# US 2016/0237545 A1 · Method of fabricating a nitrided low-alloy steel part

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0237545 A1
- Document ID: US20160237545A1
- Status: Published application
- Kind: A1
- Application number: 15/042,196
- Filed: 2016-02-12
- Published: 2016-08-18
- Earliest claimed: 2015-02-13
- Assignees: Messier-Bugatti-Dowty
- Applicants: Messier-Bugatti-Dowty
- Inventors: Alain VIOLA; Nicolas BINOT
- Web page: https://patentgrep.com/patent/US20160237545A1

## CPC

- C23C 8/26: of ferrous surfaces
- C21D 1/06: Surface hardening
- C21D 1/25: Hardening, combined with annealing between 300 degrees Celsius and 600 degrees Celsius, i.e. heat refining ("Vergüten")
- C21D 3/04: Decarburising
- C21D 6/002: {containing Cr (C21D6/004 takes precedence)}
- C22C 38/22: with molybdenum or tungsten
- C22C 38/24: with vanadium
- C23C 8/02: Pretreatment of the material to be coated (C23C8/04 takes precedence)
- C23C 8/80: After-treatment
- C23F 17/00: Multi-step processes for surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by subclass C21D or C22F or class C25 (coating for obtaining at least two superposed coatings either by methods not provided for in a single one of main groups C23C2/00 - C23C26/00, or by combinations of methods providedfor in subclasses C23C and C25D, C23C28/00)
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C23F: NON-MECHANICAL REMOVAL OF METALLIC MATERIAL FROM SURFACE (working metal by laser beams B23K26/00; desurfacing by applying flames B23K7/00; working of metal by electro-erosion B23H; producing decorative effects by removing surface material, e.g. by engraving, by etching, B44C1/22; electrolytic etching or polishing C25F); INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION IN GENERAL; MULTI-STEP PROCESSES FOR SURFACE TREATMENT OF METALLIC MATERIAL INVOLVING AT LEAST ONE PROCESS PROVIDED FOR IN CLASS C23 AND AT LEAST ONE PROCESS COVERED BY SUBCLASS C21D OR C22F OR CLASS C25

## Abstract

A method of fabricating a nitrided low-alloy steel part, includes a) decarburizing the surface of a low-alloy steel part including at least one alloying element that is both nitride-forming and carbide forming in order to obtain a decarburized part presenting a carbon-depleted surface layer of thickness less than or equal to 1.5 mm, the minimum content of carbon by weight in the carbon-depleted surface layer being less than or equal to 70% of the carbon content by weight in the core of the decarburized part; b) treating the decarburized part with quenching treatment followed by annealing treatment; and c) nitriding the carbon-depleted surface layer in order to obtain a nitrided low-alloy steel part, step c) being performed after step b).

## Claims

### Claim 1

A method of fabricating a nitrided low-alloy steel part, the method comprising:
a) decarburizing the surface of a low-alloy steel part including at least one alloying element that is both nitride-forming and carbide-forming in order to obtain a decarburized part presenting a carbon-depleted surface layer of thickness less than or equal to 1.5 mm, the minimum content of carbon by weight in the carbon-depleted surface layer being less than or equal to 70% of the carbon content by weight in the core of the decarburized part, and the minimum content of carbon by weight in the carbon-depleted surface layer being greater than or equal to 0.05%;
b) treating the decarburized part with quenching treatment followed by annealing treatment; and
c) nitriding the carbon-depleted surface layer in order to obtain a nitrided low-alloy steel part, step c) being performed after step b).

### Claim 2 (depends on 1)

A method according to claim 1, wherein the thickness of the carbon-depleted surface layer lies in the range 0.3 mm to 1.5 mm.

### Claim 3 (depends on 1)

A method according to claim 1, wherein, prior to step c), a step is performed of machining the carbon-depleted surface layer.

### Claim 4 (depends on 1)

A method according to claim 1, wherein, after step c), a step is performed of machining the nitrided layer formed during step c).

### Claim 5 (depends on 1)

A method according to claim 1, wherein the treated low-alloy steel part is made of 32CrMoV13 steel.

### Claim 6

A decarburized low-alloy steel part including at least one alloying element that is both nitride-forming and carbide-forming, presenting a carbon-depleted surface layer of thickness less than or equal to 1.5 mm that is to be subjected to nitriding, the minimum carbon content by weight in the carbon-depleted surface layer being less than or equal to 70% of the carbon content by weight in the core of the decarburized part, and the minimum content of carbon by weight in the carbon-depleted surface layer being greater than or equal to 0.05%.

### Claim 7 (depends on 6)

A part according to claim 6, wherein the carbon-depleted surface layer presents a thickness lying in the range 0.3 mm to 1.5 mm.

### Claim 8 (depends on 6)

A part according to claim 6, wherein the low-alloy steel is 32CrMoV13 steel.