# US 2016/0237269 A1 · Long-fiber-reinforced resin composition and molded article thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0237269 A1
- Document ID: US20160237269A1
- Status: Published application
- Kind: A1
- Application number: 15/139,547
- Filed: 2016-04-27
- Published: 2016-08-18
- Earliest claimed: 2008-03-21
- Assignees: Prime Polymer Co., Ltd.
- Applicants: Prime Polymer Co., Ltd.
- Inventors: Hirofumi GODA; Toru IWASHITA
- Web page: https://patentgrep.com/patent/US20160237269A1

## CPC

- C08L 23/12: Polypropene
- C08K 5/14: Peroxides
- C08L 23/02: not modified by chemical after-treatment
- C08L 23/10: Homopolymers or copolymers of propene
- C08L 51/003: {grafted on to macromolecular compounds obtained by reactions only involving unsaturated carbon-to-carbon bonds (C08L51/04, C08L51/06 take precedence)}
- C08K 7/14: Glass
- C08L 2203/12: used for fibers
- C08L 2205/02: containing two or more polymers of the same C08L -group
- C08L 2205/025: containing two or more polymers of the same hierarchy C08L, and differing only in parameters such as density, comonomer content, molecular weight, structure
- C08L 2205/03: containing three or more polymers in a blend
- C08L 2205/16: Fibres; Fibrils
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)

## Abstract

A long-fiber-reinforced resin composition including the following component (A) and the component (B), the content of the component (A) being 50 to 90 wt % and the content of the component (B) being 10 to 50 wt %; and the content of reinforcing fiber contained in the component (A) being 20 to 60 wt % relative to the total amount of the fiber-reinforced resin composition: [Component (A)] a long-fiber-reinforced thermoplastic resin pellet including a thermoplastic resin, a modified polyolefin-based resin modified with an unsaturated carboxylic acid or its derivative and reinforcing fiber and satisfying the following (A-1) to (A-4): (A-1): the melt index of the thermoplastic resin (resin temperature: 230° C., load: 21.18N) is 100 to 250 g/10 min; (A-2): the relaxation time λ of the thermoplastic resin at an angular frequency ω=1 (rad/sec) calculated from the storage modulus G′ and the loss modulus G″ measured by means of a cone-and-plate rheometer is 0.1 (sec) or less; (A-3) the content of the reinforcing fiber is 40 to 70 wt %; and (A-4) the content of the modified polyolefin-based resin is 1 to 5 wt %; [Component (B)] a polyolefin-based resin satisfying the following (B-1) and (B-2): (B-1) the melt index of the polyolefin-based resin (resin temperature: 230° C., load: 21.18N) is 20 to 70 g/10 min; and (B-2) the relaxation time λ of the polyolefin-based resin at an angular frequency ω=1 (rad/sec) calculated from the storage modulus G′ and the loss modulus G″ measured by means of a cone-and-plate rheometer is 0.23 (sec) or less.

## Claims

### Claim 1

A long-fiber-reinforced resin composition comprising the following component (A) and the component (B),
the content of the component (A) being 50 to 90 wt % and the content of the component (B) being 10 to 50 wt %; and
the content of reinforcing fiber contained in the component (A) being 20 to 60 wt % relative to the total amount of the fiber-reinforced resin composition:
[Component (A)]
a long-fiber-reinforced thermoplastic resin pellet comprising a thermoplastic resin, a modified polyolefin-based resin modified with an unsaturated carboxylic acid or its derivative and reinforcing fiber and satisfying the following (A-1) to (A-4):
(A-1): the melt index of the thermoplastic resin (resin temperature: 230° C., load: 21.18N) is 100 to 250 g/10 min;
(A-2): the relaxation time λ of the thermoplastic resin at an angular frequency ω=1 (rad/sec) calculated from the storage modulus G′ and the loss modulus G″ measured by means of a cone-and-plate rheometer is 0.1 (sec) or less;
(A-3) the content of the reinforcing fiber is 40 to 70 wt %; and
(A-4) the content of the modified polyolefin-based resin is 1 to 5 wt %;
[Component (B)]
a polyolefin-based resin satisfying the following (B-1) and (B-2):
(B-1) the melt index of the polyolefin-based resin (resin temperature: 230° C., load: 21.18N) is 20 to 70 g/10 min; and
(B-2) the relaxation time λ of the polyolefin-based resin at an angular frequency ω=1 (rad/sec) calculated from the storage modulus G′ and the loss modulus G″ measured by means of a cone-and-plate rheometer is 0.23 (sec) or less.

### Claim 2 (depends on 1)

The long-fiber-reinforced resin composition according to claim 1, wherein the long-fiber-reinforced thermoplastic resin pellet further satisfies the following (A-5):
(A-5): the pellet length of the long-fiber-reinforced thermoplastic resin pellet is 4 mm to 8 mm.

### Claim 3 (depends on 1)

The long-fiber-reinforced resin composition according to claim 1, wherein the reinforcing fiber is glass fiber and the thermoplastic resin is a polyolefin-based resin.

### Claim 4 (depends on 1)

A molded article formed from the long-fiber-reinforced resin composition according to claim 1.