# US 2016/0240383 A1 · Method for roughness improvement and selectivity enhancement during arc layer etch via adjustment of carbon-fluorine content

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0240383 A1
- Document ID: US20160240383A1
- Status: Published application
- Kind: A1
- Application number: 14/751,643
- Filed: 2015-06-26
- Published: 2016-08-18
- Earliest claimed: 2015-02-13
- Assignees: Tokyo Electron Limited
- Applicants: Tokyo Electron Limited
- Inventors: Vinayak Rastogi; Alok Ranjan
- Web page: https://patentgrep.com/patent/US20160240383A1

## CPC

- H10P 95/94: {Hydrogenation or deuterisation, e.g. using atomic hydrogen from a plasma}
- H10P 14/2905: {Silicon, silicon germanium or germanium}
- H10P 50/283: {by chemical means}
- H10P 74/203: {Structural properties, e.g. testing or measuring thicknesses, line widths, warpage, bond strengths or physical defects}
- H10P 76/2043: {using an anti-reflective coating}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A method of patterning a silicon containing ARC (anti-reflective coating) layer underlying a patterned layer is described that includes establishing a flow of a process gas to a plasma processing system, selecting a process condition that increases an etch selectivity of the silicon containing ARC layer relative to the patterned layer, igniting plasma from the process gas using a plasma source in accordance with the process condition, and exposing the substrate to the plasma to extend the feature pattern of the patterned layer into the silicon containing ARC layer. The composition of the process gas and the flow rate(s) of the gaseous constituents in the process gas are selected to adjust the carbon-fluorine content.

## Claims

### Claim 1

A method of patterning a layer on a substrate, comprising:
disposing a substrate comprising a multi-layer mask in a plasma processing system, wherein the multi-layer mask has a patterned layer defining an open feature pattern overlying a silicon containing ARC (anti-reflective coating) layer;
establishing a flow of a process gas to the plasma processing system, the process gas containing:
a first gaseous molecular constituent composed of C, F and optionally H, and having a carbon-to-fluorine ratio of 1-to-4, and
a second gaseous molecular constituent composed of C, F, and optionally H, and having a carbon-to-fluorine ratio of 1-to-3,
selecting a process condition that adjusts the C-F molecular ratio to increase an etch selectivity, measured as the ratio of the etch rate of the silicon containing ARC layer to the etch rate of the patterned layer, to a value that exceeds 5-to-1 by selecting a ratio of the flow rate of the first gaseous molecular constituent to the flow rate of the second gaseous molecular constituent greater than or equal to 0.5 and less than 2.5;
igniting plasma from the process gas using a plasma source in accordance with the process condition; and
exposing the substrate to the plasma to extend the feature pattern of the patterned layer into the silicon containing ARC layer.

### Claim 2 (depends on 1)

The method of claim 1, wherein the first gaseous molecular constituent includes CF4.

### Claim 3 (depends on 2)

The method of claim 2, wherein the second gaseous molecular constituent includes CHF3.

### Claim 4 (depends on 3)

The method of claim 3, wherein the process gas contains CF4 and CHF3, and the ratio of the CF4 flow rate to the CHF3 flow rate ranges from 0.5 to 2.0.

### Claim 5 (depends on 1)

The method of claim 1, wherein the first gaseous molecular constituent includes CF4, the second gaseous molecular constituent includes OH F3, and the molecular ratio of carbon-to-fluorine for the combined flows of the process gas ranges from 0.274 to 0.300.

### Claim 6 (depends on 1)

The method of claim 1, wherein the introducing of the process gas further includes introducing:
a third gaseous molecular constituent composed of atomic hydrogen, diatomic hydrogen, or C and an element selected from the group consisting of H and F, wherein the carbon-to-fluorine ratio of the third gaseous molecular constituent is greater than the maximum carbon-to-fluorine ratio of the first and second gaseous molecular constituents.

### Claim 7 (depends on 6)

The method of claim 6, wherein the third gaseous molecular constituent includes a CxFy-containing gas, and wherein x and y represent a real number greater than 0.

### Claim 8 (depends on 7)

The method of claim 7, wherein the ratio x/y exceeds the C-to-F ratio of the first and the second gaseous molecular constituents.

### Claim 9 (depends on 7)

The method of claim 7, wherein the third gaseous molecular constituent includes a O4F8.

### Claim 10 (depends on 6)

The method of claim 6, wherein the third gaseous molecular constituent includes a CxHy-containing gas, and wherein x and y represent a real number greater than 0.

### Claim 11 (depends on 10)

The method of claim 10, wherein the ratio y/x exceeds the H-to-C ratio of the first and the second gaseous molecular constituents.

### Claim 12 (depends on 10)

The method of claim 10, wherein the CxHy-containing gas includes CH4, C2H4, C2H2, C2H6, C3H4, C3H6, C3H8, C4H6, C4H8, C4H10, C5H8, C5H10, C6H6, C6H10, or C6H12, or any combination of two or more thereof.

### Claim 13 (depends on 1)

The method of claim 1, further comprising:
pulse modulating the introducing of the second gaseous molecular constituent.

### Claim 14 (depends on 13)

The method of claim 13, further comprising:
selecting a process condition for the pulse modulating and controlling a profile of the open feature pattern formed within the silicon containing ARC layer, the process condition including setting a pulse amplitude, a pulse frequency, a pulse duty cycle, or a pulse waveform, or any combination thereof.

### Claim 15 (depends on 13)

The method of claim 13, wherein the pulse modulating comprises pulsing the flow rate of the second gaseous molecular constituent between an off-state and an on-state.

### Claim 16 (depends on 1)

The method of claim 1, further comprising:
selecting a process condition that includes setting a flow rate of the second gaseous molecular constituent to decrease a roughness of the open feature pattern formed in the patterned layer and the silicon containing ARC layer relative to a nominal roughness achievable using the process condition while introducing only the primary etchant gas composition.

### Claim 17 (depends on 16)

The method of claim 16, wherein the reduction of roughness exceeds 10% of the nominal roughness.

### Claim 18 (depends on 1)

The method of claim 1, further comprising:
electrically biasing a substrate holder that supports the substrate with radio frequency (RF) power; and
pulsing the RF power for the electrical biasing.

### Claim 19 (depends on 1)

The method of claim 1, wherein the etch selectivity exceeds a value of 10.

### Claim 20 (depends on 1)

The method of claim 1, wherein the patterned layer has an open feature pattern characterized by a first critical dimension (CD), and wherein a difference between a second CD measured at a bottom of the open feature pattern formed in the silicon containing ARC layer and the first CD is less than 20% of the first CD.