# US 2016/0145706 A1 · High-strength steel sheet and manufacturing method therefor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0145706 A1
- Document ID: US20160145706A1
- Status: Published application
- Kind: A1
- Application number: 14/392,119
- Filed: 2014-06-27
- Published: 2016-05-26
- Earliest claimed: 2013-06-27
- Assignees: Hyundai Steel Company
- Applicants: Hyundai Steel Company
- Inventors: Jun Ho Chung; Seong-Ju Kim; Hyo Dong Shin
- Web page: https://patentgrep.com/patent/US20160145706A1

## CPC

- C21D 9/46: for sheet metals
- C21D 1/26: Methods of annealing
- C21D 6/002: {containing Cr (C21D6/004 takes precedence)}
- C21D 6/005: {containing Mn}
- C21D 8/02: during manufacturing of plates or strips (C21D8/12 takes precedence)
- C21D 8/0226: {Hot rolling}
- C21D 8/0236: {Cold rolling}
- C21D 8/0247: characterised by the heat treatment
- C21D 8/0263: {following hot rolling}
- C22C 38/001: {containing N}
- C22C 38/04: containing manganese
- C22C 38/06: containing aluminium
- C22C 38/12: containing tungsten, tantalum, molybdenum, vanadium, or niobium
- C22C 38/22: with molybdenum or tungsten
- C22C 38/24: with vanadium
- C22C 38/26: with niobium or tantalum
- C22C 38/38: with more than 1.5% by weight of manganese
- C22C 38/58: with more than 1.5% by weight of manganese
- C21D 2211/001: Austenite
- C21D 2211/004: Dispersions; Precipitations
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

A high-strength steel sheet according to the present invention comprises, by weight, 10.0-15.0% Mn, 6.0-9.0% Al, 0.5-2.0% Cr, 0.8-1.6% C, and 0.001-0.01% N, and further comprises, by weight, 0.02-0.1% V, 0.005-0.015% Nb, and 0.005-0.02% Mo, or further comprises 0.1-0.5 wt % TiAl particles. The high-strength steel sheet has a mixed structure comprising austenite and a fine k-carbide having a mean particle diameter of 10-500 nm.

## Claims

### Claim 1

A high-strength steel sheet comprising, by weight, 10.0-15.0% manganese (Mn), 6.0-9.0% aluminum (Al), 0.5-2.0% chromium (Cr), 0.8-1.6% carbon (C), 0.001-0.01% nitrogen (N), 0.02-0.1% vanadium (V), 0.005-0.015% niobium (Nb), and 0.005-0.02% molybdenum (Mo), with the remainder being iron (Fe) and inevitable impurities, and the steel sheet having a mixed structure comprising austenite and a fine k-carbide ((Fe,Mn)3AlC) having a mean grain size of 10-500 nm.

### Claim 2 (depends on 1)

The high-strength steel sheet of claim 1, wherein a density of the high-strength steel sheet is 7.1 g/cm3 or lower.

### Claim 3 (depends on 1)

The high-strength steel sheet of claim 1, wherein the high-strength steel sheet is a cold-rolled steel sheet, the high-strength steel sheet having a tensile strength of 1000 MPa or higher and an elongation of 20% or higher.

### Claim 4 (depends on 1)

The high-strength steel sheet of claim 1, further comprising, by weight, 11.0-13.0% manganese (Mn), 6.0-7.5% aluminum (Al), 1.0-2.0% chromium (Cr), and 1.0-1.2% carbon (C).

### Claim 5

A high-strength steel sheet comprising, by weight, 10.0-15.0% manganese (Mn), 6.0-9.0% aluminum (Al), 0.5-2.0% chromium (Cr), 0.8-1.6% carbon (C), 0.001-0.01% nitrogen (N), and 0.1-0.5% TiAl particles, with the remainder being iron (Fe) and inevitable impurities, the steel sheet having a mixed structure comprising austenite and a fine k-carbide ((Fe,Mn)3AlC) having a mean grain size of 10-500 nm.

### Claim 6 (depends on 5)

The high-strength steel sheet of claim 5, wherein the high-strength steel sheet has a density of 7.1 g/cm3 or lower.

### Claim 7 (depends on 5)

The high-strength steel sheet of claim 5, wherein the high-strength steel sheet is a hot-rolled steel sheet, the high-strength steel sheet having a tensile strength of 1200 MPa or higher and a product of tensile strength and elongation being 35,000 MPa-% or higher.

### Claim 8 (depends on 5)

The high-strength steel sheet of claim 5, further comprising, by weight, 11.0-13.0% manganese (Mn), 6.0-7.5% aluminum (Al), 1.0-2.0% chromium (Cr), and 1.0-1.2% carbon (C).

### Claim 9

A method for producing a high-strength steel sheet, comprising:
hot-rolling a steel slab comprising, by weight, 10.0-15.0% manganese (Mn), 6.0-9.0% aluminum (Al), 0.5-2.0% chromium (Cr), 0.8-1.6% carbon (C), 0.001-0.01% nitrogen (N), 0.02-0.1% vanadium (V), 0.005-0.015% niobium (Nb), and 0.005-0.02% molybdenum (Mo), with the remainder being iron (Fe) and inevitable impurities, at a finish-rolling temperature equal to or higher than an Ar3 point of the steel slab to obtain hot-rolled steel sheet; and
coiling the hot-rolled steel sheet at a temperature between 300° C. and 700° C.

### Claim 10 (depends on 9)

The method of claim 9, further comprising:
cold-rolling the hot-rolled steel sheet to obtain a cold-rolled steel sheet; and
annealing the cold-rolled steel sheet at an austenite single-phase region temperature equal to or higher than the Ac3 point for about 100 to 300 seconds.

### Claim 11

A method for producing a high-strength steel sheet, comprising:
hot-rolling a steel slab comprising, by weight, 10.0-15.0% manganese (Mn), 6.0-9.0% aluminum (Al), 0.5-2.0% chromium (Cr), 0.8-1.6% carbon (C), 0.001-0.01% nitrogen (N), and 0.1-0.5% TiAl particles, with the remainder being iron (Fe) and inevitable impurities, at a finish-rolling temperature equal to or higher than an Ar3 point of the steel slab to obtain hot-rolled steel sheet; and
coiling the hot-rolled steel sheet at a temperature between 300° C. and 700° C.