# US 2016/0240373 A1 · Method for forming oxide layer by oxidizing semiconductor substrate with hydrogen peroxide

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0240373 A1
- Document ID: US20160240373A1
- Status: Published application
- Kind: A1
- Application number: 14/621,174
- Filed: 2015-02-12
- Published: 2016-08-18
- Earliest claimed: 2015-02-12
- Assignees: ASM IP Holding B.V.
- Applicants: ASM IP Holding B.V.
- Inventors: Fu Tang; Michael Givens; Qi Xie; Jan Willem Maes; Bert Jongbloed; Radko G. Bankras; Theodorus G.M. Oosterlaken; Dieter Pierreux; Werner Knaepen; Harald B. Profijt; Cornelius A. van der Jeugd
- Web page: https://patentgrep.com/patent/US20160240373A1

## CPC

- H10P 14/6308: {of Group IV semiconductors}
- H10P 14/6309: {of silicon in uncombined form, i.e. pure silicon}
- H10P 14/68: Organic materials, e.g. photoresists
- H10P 14/69215: {the material being a silicon oxide, e.g. SiO2}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

In some embodiments, an oxide layer is grown on a semiconductor substrate by oxidizing the semiconductor substrate by exposure to hydrogen peroxide at a process temperature of about 500° C. or less. The exposure to the hydrogen peroxide may continue until the oxide layer grows by a thickness of about 1 Å or more. Where the substrate is a germanium substrate, while oxidation using H2O has been found to form germanium oxide with densities of about 4.25 g/cm3, oxidation according to some embodiments can form an oxide layer with a density of about 6 g/cm3 or more (for example, about 6.27 g/cm3). In some embodiments, another layer of material is deposited directly on the oxide layer. For example, a dielectric layer may be deposited directly on the oxide layer.

## Claims

### Claim 1

A method for semiconductor processing, comprising:
growing an oxide layer on a semiconductor substrate, the oxide layer growing by a thickness of about 1 Å or more, wherein growing the oxide layer comprises:
oxidizing the semiconductor substrate by exposing the semiconductor substrate to hydrogen peroxide at a process temperature of about 500° C. or less.

### Claim 2 (depends on 1)

The method of claim 1, wherein growing the oxide layer comprises:
oxidizing a germanium-containing substrate,
wherein the oxide layer comprises germanium oxide.

### Claim 3 (depends on 2)

The method of claim 2, wherein oxidizing the germanium-containing substrate comprises oxidizing a silicon-germanium substrate.

### Claim 4 (depends on 2)

The method of claim 2, wherein oxidizing the germanium-containing substrate comprises oxidizing a germanium substrate.

### Claim 5 (depends on 2)

The method of claim 2, wherein the germanium oxide has a density of about 6 g/cm3 or more.

### Claim 6 (depends on 5)

The method of claim 5, wherein the germanium oxide is in a rutile form.

### Claim 7 (depends on 1)

The method of claim 1, wherein oxidizing the substrate comprises oxidizing a silicon substrate.

### Claim 8 (depends on 1)

The method of claim 1, wherein the substrate comprises a group III-V semiconductor.

### Claim 9 (depends on 1)

The method of claim 1, wherein the process temperature is about 400° C. or less.

### Claim 10 (depends on 1)

The method of claim 1, wherein oxidizing the semiconductor substrate further comprises exposing the semiconductor substrate to water vapor.

### Claim 11 (depends on 10)

The method of claim 10, wherein exposing the semiconductor substrate to water vapor and exposing the semiconductor substrate to hydrogen peroxide are performed simultaneously.

### Claim 12 (depends on 1)

The method of claim 1, wherein growing the oxide layer is accomplished by thermal oxidation.

### Claim 13

A method for semiconductor processing, comprising:
forming an oxide layer by exposing a semiconductor substrate to hydrogen peroxide, wherein a process temperature for exposing the semiconductor substrate is about 500° C. or less while forming the oxide layer; and
depositing an other layer of material directly on the oxide layer.

### Claim 14 (depends on 13)

The method of claim 13, wherein the process temperature is about 400° C. or less while forming the oxide layer.

### Claim 15 (depends on 14)

The method of claim 14, wherein the process temperature is about 300° C. or less while forming the oxide layer.

### Claim 16 (depends on 13)

The method of claim 13, wherein exposing the semiconductor substrate comprises exposing a germanium-containing substrate to the hydrogen peroxide.

### Claim 17 (depends on 13)

The method of claim 13, wherein exposing the semiconductor substrate comprises increasing a density of oxide on a surface of the germanium-containing substrate.

### Claim 18 (depends on 17)

The method of claim 17, wherein an oxide on a surface of the germanium-containing substrate has a density of about 5 g/cm3 or less before exposing, and a density of about 6 g/cm3 or more after exposing.

### Claim 19 (depends on 13)

The method of claim 13, wherein exposing the semiconductor substrate comprises feeding an aqueous hydrogen peroxide solution to and evaporating in an evaporator heated to an evaporation temperature of 120° C. to 40° C.

### Claim 20 (depends on 13)

The method of claim 13, wherein forming the oxide layer is performed without exposing the semiconductor substrate to radical species.

### Claim 21 (depends on 13)

The method of claim 13, wherein depositing the other layer of material comprises depositing a dielectric layer.