# US 2016/0240724 A1 · Method for producing a solar cell

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0240724 A1
- Document ID: US20160240724A1
- Status: Published application
- Kind: A1
- Application number: 15/024,879
- Filed: 2014-09-26
- Published: 2016-08-18
- Earliest claimed: 2013-09-27
- Assignees: Ion Beam Services
- Applicants: International Solar Energy Research Center Konstanz E.V.
- Inventors: Tim BOESCKE; Daniel KANIA
- Web page: https://patentgrep.com/patent/US20160240724A1

## CPC

- H10F 71/128: {Annealing}
- H10F 10/14: Photovoltaic cells having only PN homojunction potential barriers
- H10F 10/146: {Back-junction photovoltaic cells, e.g. having interdigitated base-emitter regions on the back side}
- H10F 10/148: {Double-emitter photovoltaic cells, e.g. bifacial photovoltaic cells}
- H10F 71/121: {The active layers comprising only Group IV materials}
- H10F 71/129: {Passivating}
- H10F 77/315: {the coatings being antireflective or having enhancing optical properties}
- H10F 77/703: {of the semiconductor bodies, e.g. textured active layers}
- Y02E 10/547: Monocrystalline silicon PV cells
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H10F: INORGANIC SEMICONDUCTOR DEVICES SENSITIVE TO INFRARED RADIATION, LIGHT, ELECTROMAGNETIC RADIATION OF SHORTER WAVELENGTH OR CORPUSCULAR RADIATION
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

The invention relates to a method for producing a solar cell (1) from crystalline semiconductor material. In a first surface (3a) of a semiconductor substrate (3), a first doping area (5) is formed by thermally diffusing a first dopant and in the second surface (3b) of the semiconductor substrate, a second doping area (7) is formed by implanting ions and thermally implanting a second dopant.

## Claims

### Claim 1

A method for producing a solar cell (1) from crystalline semiconductor material, wherein in a first surface (3a) of a semiconductor substrate (3) a first doping region (5) is formed by thermal indiffusion of a first dopant and in the second surface (3b) of the semiconductor substrate a second doping region (7) is formed through ion implantation or thermal indiffusion of a second dopant,
whereas through the ion implantation of the second dopant, a dopant deposition layer is formed on or close to the second surface and on the second surface a diffusion barrier layer (9b) for preventing an outdiffusion of the second dopant is generated out of the second surface and then at least one thermal process step is carried to form the first and second doping regions.

### Claim 2 (depends on 1)

The method of claim 1,
wherein the semiconductor material can be silicon, the first dopant can be an element from the group incorporating boron, indium, gallium, aluminium, in particular boron, and the second dopant can be an element from the group incorporating phosphorus, arsenic, antimony, in particular phosphorus.

### Claim 3 (depends on 1)

The method of claim 1,
wherein the first doping region (5) is formed as the emitter region in the front side surface (3a) of an n-silicon substrate (3) and the second dopant region is formed as a back surface field (7) in the rear side surface (3b) of the n-silicon substrate.

### Claim 4 (depends on 1)

A method according to claim 1,
whereas the doping profile of the second doping region (7) is flatter with respect to the doping profile of the first doping region (5) and/or is characterised by a higher surface concentration of the second dopant with respect to that of the first dopant.

### Claim 5 (depends on 1)

A method according to claim 1,
whereas only one thermal process step is carried out to form the first and second doping regions (5; 7) whereby the thermal budget used for indiffusion of the first dopant causes the activation of the second dopant out of the previously formed dopant deposition layer, for which purpose the indiffusion of the first dopant is performed after forming the diffusion barrier layer (9b) on the second surface (3b) and whereas the diffusion barrier layer is formed as the indiffusion barrier to prevent any indiffusion of the first dopant into the second surface.

### Claim 6 (depends on 5)

The method of claim 5,
whereas the diffusion barrier layer (9b) is formed at the same time as an oxygen diffusion barrier and the indiffusion of the first dopant is carried out at least in sections in an oxygen-containing atmosphere.

### Claim 7 (depends on 1)

A method according to claim 1,
whereas the formation of the first doping region (5) encompasses applying on the first and optionally the second surfaces (3a;3b) a glass containing the first dopant and preparing the first dopant in gaseous state in a process atmosphere.

### Claim 8 (depends on 1)

A method according to claim 1,
whereas the diffusion barrier layer (9b) on the second surface (3b) with a solar cell construction, in which the second surface forms the rear side of the solar cell (1), is left on the second surface as rear side passivation and/or rear side anti-reflection layer.

### Claim 9 (depends on 1)

A method according to claim 1, designed as a method for producing of a solar cell (1) contacted on both sides with a front side emitter or a solar cell with a rear side emitter or a MWT (Metal-Wrap-Through) solar cell or an IBC (Interdigital-Back-Contact) solar cell.

### Claim 10 (depends on 1)

A method according to claim 1,
whereas as a diffusion barrier layer (9b) an SiN layer, in particular with a refractive index of n=1, 8 . . . 2, 2, even more especially n=1, 9 . . . 2, 0, and in particular with a thickness between 1 and 250 nm, even more especially between 30 and 80 nm, is used.

### Claim 11 (depends on 10)

The method of claim 10,
whereas a layer stack is used as a diffusion barrier layer, a layer stack which contains in addition to an SiN layer, an SiO2—, Al2O3—, TiO— and/or SiON layer and with which the additional layer or additional layers has/have in particular a thickness in the region between 0.5 and 50 nm.

### Claim 12 (depends on 10)

The method of claim 10,
whereas the diffusion barrier layer (9b) is generated by means of a PECVD-, LPCVD-, APCVD- or PVD-Process.