# US 2016/0237558 A1 · Seamless hexagonal boron nitride atomic monolayer thin film and method of fabricating the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0237558 A1
- Document ID: US20160237558A1
- Status: Published application
- Kind: A1
- Application number: 15/017,753
- Filed: 2016-02-08
- Published: 2016-08-18
- Earliest claimed: 2015-02-12
- Assignees: Samsung Electronics Co., Ltd.; Research & Business Foundation Sungkyunkwan University
- Applicants: Samsung Electronics Co., Ltd.; Research & Business Foundation Sungkyunkwan University
- Inventors: Hwansoo SUH; Youngjae SONG; Qinke WU; Sungjoo LEE; Minwoo KIM; Sangwoo PARK
- Web page: https://patentgrep.com/patent/US20160237558A1

## CPC

- C01B 21/064: with boron
- C23C 16/02: Pretreatment of the material to be coated (C23C16/04 takes precedence)
- C23C 16/0209: {by heating}
- C23C 16/0254: {Physical treatment to alter the texture of the surface, e.g. scratching or polishing}
- C23C 16/342: {Boron nitride}
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

A seamless hexagonal h-BN atomic monolayer thin film has a pseudo-single crystal structure including a plurality of h-BN grains that are seamlessly merged. Each of the h-BN grains has a dimension in a range from about 10 μm to about 1,000 μm.

## Claims

### Claim 1

A seamless hexagonal boron nitride (h-BN) atomic monolayer thin film having a pseudo-single crystal structure comprising a plurality of h-BN grains that are seamlessly merged, each of the plurality of h-BN grains having a dimension in a range from about 10 μm to about 1,000 μm.

### Claim 2 (depends on 1)

The seamless h-BN atomic monolayer thin film of claim 1, wherein the plurality of h-BN grains are grown from a plurality of h-BN seeds having gaps amongst one another, the gaps between the plurality of h-BN seeds ranging between about 10 μm and about 1,000 μm.

### Claim 3 (depends on 1)

The seamless h-BN atomic monolayer thin film of claim 1, wherein the h-BN atomic monolayer thin film made from the seamlessly merged plurality of h-BN grains has a dimension in a range from about 1 cm to 30 cm.

### Claim 4 (depends on 1)

The seamless h-BN atomic monolayer thin film of claim 1, wherein the h-BN atomic monolayer thin film is line defect-free at a grain boundary.

### Claim 5 (depends on 1)

The seamless h-BN atomic monolayer thin film of claim 1, further comprising a metal thin film provided on the h-BN atomic monolayer thin film, wherein the metal thin film comprises a plurality of metal thin film grains, each of the plurality of metal thin film grains having one of a plurality of crystal direction planes, the h-BN grains on respective one of the plurality of metal thin film grains have same crystalline direction and each of the plurality of h-BN grains on a grain boundary of the metal thin film has the same crystalline direction as a crystalline direction of the h-BN grains on one of the metal thin film grains contacting the grain boundary of the metal thin film.

### Claim 6

A method of fabricating a seamless hexagonal boron nitride (h-BN) atomic monolayer thin film, the method comprising:
pre-annealing a metal thin film at a first temperature in a chamber while supplying hydrogen gas to the chamber;
supplying nitrogen source gas and boron source gas to the chamber; and
forming the seamless h-BN atomic monolayer thin film having a pseudo-single crystal atomic monolayer structure having a grain dimension in a range from about 10 μm to about 1,000 μm by annealing the pre-annealed metal thin film at a second temperature.

### Claim 7 (depends on 6)

The method of claim 6, wherein the pre-annealing and the forming of the h-BN atomic monolayer thin film are consecutively performed in the chamber.

### Claim 8 (depends on 6)

The method of claim 6, wherein the first temperature and the second temperature are substantially the same.

### Claim 9 (depends on 6)

The method of claim 6, wherein the forming of the h-BN atomic monolayer thin film comprises:
forming a plurality of h-BN seeds from the supplying nitrogen source gas and boron source gas to the chamber;
growing a plurality of h-BN grains from the plurality of h-BN seeds; and
forming the seamless h-BN atomic monolayer thin film having the pseudo-single crystal structure by merging the plurality of h-BN grains.

### Claim 10 (depends on 9)

The method of claim 9, wherein the forming of the h-BN atomic monolayer thin film comprises supplying the hydrogen gas in an amount from 100 times to 200 times greater than amounts of the nitrogen source gas and the boron source gas.

### Claim 11 (depends on 9)

The method of claim 9, wherein the plurality of h-BN seeds are formed in gaps in a range from about 10 μm to about 1,000 μm amongst one another.

### Claim 12 (depends on 9)

The method of claim 9, wherein the seamless h-BN atomic monolayer thin film has a dimension in a range from about 1 cm to about 30 cm.

### Claim 13 (depends on 9)

The method of claim 9, wherein the h-BN atomic monolayer thin film is line defect-free at a grain boundary between the plurality of h-BN grains.

### Claim 14 (depends on 9)

The method of claim 9, wherein the metal thin film comprises a plurality of metal thin film grains, each of the plurality of metal thin film grains having one of a plurality of crystalline direction planes, the h-BN grains on respective one of the plurality of metal thin film grains have same crystalline direction and each of the plurality of h-BN grains on a grain boundary of the metal thin film has the same crystalline direction as a crystalline direction of the h-BN grains on one of the metal thin film grains contacting the grain boundary of the metal thin film.

### Claim 15 (depends on 6)

The method of claim 6, further comprising polishing a first surface of the metal thin film before the pre-annealing the metal thin film.

### Claim 16 (depends on 15)

The method of claim 15, wherein the polishing comprises at least one of chemical polishing, physical polishing, chemical-mechanical polishing, and electrolyte polishing.

### Claim 17 (depends on 6)

The method of claim 6, wherein the nitrogen source gas comprises at least one of NH3 and N2.

### Claim 18 (depends on 6)

The method of claim 6, wherein the boron source gas is at least one selected from the group consisting of BH3, BF3, BCl3, B2H6, (CH3CH2)3B, and (CH3)3B.

### Claim 19 (depends on 6)

The method of claim 6, wherein the nitrogen source gas and the boron source gas are supplied by at least one of ammonia borane and borazine.

### Claim 20 (depends on 6)

The method of claim 6, wherein the metal thin film comprises at least one of Ni, Co, Fe, Pt, Pd, Au, Al, Cr, Cu, Mg, Mn, Mo, Rh, Ta, Ti, W, U, V, or Zr.