aluminium or silicon
- C22C 38/001: {containing N}
- C22C 38/002: {containing In, Mg, or other elements not provided for in one single group C22C38/001 - C22C38/60}
- C22C 38/02: containing silicon
- C22C 38/04: containing manganese
- C22C 38/22: with molybdenum or tungsten
- C22C 38/24: with vanadium
- C22C 38/26: with niobium or tantalum
- C22C 38/30: with cobalt
- C22C 38/32: with boron
- C22C 38/36: with more than 1.7% by weight of carbon
- C22C 38/44: with molybdenum or tungsten
- C22C 38/46: with vanadium
- C22C 38/48: with niobium or tantalum
- C22C 38/52: with cobalt
- C22C 38/54: with boron
- C22C 38/56: with more than 1.7% by weight of carbon
- F16K 25/005: {Particular materials for seats or closure elements}
- C21D 6/005: {containing Mn}
- C21D 6/008: {containing Si}
- C21D 2211/004: Dispersions; Precipitations
- C21D 2211/008: Martensite
- Y10T 29/49409: Valve seat forming
- F01L: CYCLICALLY OPERATING VALVES FOR MACHINES OR ENGINES
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- F16K: VALVES; TAPS; COCKS; ACTUATING-FLOATS; DEVICES FOR VENTING OR AERATING {(devices for emptying and evacuating the excess liquid in valves or conduits F16L55/07)}
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

An iron-based alloy includes (in weight percent) carbon from about 1 to about 2 percent; manganese up to about 1 percent; silicon up to about 1 percent; nickel up to about 4 percent; chromium from about 10 to about 25 percent; molybdenum from about 5 to about 20 percent; tungsten up to about 4 percent; cobalt from about 17 to about 23 percent; vanadium up to about 1.5 percent; boron up to about 0.2 percent; sulfur up to about 0.03 percent; nitrogen up to about 0.4 percent; phosphorus up to about 0.06 percent; niobium up to about 4 percent; iron from about 35 to about 55 percent; and incidental impurities. The chromium/molybdenum ratio of the iron-based alloy is from about 1 to about 2.5. The alloy is suitable for use in elevated temperature applications, such as valve seat inserts for combustion engines.

## Claims

### Claim 1

An iron-based alloy comprising, in weight percent:
carbon from about 1 to about 2 percent;
manganese up to about 1 percent;
silicon up to about 1 percent;
nickel up to about 4 percent;
chromium from about 10 to about 25 percent;
molybdenum from about 5 to about 20 percent;
tungsten up to about 4 percent;
cobalt from about 17 to about 23 percent;
vanadium up to about 1.5 percent;
boron up to about 0.2 percent;
sulfur up to about 0.03 percent;
nitrogen from about 0.1 to about 0.4 percent;
phosphorus up to about 0.06 percent;
niobium up to about 4 percent;
iron from about 35 to about 55 percent; and
incidental impurities;
wherein the chromium/molybdenum ratio of the iron-based alloy is from about 1 to about 2.5.

### Claim 2 (depends on 1)

The iron-based alloy of claim 1, wherein the iron-based alloy consists essentially of, in weight percent:
carbon from about 1.4 to about 1.9 percent;
manganese up to about 1 percent;
silicon up to about 1 percent;
nickel up to about 1 percent;
chromium from about 13 to about 19 percent;
molybdenum from about 8 to about 14 percent;
tungsten up to about 1 percent;
cobalt from about 19 to about 22 percent;
vanadium up to about 0.5 percent;
niobium up to about 1 percent;
nitrogen from about 0.1 to about 0.4 percent;
phosphorus up to about 0.06 percent;
sulfur up to about 0.03 percent;
boron up to about 0.2 percent;
iron from about 38 to about 51 percent; and
incidental impurities.

### Claim 3 (depends on 1)

The iron-based alloy of claim 1, wherein the iron-based alloy comprises, in weight percent:
carbon from about 1.6 to about 1.9 percent;
manganese from about 0.15 to about 0.35 percent;
silicon from about 0.2 to about 0.6 percent;
nickel from about 0.8 to about 4 percent;
chromium from about 14 to about 16 percent;
molybdenum from about 12 to about 14 percent;
tungsten up to about 3 percent;
cobalt from about 19 to about 21 percent;
vanadium up to about 0.5 percent;
nitrogen from about 0.1 to about 0.4 percent;
boron up to about 0.2 weight percent;
iron from about 38 to about 51 percent; and
incidental impurities.

### Claim 4 (depends on 1)

The iron-based alloy according to claim 1, wherein the sum of the chromium content and the molybdenum content is from about 20 to about 35 weight percent.

### Claim 5 (depends on 1)

The iron-based alloy of claim 1, wherein the molybdenum content is from about 7 to about 15 weight percent, and the chromium content is from about 12 to about 20 weight percent.

### Claim 6 (depends on 1)

The iron-based alloy of claim 1, wherein the chromium/molybdenum ratio is from about 1.25 to about 1.35.

### Claim 7 (depends on 1)

The iron-based alloy of claim 1, wherein the iron-based alloy comprises, in weight percent:
niobium from about 0.1 to about 0.2 percent;
tungsten up to about 0.25 percent;
vanadium from about 0.01 to about 0.05 percent;
nitrogen from about 0.1 to about 0.25 percent;
nickel up to about 0.6 percent; and
chromium from about 13 to about 19 percent.

### Claim 8 (depends on 1)

The iron-based alloy of claim 1, wherein the boron content is from about 0.03 to about 0.15 weight percent.

### Claim 9 (depends on 1)

The iron-based alloy of claim 1, wherein the nickel content is less than about 2 weight percent.

### Claim 10 (depends on 1)

The iron-based alloy of claim 1, wherein the iron-based alloy is in a hardened and tempered condition, and the iron-based alloy is strengthened by at least two matrix strengthening mechanisms selected from the group consisting of sigma phase strengthening, Laves phase strengthening, and carbide strengthening.

### Claim 11 (depends on 1)

The iron-based alloy of claim 1, wherein the iron-based alloy comprises sigma phase in an amount of from about 3 to about 9 volume percent.

### Claim 12 (depends on 1)

The iron-based alloy of claim 1, wherein the iron-based alloy has a compressive yield strength of at least 175 ksi at 1000° F.

### Claim 13 (depends on 1)

The iron-based alloy of claim 1, wherein the iron-based alloy is in a hardened and tempered condition and has a bulk hardness of at least 50 HRc.

### Claim 14 (depends on 1)

The iron-based alloy of claim 1, wherein the iron-based alloy is in a hardened and tempered condition and exhibits a Vickers hot hardness of from about 500 to about 700 HV10 at a temperature of from about 600° F. to about 800° F.

### Claim 15 (depends on 1)

A part for an internal combustion engine comprising the iron-based alloy of claim 1.

### Claim 16

A valve seat insert for use in an internal combustion engine, the valve seat insert being made of an iron-based alloy comprising, in weight percent:
chromium from about 10 to about 25 percent;
molybdenum from about 5 to about 20 percent;
cobalt from about 17 to about 23 percent;
iron from about 35 to about 55 percent; and
wherein the chromium/molybdenum ratio of the iron-based alloy is from about 1 to about 2.5, the valve seat insert having a microstructure with martensite in intradendritic regions and carbides and sigma phase in interdendritic regions of the microstructure.

### Claim 17 (depends on 16)

The valve seat insert of claim 16, wherein the sigma phase is present in an amount of about 3 to about 9 volume percent and/or a ratio of interdendritic/intradendritic phases is about 40:60 percent to about 60:40 percent.

### Claim 18 (depends on 16)

The valve seat insert of claim 16, having (a) a hot hardness HV10 of about 500 to about 700 at 600 to 800° F., (b) a hot hardness HV10 of about 150 to about 220 at 1600° F., (c) an ultimate tensile strength of about 80 to about 90 ksi at 75° F. and about 75 to about 85 ksi at 1200° F., (d) a compressive yield strength of 185 to about 250 ksi from 75 to 1000° F., and/or (d) a hardness HRC of about 50 to about 70 from 75 to 1350° F.

### Claim 19 (depends on 16)

A method of manufacturing the valve seat insert according to claim 16, the method comprising casting the iron-based alloy and machining a piece of the iron-based alloy into the valve seat insert, hardening and tempering the valve seat insert such that the alloy has a microstructure wherein martensite is formed in intradendritic regions and sigma and carbides precipitate in interdendritic regions of the microstructure.

### Claim 20

A method of manufacturing a valve seat insert, the method comprising:
forming a valve seat insert by melting and casting an iron-based alloy comprising, in weight percent:
carbon from about 1 to 2.93 percent;
manganese up to about 1 percent;
silicon up to about 1 percent;
nickel up to 12.03 percent;
chromium from about 10 to about 25 percent;
molybdenum from about 5 to about 20 percent;
tungsten up to about 4 percent;
cobalt from about 17 to about 23 percent;
vanadium up to about 1.5 percent;
boron up to about 0.2 percent;
sulfur up to about 0.03 percent;
nitrogen from about 0.1 to about 0.4 percent;
phosphorus up to about 0.06 percent;
niobium up to about 4 percent;
iron from about 35 to about 55 percent; and
incidental impurities,
wherein the chromium/molybdenum ratio of the iron-based alloy is from about 1 to about 2.5 and total chromium plus molybdenum is about 20 to about 35 percent.