# US 2016/0243515 A1 · SOL CONTAINING AMORPHOUS Zr-O-BASED PARTICLES AS DISPERSOID, AND PRODUCTION METHOD OF THE SOL

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0243515 A1
- Document ID: US20160243515A1
- Status: Published application
- Kind: A1
- Application number: 14/888,170
- Filed: 2015-06-05
- Published: 2016-08-25
- Earliest claimed: 2014-09-29
- Assignees: Daiichi Kigenso Kagaku Kogyo Co., Ltd.
- Applicants: Daiichi Kigenso Kagaku Kogyo Co., Ltd.
- Inventors: Fumiyuki Takasaki
- Web page: https://patentgrep.com/patent/US20160243515A1

## CPC

- C09K 23/002: {Inorganic compounds}
- B01J 13/0008: {Sols of inorganic materials in water}
- B01J 13/0034: {Additives, e.g. in view of promoting stabilisation or peptisation}
- C01G 25/02: Oxides
- C01P 2002/02: Amorphous compounds
- C01P 2002/72: by d-values or two theta-values, e.g. as X-ray diagram
- C01P 2002/88: by thermal analysis data, e.g. TGA, DTA, DSC
- C01P 2004/62: Submicrometer sized, i.e. from 0.1-1 micrometer
- C01P 2004/64: Nanometer sized, i.e. from 1-100 nanometer
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS

## Abstract

The present invention provides a sol comprising, as a dispersoid, amorphous Zr—O--based particles having a median particle diameter D50 of 50 to 200 nm, so as to enable control of the optimal rheology and the application characteristics of a mixture system incorporating the sol. More specifically, the present invention provides a sol comprising, as a dispersoid, amorphous compound particles containing zirconium and oxygen, the amorphous compound particles having a median diameter in a range of 50 to 200 nm.

## Claims

### Claim 1

A sol comprising, as a dispersoid, amorphous compound particles containing zirconium and oxygen, the amorphous compound particles having a median diameter in a range of 50 to 200 nm.

### Claim 2 (depends on 1)

The sol according to claim 1, wherein when powder obtained by drying the sol at 45 to 55° C. to a constant weight is subjected to thermogravimetry in which the temperature is increased from 50° C. to 1000° C., the weight change rate (weight reduction rate) is 20% or more.

### Claim 3 (depends on 1)

The sol according to claim 1, wherein when powder obtained by drying the sol at 45 to 55° C. to a constant weight is subjected to thermogravimetry in which the temperature is increased from 50° C. to 1000° C., the weight change rate (weight reduction rate) is 25% or more.

### Claim 4 (depends on 1)

A method for producing the sol according to claim 1, the method comprising the steps of:
(1) Step 1 of hydrolyzing a zirconium salt aqueous solution having a molar ratio (Cl/Zr) of a chlorine element to a zirconium element in a range of 1.0 to 3.0, a pH of 5 or less, and a zirconium element concentration in a range of 6 to 15 wt % on a zirconium oxide basis (however, the above molar ratio Cl/Zr does not include Cl that can be regarded as a chloride salt other than zirconium chloride salt), thereby obtaining a hydrolyzed solution; and
(2) Step 2 of further hydrolyzing a diluted solution obtained by diluting the hydrolyzed solution obtained in Step 1 with water, wherein the dilution is performed so that the weight of a solution after the dilution is 2 to 15 times the weight of a solution before the dilution.