# US 2016/0236970 A1 · Transparent glass-ceramic articles, glass-ceramic precursor glasses and methods for forming the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0236970 A1
- Document ID: US20160236970A1
- Status: Published application
- Kind: A1
- Application number: 15/142,654
- Filed: 2016-04-29
- Published: 2016-08-18
- Earliest claimed: 2014-05-13
- Assignees: Corning Incorporated
- Applicants: Corning Incorporated
- Inventors: George Halsey Beall; Charlene Marie Smith; Steven Alvin Tietje
- Web page: https://patentgrep.com/patent/US20160236970A1

## CPC

- C03C 10/0018: {containing SiO2, Al2O3 and monovalent metal oxide as main constituents}
- C03B 32/02: Thermal crystallisation, e.g. for crystallising glass bodies into glass-ceramic articles {(C03B27/012 takes precedence)}
- C03C 3/062: with less than 40% silica by weight
- C03C 3/064: containing boron
- C03C 3/097: containing phosphorus, niobium or tantalum
- C03C 4/18: for ion-sensitive glass
- C03C 21/00: Treatment of glass, not in the form of fibres or filaments, by diffusing ions or metals in the surface
- C03C 21/002: {to perform ion-exchange between alkali ions (C03C21/005 takes precedence)}
- C03C 2204/00: Glasses, glazes or enamels with special properties
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- C03B: MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES

## Abstract

Embodiments of glass ceramic articles and precursor glasses are disclosed. In one or more embodiments, the glass-ceramic articles are transparent and include a nepheline phase and a phosphate phase. The glass-ceramic articles are colorless and exhibit a transmittance of about 70% or greater across the visible spectrum. The glass-ceramic articles may optionally include a lithium aluminosilicate phase. The crystals of the glass-ceramic articles may have a major cross-section of about 100 nm or less.

## Claims

### Claim 1

A device comprising:
a glass-ceramic article comprising:
a major nepheline phase; and
a minor phosphate phase,
wherein the glass-ceramic article is colorless and has transmission or reflection color coordinates under the CIE L*, a*, b* colorimetry system of L* in the range from about 80 to about 100, a* in the range from about −5 to about 5, and b* in the range from about b* in the range from about −5 to about 5, and exhibits a transmittance of about 70% or greater across the visible spectrum, in the range from about 390 nm to about 700 nm,
wherein the device comprises any one of an electronic device, an automotive application, an architectural applications and an energy production application.

### Claim 2 (depends on 1)

The device of claim 1, wherein the device comprises an electronic device selected from the group comprising, a mouse, a keyboard, a monitor, a tablet, a whiteboard, a personal digital assistant, a navigation device an inventory device, a media player, an electronic reader, a mobile phone and a smart phone.

### Claim 3 (depends on 2)

The device of claim 2, wherein the glass-ceramic article further comprises a lithium aluminosilicate phase.

### Claim 4 (depends on 2)

The device of claim 2, wherein at least one of the nepheline phase and the phosphate phase comprises a plurality of nanocrystals having a major cross-sectional dimension of about 100 nm or less.

### Claim 5 (depends on 4)

The device of claim 4, wherein the plurality of nanocrystals form at least one of the nepheline phase, the phosphate phase and the lithium aluminosilicate phase, and the plurality of nanocrystals have a major cross-sectional dimension of about 100 nm or less.

### Claim 6 (depends on 5)

The device of claim 5, wherein the plurality of nanocrystals form the nepheline phase, the phosphate phase and the lithium aluminosilicate phase.

### Claim 7 (depends on 2)

The device of claim 2, wherein the glass-ceramic article comprises a composition, the composition comprising, in mol %:
SiO2 in the range from about 35 to about 60,
Al2O3 in the range from about 10 to about 30,
Na2O in the range from about 7 to about 31,
K2O in the range from about 0 to about 20,
Li2O in the range from about 0 to about 20,
P2O5 in the range from about 1.5 to about 8, and
a rare earth oxide in the range from about 0 to about 6.

### Claim 8 (depends on 7)

The device of claim 7, wherein the composition further comprises at least one oxide in an amount in the range from 0 mol % to about 8 mol %, wherein the at least one oxide comprises one of B2O3, MgO, CaO, SrO, BaO, and ZrO2.

### Claim 9 (depends on 2)

The device of claim 2, wherein the glass-ceramic article further comprises a composition, the composition comprising, in mol %:
SiO2 in the range from about 40 to about 55,
Al2O3 in the range from about 14 to about 21,
Na2O in the range from about 13 to about 29,
K2O in the range from about 2 to about 14,
Li2O in the range from about 0 to about 10,
P2O5 in the range from about 2.5 to about 5, and
at least one of ZrO2, Y2O3 and La2O3 in an amount in the range from about 0 to about 4.

### Claim 10 (depends on 7)

The device of claim 7, wherein the composition comprises less than about 1 mol % TiO2.

### Claim 11 (depends on 2)

The device of claim 2, wherein the nepheline phase comprises a solid solution.

### Claim 12 (depends on 1)

The device of claim 1, wherein the glass-ceramic article further comprises a compressive stress layer, the compressive stress layer optionally comprising kalsilite.

### Claim 13 (depends on 1)

The device of claim 1, wherein the glass-ceramic article further comprises an average surface compressive stress of about 400 MPa or greater.

### Claim 14 (depends on 2)

The device of claim 2, wherein the glass-ceramic article further comprises a compressive stress layer, the compressive stress layer optionally comprising kalsilite.

### Claim 15 (depends on 2)

The device of claim 2, wherein the glass-ceramic article further comprises an average surface compressive stress of about 400 MPa or greater.

### Claim 16

A glass comprising a composition, in mol %, comprising:
SiO2 in the range from about 35 to about 60,
Al2O3 in the range from about 10 to about 30,
Na2O in the range from about 7 to about 31,
K2O in the range from about 0 to about 20,
Li2O in the range from about 0 to about 20,
P2O5 in the range from about 1.5 to about 8, and
a rare earth oxide in the range from about 0 to about 6.

### Claim 17 (depends on 16)

The glass of claim 16, wherein the composition further comprises at least one oxide in an amount in the range from 0 mol % to about 8 mol %, wherein the at least one oxide comprises one of B2O3, MgO, CaO, SrO, BaO, and ZrO2.

### Claim 18 (depends on 16)

The glass of claim 16, wherein the composition further comprises, in mol %:
SiO2 in the range from about 40 to about 55,
Al2O3 in the range from about 14 to about 21,
Na2O in the range from about 13 to about 29,
K2O in the range from about 2 to about 14,
Li2O in the range from about 0 to about 10,
P2O5 in the range from about 2.5 to about 5, and
at least one of ZrO2, Y2O3 and La2O3 in an amount in the range from about 0 to about 4,
wherein the composition comprises less than about 1 mol % TiO2.

### Claim 19 (depends on 16)

The glass of claim 16, further comprising a compressive stress layer having a surface compressive stress in the range from about 200 MPa to about 600 MPa and a depth of layer in the range from about 50 μm to about 150 μm.

### Claim 20 (depends on 16)

The glass of claim 16, wherein the glass comprises a glass sheet having a thickness of less than about 5 mm.

### Claim 21 (depends on 20)

The glass of claim 20, wherein the glass sheet comprising a compressive stress layer having a surface compressive stress in the range from about 200 MPa to about 600 MPa and a depth of layer in the range from about 50 μm to about 150 μm

### Claim 22

A method of forming a glass ceramic comprising:
heat treating a precursor glass article by heating the at a rate in the range from about 1° C./minute to about 10° C./minute to a temperature in the range from about 600° to about 1000° C.; and cooling the glass-ceramic article to about room temperature,
wherein heating treating the precursor glass article comprises any one or more of:
a) heating the precursor glass article to a nucleating temperature (Tn) in the range from about 700° C. to about 900° C.,
b) maintaining the precursor glass article at the Tn to produce a nucleated precursor glass article,
c) heating the nucleated precursor glass article at a rate in the range from about 1° C./minute to about 10° C./minute to a crystallization temperature (Tc) in the range from about 600° to about 1000° C., and
d) maintaining the nucleated precursor glass article at the Tc to produce a glass-ceramic article having a nepheline crystalline phase.

### Claim 23 (depends on 22)

The method of claim 22, further comprising ion exchanging the glass-ceramic article to generate a compressive stress layer comprising a compressive stress of at least 400 MPa.

### Claim 24 (depends on 22)

The method of claim 22, further comprising ion exchanging the glass-ceramic article to generate a kalsilite surface layer.