# US 2016/0221858 A1 · Reforming mandrel geometry for flatness control

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0221858 A1
- Document ID: US20160221858A1
- Status: Published application
- Kind: A1
- Application number: 15/006,615
- Filed: 2016-01-26
- Published: 2016-08-04
- Earliest claimed: 2015-01-30
- Assignees: Corning Incorporated
- Applicants: Corning Incorporated
- Inventors: Thierry Luc Alain Dannoux; Mickaël Mabrut; Ronan Tanguy
- Web page: https://patentgrep.com/patent/US20160221858A1

## CPC

- C03B 23/045: Tools or apparatus specially adapted for re-forming tubes or rods in general, e.g. glass lathes, chucks (C03B23/043 takes precedence)
- C03B 17/04: Forming tubes or rods by drawing from stationary or rotating tools or from forming nozzles
- C03B 23/0476: {onto a forming die, e.g. a mandrel or a wire}
- C03B 23/09: Reshaping the ends, e.g. as grooves, threads or mouths
- C03B 40/04: using gas
- Y02P 40/57: Improving the yield, e-g- reduction of reject rates
- C03B: MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A reforming mandrel and a method of use reforming mandrel to reform glass are described. The reforming mandrel comprises an upstream portion, a downstream portion and an at least partially hollow interior. The upstream portion may have an intake inlet for fluid flow. The downstream portion may be axially spaced from the upstream portion. The downstream portion may have a flattened cross-section defined by flattened peripheral portions joined by curved peripheral portions. At least one curved peripheral portion may be made of porous material resistant to a temperature of at least 1000° C. The at least partially hollow interior may communicate with the intake inlet and the porous material.

## Claims

### Claim 1

A reforming mandrel comprising:
an upstream portion having an intake inlet for fluid flow;
a downstream portion axially spaced from the upstream portion, the downstream portion having a flattened cross-section defined by flattened peripheral portions joined by curved peripheral portions, at least one curved peripheral portion made of porous material resistant to a temperature of at least 1000° C.; and at least partially hollow interior communicating with the intake inlet and the porous material.

### Claim 2 (depends on 1, 2)

The reforming mandrel of claim 1, wherein the porous material comprises carbon. The reforming mandrel of claim 2, wherein the porous material comprises graphite.

### Claim 4 (depends on 1)

The reforming mandrel of claim 1, wherein the porous material is resistant to a temperature of at least 1200° C.

### Claim 5 (depends on 1)

The reforming mandrel of claim 1, wherein the intake inlet is configured to allow gas to enter into the at least partially hollow interior and wherein the porous material is configured to allow gas to permeate to an exterior of the reforming mandrel.

### Claim 6 (depends on 1)

The reforming mandrel of claim 1, wherein the at least one curved peripheral portion comprises at least one passage, the at least one passage communicating with the at least partially hollow interior.

### Claim 7 (depends on 6)

The reforming mandrel of claim 6, wherein the at least one passage comprises a first passage and a second passage, the first passage having a first corresponding exterior surface, the second passage having a second corresponding exterior surface, wherein the first corresponding exterior surface is progressively reduced to the flattened cross-section via a second corresponding exterior surface.

### Claim 8 (depends on 1)

The reforming mandrel of claim 1, wherein two flattened peripheral portions are separated by a first width, and wherein the at least one curved peripheral portion has a second width that is greater than the first width.

### Claim 9 (depends on 8)

The reforming mandrel of claim 8, comprising two curved peripheral portions separated by the flattened peripheral portions, wherein there is a corner between each flattened peripheral portion and each curved peripheral portion and further wherein at least one passage is provided adjacent to each corner.

### Claim 10 (depends on 5)

The reforming mandrel of claim 5, wherein the intake inlet is configured to allow gas to enter into the at least partially hollow interior and wherein the porous material and at least one passage are each configured to allow gas to permeate to an exterior of the reforming mandrel.

### Claim 11 (depends on 10)

The reforming mandrel of claim 10, wherein the gas is at a gas pressure when it reaches the exterior of the reforming mandrel and wherein the gas pressure is higher adjacent to each corner than it is away from each corner.

### Claim 12

A method for producing a glass sleeve with a flattened portion comprising:
a. providing a substantially cylindrical glass tube made of glass, the substantially cylindrical tube having a longitudinal axis and an inner curved surface enclosing a space;
b. heating at least a portion of the substantially cylindrical tube to a temperature within the softening range of the glass;
c. moving the softened substantially cylindrical tube over a reforming mandrel to reform the glass tube into a glass sleeve with a flattened portion;
wherein the reforming mandrel comprises an upstream portion having an intake inlet for fluid flow, a downstream portion axially spaced from the upstream portion, the downstream portion having a flattened cross-section defined by flattened peripheral portions joined by curved peripheral portions, at least one curved peripheral portion made of porous material resistant to a temperature of at least 1000° C., and an at least partially hollow interior communicating with the intake inlet and the porous material.

### Claim 13 (depends on 12)

The method of claim 12, wherein the porous material is resistant to a temperature of at least 1200° C.

### Claim 14 (depends on 12)

The method of claim 12, further comprising allowing gas to enter through the intake inlet into the at least partially hollow interior and permeate to an exterior of the reforming mandrel through the porous material.

### Claim 15 (depends on 12)

The method of claim 12, wherein the at least one curved peripheral portion comprises at least one passage, the at least one passage communicating with the at least partially hollow interior.

### Claim 16 (depends on 15)

The method of claim 15, wherein the at least one passage comprises a first passage and a second passage, the first passage having a first corresponding exterior surface, the second passage having a second corresponding exterior surface, wherein the first corresponding exterior surface is progressively reduced to the flattened cross-section via the second corresponding exterior surface.

### Claim 17 (depends on 12)

The method of claim 12, wherein two flattened peripheral portions are separated by a first width, and wherein the at least one curved peripheral portion has a second width that is greater than the first width.

### Claim 18 (depends on 17)

The method of claim 17, wherein the reforming mandrel further comprises two curved peripheral portions separated by the flattened peripheral portions, wherein there is a corner between each flattened peripheral portion and each curved peripheral portion and further wherein at least one passage is provided adjacent to each corner.

### Claim 19 (depends on 18)

The method of claim 18, further comprising allowing gas to enter through the intake inlet into the at least partially hollow interior and permeating to an exterior of the reforming mandrel through the porous material and at least one passage.

### Claim 20 (depends on 19)

The method of claim 19, wherein the gas is at a gas pressure when it reaches the exterior of the reforming mandrel and wherein the gas pressure is higher adjacent to each corner than it is away from each corner.