# US 2016/0238958 A1 · Toner for developing electrostatic charge image and method for preparing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0238958 A1
- Document ID: US20160238958A1
- Status: Published application
- Kind: A1
- Application number: 15/046,822
- Filed: 2016-02-18
- Published: 2016-08-18
- Earliest claimed: 2015-02-18
- Assignees: Samsung Electronics Co., Ltd.
- Applicants: Samsung Electronics Co., Ltd.
- Inventors: Masahide YAMADA; Akinori TERADA; Keiichi ISHIKAWA; Kenichi MIYAMOTO
- Web page: https://patentgrep.com/patent/US20160238958A1

## CPC

- G03G 9/08755: {Polyesters}
- G03G 9/0804: {whereby the components are brought together in a liquid dispersing medium}
- G03G 9/0806: {whereby chemical synthesis of at least one of the toner components takes place}
- G03G 9/0819: {characterised by the dimensions of the particles}
- G03G 9/0821: {characterised by physical parameters (magnetic parameters G03G9/083)}
- G03G 9/08797: {characterised by their physical properties, e.g. viscosity, solubility, melting temperature, softening temperature, glass transition temperature}
- G03G 9/09328: {obtained otherwise than by reactions only involving carbon-to-carbon unsaturated bonds}
- G03G: ELECTROGRAPHY; ELECTROPHOTOGRAPHY; MAGNETOGRAPHY

## Abstract

A toner for developing an electrostatic charge image, the toner including: elemental iron, wherein a content of the elemental iron is in a range of 1.0×103 to 1.0×104 ppm, based on a total weight of the toner; elemental silicon, wherein a content of the elemental silicon is in a range of 1.0×103 to 5.0×103 ppm, based on a total weight of the toner; elemental sulfur, wherein a content of the elemental sulfur is in a range of 500 to 3,000 ppm, based on a total weight of the toner; optionally elemental fluorine, wherein a content of the elemental fluorine, if present, is in a range of 1.0×103 to 1.0×104 ppm; and a binder resin

## Claims

### Claim 1

A toner for developing an electrostatic charge image, the toner comprising:
elemental iron, wherein a content of the elemental iron is in a range of 1.0×103 to 1.0×104 ppm, based on a total weight of the toner;
elemental silicon, wherein a content of the elemental silicon is in a range of 1.0×103 to 5.0×103 ppm, based on a total weight of the toner;
elemental sulfur, wherein a content of the elemental sulfur is in a range of 500 to 3,000 ppm, based on a total weight of the toner;
optionally elemental fluorine, wherein a content of the elemental fluorine, if present, is in a range of 1.0×103 to 1.0×104 ppm; and
a binder resin comprising
an amorphous polyester resin, wherein
(1) a mole ratio of an aromatic portion of the amorphous polyester resin to an aliphatic portion amorphous polyester resin is in a range of 4.5 to 5.8,
(2) a glass transition temperature of the amorphous polyester resin, when measured by a differential scanning calorimetry, is in a range of 50 to 70° C., and
(3) an endothermic gradient in the glass transition temperature of the amorphous polyester resin is in a range of 0.1 to 1.0 W/g° C., and
a crystalline polyester resin comprising elemental sulfur and elemental fluorine, wherein
(a) an endotherm in the melting of the crystalline polyester resin, when measured by the differential scanning calorimetry, is in a range of 2.0 to 10.0 W/g,
(b) a weight average molecular weight of the crystalline polyester resin is in a range of 5,000 to 15,000 Daltons,
(c) a difference between an endothermic start temperature and an endothermic peak temperature of the crystalline polyester is in range of 3 to 5° C. when the temperature of the crystalline polyester resin is increased in the differential scanning calorimetry curve when determined by the differential scanning calorimetry,
(d) a content of the crystalline polyester resin having a weight average molecular weight of 1,000 Daltons or less which is in a range of 1 to less than 10%, based on a total content of the crystalline polyester resin.

### Claim 2 (depends on 1)

The toner of claim 1, further comprising
a coating layer disposed on an external surface of the toner,
wherein the coating layer comprises the amorphous polyester resin.

### Claim 3 (depends on 2)

The toner of claim 2, wherein a thickness of the coating layer is in a range of 0.2 to 1.0 μm.

### Claim 4 (depends on 1)

The toner of claim 1, wherein an acid value of the toner is in a range of 3 to 25 mg KOH/g.

### Claim 5 (depends on 1)

The toner of claim 1, wherein a volume average particle diameter of the toner is in a range of 3 to 9 μm,
a content of particles having number average particle size of 3 μm or less is equal to or less than 3%, based on a total content of the toner, and
a content of particles the number average particle size of 3 μm or less to a number average particle size of 1 μm or less is in a range of 2.0 to 4.0, based on a total content of the toner.

### Claim 6

A method for preparing a toner, which comprises a binder resin, for developing an electrostatic charge image, the method comprising:
dehydro-condensing a polycarboxylic acid component and a polyol component in a temperature of 150° C. or less under the presence of a catalyst to provide a condensed amorphous resin;
urethane-extending the condensed amorphous resin to synthesize the amorphous polyester resin;
forming a latex of the amorphous polyester resin;
dehydro-condensing an aliphatic polycarboxylic acid component and an aliphatic polyol component in a temperature of 100° C. or less under the presence of a catalyst to provide a crystalline polyester resin;
forming a latex of the crystalline polyester resin;
mixing the amorphous polyester resin latex and the crystalline polyester resin latex to form a mixture;
adding a flocculant comprising elemental iron and elemental silicon into the mixture;
aggregating the amorphous polyester resin and the crystalline polyester resin to form a primary aggregated particle;
disposing a coating layer comprising the amorphous polyester resin on a surface of the primary aggregated particle to form a coated aggregated particle; and
fusing and coalescing the coated aggregated particle in a temperature that is greater than a glass transition temperature of the amorphous polyester resin to form the toner,
wherein
(1) a mole ratio of an aromatic portion of the amorphous polyester resin to an aliphatic portion of the amorphous polyester resin is in a range of 4.5 to 5.8,
(2) a glass transition temperature of the amorphous polyester resin, when measured by a differential scanning calorimetry, is in a range of 50 to 70° C., and
(3) an endothermic gradient in the glass transition temperature is in a range of 0.1 to 1.0 W/g° C., and
wherein crystalline polyester resin comprises elemental sulfur and elemental fluorine, and
(a) an endotherm in the melting of the crystalline polyester resin, when measured by the differential scanning calorimetry, is in a range of 2.0 to 10.0 W/g,
(b) a weight average molecular weight of the crystalline polyester resin is in a range of 5,000 to 15,000 Daltons,
(c) a difference between an endothermic start temperature and an endothermic peak temperature of the crystalline polyester resin is in range of 3 to 5° C. when the temperature of the crystalline polyester resin is increased in the differential scanning calorimetry curve determined by the differential scanning calorimetry, and
(d) a content of the crystalline polyester resin having a weight average molecular weight of 1,000 Daltons or less which is in a range of 1 to less than 10%, based on a total content of the crystalline polyester resin, and
wherein the catalyst comprises elemental sulfur.