# US 2016/0145765 A1 · Garnet single crystal and method for producing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0145765 A1
- Document ID: US20160145765A1
- Status: Published application
- Kind: A1
- Application number: 14/787,954
- Filed: 2014-03-20
- Published: 2016-05-26
- Earliest claimed: 2013-06-17
- Assignees: Sumitomo Metal Mining Co., Ltd.
- Applicants: Sumitomo Metal Mining Co., Ltd
- Inventors: Masayoshi MATSUI; Kazuki TATSUMIYA; Fumiaki ISHIDA
- Web page: https://patentgrep.com/patent/US20160145765A1

## CPC

- C30B 15/30: Mechanisms for rotating or moving either the melt or the crystal (flotation methods C30B15/28)
- C30B 15/20: Controlling or regulating (controlling or regulating in general G05)
- C30B 29/20: Aluminium oxides
- C30B 29/28: with formula A3Me5O12 wherein A is a rare earth metal and Me is Fe, Ga, Sc, Cr, Co or Al, e.g. garnets
- G02F 1/0036: {Magneto-optical materials}
- G02F 1/093: {used as non-reciprocal devices, e.g. optical isolators, circulators (G02F1/0955 takes precedence)}
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR
- G02F: OPTICAL DEVICES OR ARRANGEMENTS FOR THE CONTROL OF LIGHT BY MODIFICATION OF THE OPTICAL PROPERTIES OF THE MEDIA OF THE ELEMENTS INVOLVED THEREIN; NON-LINEAR OPTICS; FREQUENCY-CHANGING OF LIGHT; OPTICAL LOGIC ELEMENTS; OPTICAL ANALOGUE/DIGITAL CONVERTERS

## Abstract

[Object] To provide a high-quality, transparent garnet single crystal with suppressed cell growth that would otherwise lead to partially inhomogeneous crystal composition, and a method for producing the garnet single crystal. [Solving means] The garnet single crystal is grown by bringing a seed crystal into contact with a raw-material melt in a crucible disposed inside a chamber and pulling, while rotating, the seed crystal. The garnet single crystal is characterized by being represented by a general formula: (Tb3-xScx) (Sc2-yAly)Al3O12-z (provided that 0.11≦x≦0.14, and 0.17≦y≦0.23). The garnet single crystal is grown as follows. First, a mixture powder containing 20.9 to 21.2% by mole terbium oxide, 32.7 to 33.3% by mole scandium oxide, and the balance of aluminium oxide and unavoidable impurities is filled into the crucible and melted. Then, while a nitrogen gas is supplied into the chamber, the number of rotations of the seed crystal is set to 5 to 20 rpm, and the rate of pulling the seed crystal is set to 0.3 to 0.8 mm/h for the growth.

## Claims

### Claim 1

A garnet single crystal characterized in that the garnet single crystal is represented by the following general formula:
(Tb3-xScx)(Sc2-yAly)Al3O12-z (1)
(where x satisfies 0.11≦x≦0.14, and y satisfies 0.17≦y≦0.23).

### Claim 2 (depends on 1)

A method for producing a garnet single crystal using a growth furnace including a crucible in a cylindrical chamber by a Czochralski process for growing a garnet single crystal by bringing a seed crystal into contact with a raw-material melt in the crucible and pulling, while rotating, the seed crystal, characterized in that the production method comprises:
preparing the raw-material melt by filling the crucible with a mixture powder containing 20.9 to 21.2% by mole terbium oxide, 32.7 to 33.3% by mole scandium oxide, and the balance of aluminium oxide and unavoidable impurities, followed by melting of the mixture powder; and
growing the garnet single crystal according to claim 1, while supplying an inert gas into the chamber, by setting conditions such that the number of rotations of the seed crystal is 20 rpm or less, and a rate of pulling the seed crystal is 0.8 mm/h or less.

### Claim 3 (depends on 2)

The method for producing a garnet single crystal according to claim 2, characterized in that the conditions are set such that
the number of rotations of the seed crystal is from 5 rpm or more to 20 rpm or less, and
the rate of pulling the seed crystal is from 0.3 mm/h or more to 0.8 mm/h or less.

### Claim 4 (depends on 2)

The method for producing a garnet single crystal according to claim 2, characterized in that the inert gas is supplied into the chamber at a flow rate of from 3 L/min or more to 6 L/min or less.

### Claim 5 (depends on 3)

The method for producing a garnet single crystal according to claim 3, characterized in that the inert gas is supplied into the chamber at a flow rate of from 3 L/min or more to 6 L/min or less.

### Claim 6 (depends on 2)

The method for producing a garnet single crystal according to claim 2, characterized in that the inert gas is a nitrogen gas.

### Claim 7 (depends on 3)

The method for producing a garnet single crystal according to claim 3, characterized in that the inert gas is a nitrogen gas.

### Claim 8 (depends on 4)

The method for producing a garnet single crystal according to claim 4, characterized in that the inert gas is a nitrogen gas.

### Claim 9 (depends on 5)

The method for producing a garnet single crystal according to claim 5, characterized in that the inert gas is a nitrogen gas.