# US 2016/0237194 A1 · A method for increasing the reactivity of lignin

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0237194 A1
- Document ID: US20160237194A1
- Status: Published application
- Kind: A1
- Application number: 15/024,725
- Filed: 2014-09-29
- Published: 2016-08-18
- Earliest claimed: 2013-09-30
- Assignees: Upm-Kymmene Corporation
- Applicants: Upm-Kymmene Corporation
- Inventors: Suvi PIETARINEN; Sanna VALKONEN; Okko RINGENA
- Web page: https://patentgrep.com/patent/US20160237194A1

## CPC

- C08G 8/38: Block or graft polymers prepared by polycondensation of aldehydes or ketones onto macromolecular compounds
- B27N 3/002: {characterised by the type of binder (compositions of macromolecular compounds C08L)}
- C08G 8/20: with polyhydric phenols
- C08H 6/00: {Macromolecular compounds derived from lignin, e.g. tannins, humic acids}
- C08L 97/02: Lignocellulosic material, e.g. wood, straw or bagasse {(manufacture of articles made from lignocellulosic material by dry processes B27N)}
- C09J 161/06: of aldehydes with phenols
- C09J 161/12: with polyhydric phenols
- C09J 197/005: {Lignin}
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- B27N: MANUFACTURE BY DRY PROCESSES OF ARTICLES, WITH OR WITHOUT ORGANIC BINDING AGENTS, MADE FROM PARTICLES OR FIBRES CONSISTING OF WOOD OR OTHER LIGNOCELLULOSIC OR LIKE ORGANIC MATERIAL (containing cementitious material B28B; shaping of substances in a plastic state B29C; fibreboards made from fibrous suspensions D21J; drying F26B17/00)
- C08H: DERIVATIVES OF NATURAL MACROMOLECULAR COMPOUNDS (polysaccharides C08B; natural rubber C08C; natural resins or their derivatives C09F; bituminous materials C10)
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- C09J: ADHESIVES; NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL; ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE; USE OF MATERIALS AS ADHESIVES (preparation of glue or gelatine C09H)

## Abstract

The present invention relates to a method for increasing the reactivity of lignin, wherein the method comprises the following steps: a) forming, under heating at a temperature of 71-94° C., an aqueous dispersion comprising alkali and lignin, wherein the alkali comprises a hydroxide of an alkali metal; and b) heating the dispersion formed in step a) at a temperature of 50-95° C. for producing alkalated lignin.

## Claims

### Claim 1

A method for increasing the reactivity of lignin, characterized in that the method comprises the following steps:
a) forming, under heating at a temperature of 71-94° C., an aqueous dispersion comprising alkali and lignin, wherein the alkali comprises a hydroxide of an alkali metal; and
b) heating the dispersion formed in step a) at a temperature of 50-95° C. for producing alkalated lignin

### Claim 2 (depends on 1)

The method of claim 1, characterized in that the concentration of alkali is 5-50 weight-%, based on the total weight of the dispersion in step a).

### Claim 3 (depends on 1)

The method of claim 1 2, characterized in that the concentration of lignin is 10-50 weight-%, based on the total weight of the dispersion in step a).

### Claim 4 (depends on 1)

The method of claim 1, characterized in that the temperature in step a) is 71-90° C.

### Claim 5 (depends on 1)

The method of claim 1, characterized in that the temperature in step b) is 60-85° C.

### Claim 6 (depends on 1)

The method of claim 1, characterized in that step b) is carried out for 15 minutes-24 hours.

### Claim 7 (depends on 1)

The method of claim 1, characterized in that the method comprises, before step a), the step i) of reacting lignin with a compound selected from the class of phenols.

### Claim 8 (depends on 7)

The method of claim 7, characterized in that step i) is carried out at a temperature of 100-140° C. for 1-3 hours in the presence of a catalyst.

### Claim 9 (depends on 1)

The method of claim 1, characterized in that the method comprises, after step b), the step ii) of adding an aldehyde, a derivative of an aldehyde, or a combination thereof to the dispersion formed in step b).

### Claim 10 (depends on 9)

The method of claim 9, characterized in that the weight ratio of the aldehyde to the lignin in the dispersion from step b) is 0.2-0.7.

### Claim 11 (depends on 9)

The method of claim 9, characterized in that the aldehyde is formaldehyde.

### Claim 12 (depends on 1)

Lignin obtainable by the method of claim 1.

### Claim 13 (depends on 1)

A method for producing a binder composition, characterized in that the method comprises the step of:
(iii) cooking an aqueous composition comprising reactant components including lignin obtainable by the method of claim 1, a polymerizable substance and a crosslinking agent in the presence of a catalyst at a temperature of 60-95° C. for polymerizing the reactant components until a binder composition with a predetermined viscosity value is formed.

### Claim 14 (depends on 13)

The method of claim 13, characterized in that step (iii) comprises cooking the composition at a temperature of 65-90° C.

### Claim 15 (depends on 13)

The method of claim 13, characterized in that the crosslinking agent is an aldehyde.

### Claim 16 (depends on 13)

The method of claim 13, characterized in that the polymerizable substance is selected from a group consisting of phenol, cresol, resorcinol and combinations thereof.

### Claim 17 (depends on 13)

The method of claim 13, characterized in that the catalyst is selected from a group consisting of sodium hydroxide, potassium hydroxide and any mixture thereof.

### Claim 18 (depends on 13)

A binder composition obtainable by the method of claim 13.

### Claim 19 (depends on 18)

An adhesive composition comprising the binder composition of claim 18.

### Claim 20

(canceled)

### Claim 21

(canceled)