# US 2016/0240394 A1 · Semiconductor Device Manufacturing Method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0240394 A1
- Document ID: US20160240394A1
- Status: Published application
- Kind: A1
- Application number: 15/024,579
- Filed: 2014-09-19
- Published: 2016-08-18
- Earliest claimed: 2013-09-25
- Assignees: Nitto Denko Corporation
- Applicants: Nitto Denko Corporation
- Inventors: Akihiro Fukui; Naohide Takamoto; Hiroyuki Hanazono
- Web page: https://patentgrep.com/patent/US20160240394A1

## CPC

- H10W 74/012: {of encapsulations on active surfaces of flip-chip devices, e.g. forming underfills}
- H10P 72/7402: {Wafer tapes, e.g. grinding or dicing support tapes}
- H10P 72/7404: {the wafer tape being a laminate of three or more layers, e.g. including additional layers beyond a base layer and an uppermost adhesive layer}
- H10W 70/099: {Connecting interconnections to insulating or insulated package substrates, interposers or redistribution layers}
- H10W 74/15: on active surfaces of flip-chip devices, e.g. underfills
- H10P 72/7416: {used during dicing or grinding}
- H10P 72/742: {involving stretching of the auxiliary support post dicing}
- H10P 72/7422: {used to protect an active side of a device or wafer}
- H10P 72/7438: {with parts of the auxiliary support remaining in the finished device}
- H10W 72/01271: {Cleaning, e.g. oxide removal or de-smearing}
- H10W 72/013: {of die-attach connectors}
- H10W 72/01304: {using temporary auxiliary members, e.g. using sacrificial coatings or handle substrates}
- H10W 72/01336: {in solid form, e.g. by using a powder or by laminating a foil}
- H10W 72/01365: {Thermally treating (reflowing H10W72/01357)}
- H10W 72/0198: {batch processes}
- H10W 72/072: {of bump connectors}
- H10W 72/07234: {Using a reflow oven}
- H10W 72/07236: {Soldering or alloying}
- H10W 72/073: {of die-attach connectors}
- H10W 72/07331: {Connecting techniques}
- H10W 72/07332: {Compression bonding, e.g. thermocompression bonding}
- H10W 72/07334: {Using a reflow oven}
- H10W 72/07338: {hardening the adhesive by curing, e.g. thermosetting}
- H10W 72/07339: {hardening the adhesive by cooling, e.g. thermoplastics}
- H10W 72/241: {Dispositions, e.g. layouts}
- H10W 72/252: {comprising solid metals or solid metalloids, e.g. PbSn, Ag or Cu}
- H10W 72/325: {Die-attach connectors having a filler embedded in a matrix}
- H10W 72/351: {Materials of die-attach connectors}
- H10W 72/352: {comprising metals or metalloids, e.g. solders}
- H10W 72/353: {not comprising solid metals or solid metalloids, e.g. ceramics}
- H10W 72/354: {comprising polymers}
- H10W 90/724: {between a chip and a stacked insulating package substrate, interposer or RDL}
- H10W 90/734: {between a chip and a stacked insulating package substrate, interposer or RDL}
- H10W 99/00: Subject matter not provided for in other groups of this subclass
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A method for producing a semiconductor device includes: a Step A of preparing a chip with sheet-shaped resin composition in which a sheet-shaped resin composition is pasted onto a bump formation surface of a semiconductor chip, a Step B of preparing a substrate for mounting on which an electrode is formed, a Step C of pasting the chip with resin composition to the substrate for mounting so that the resin composition serves as a pasting surface with the bump formed on the semiconductor chip facing toward the electrode formed on the substrate for mounting, a Step D of heating the resin composition to semi-cure the resin composition after the Step C, and a Step E of heating the resin composition at a higher temperature than that in the Step D to cure the resin composition after the Step D while bonding the bump and the electrode.

## Claims

### Claim 1

A method for producing a semiconductor device, comprising:
a Step A of preparing a chip with sheet-shaped resin composition in which a sheet-shaped resin composition is pasted to a bump formation surface of a semiconductor chip,
a Step B of preparing a substrate for mounting on which an electrode is formed,
a Step C of pasting the chip with sheet-shaped resin composition to the substrate for mounting so that the sheet-shaped resin composition serves as a pasting surface with the bump formed on the semiconductor chip facing toward the electrode formed on the substrate for mounting,
a Step D of heating the sheet-shaped resin composition to semi-cure the sheet-shaped resin composition after the Step C, and
a Step E of heating the sheet-shaped resin composition at a higher temperature than that in the Step D to cure the sheet-shaped resin composition after the Step D while bonding the bump and the electrode.

### Claim 2 (depends on 1)

The method for producing a semiconductor device according to claim 1, wherein
the sheet-shaped resin composition has a minimum melt viscosity of 10 Pa·s to 5,000 Pa·s at less than 200° C.;
a thermal curing rate of 6% or more after heating at 200° C. for 10 seconds; and
a viscosity after heating at 200° C. for 10 seconds, which is a value obtained from a viscosity curve obtained from Andrade's equation, of 100 Pa·s to 10,000 Pa·s.

### Claim 3 (depends on 1)

The method for producing a semiconductor device according to claim 1, wherein
the Step D is a step of heating the sheet-shaped resin composition at 100° C. to 230° C.,
the Step E is a step of bonding the electrode and the bump using a solder having a melting point of 180° C. to 260° C., and
the heating temperature in the Step D is lower than the melting point of the solder.