# US 2016/0145703 A1 · HOT-FORGED TiAl-BASED ALLOY AND METHOD FOR PRODUCING THE SAME

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0145703 A1
- Document ID: US20160145703A1
- Status: Published application
- Kind: A1
- Application number: 14/898,257
- Filed: 2014-06-02
- Published: 2016-05-26
- Earliest claimed: 2013-06-19
- Assignees: National Institute for Materials Science
- Applicants: National Institute for Materials Science
- Inventors: Toshimitsu TETSUI
- Web page: https://patentgrep.com/patent/US20160145703A1

## CPC

- C21D 9/0068: {for particular articles not mentioned below}
- C21D 8/00: Modifying the physical properties of ferrous metals or ferrous alloys by deformation combined with, or followed by, heat treatment (hardening articles or materials formed by forging or rolling with no further heating beyond that required for the formation C21D1/02)
- C22C 14/00: Alloys based on titanium
- C22C 30/00: Alloys containing less than 50% by weight of each constituent
- C22F 1/04: of aluminium or alloys based thereon
- C22F 1/18: High-melting or refractory metals or alloys based thereon
- C22F 1/183: {of titanium or alloys based thereon}
- F01D 5/28: Selecting particular materials; {Particular measures relating thereto;} Measures against erosion or corrosion
- C22F 1/00: Changing the physical structure of non-ferrous metals or alloys by heat treatment or by hot or cold working (apparatus for mechanical working of metal B21, B23, B24)
- F05D 2220/30: in turbines
- F05D 2230/25: by forging
- F05D 2230/40: Heat treatment
- F05D 2240/30: Characteristics of rotor blades, i.e. of any element transforming dynamic fluid energy to or from rotational energy and being attached to a rotor
- F05D 2300/174: Titanium alloys, e.g. TiAl
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C22F: CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass, C23F17/00)
- F01D: NON-POSITIVE DISPLACEMENT MACHINES OR ENGINES, e.g. STEAM TURBINES (machines or engines for liquids F03; non-positive displacement pumps F04D)
- F05D: INDEXING SCHEME FOR ASPECTS RELATING TO NON-POSITIVE-DISPLACEMENT MACHINES OR ENGINES, GAS-TURBINES OR JET-PROPULSION PLANTS

## Abstract

Provided is a hot-forged TiAl-based alloy of the present invention containing 40 to 45 atom % of Al and additive elements in the following composition ratio (A) or (B), and the balance Ti with inevitable impurities: (A) Nb: 7 to 9 atom %, Cr: 0.4 to 4.0 atom %, Si: 0.3 to 1.0 atom %, and C: 0.3 to 1.0 atom %; and (B) at least one of Cr: 0.1 to 2.0 atom %, Mo: 0.1 to 2.0 atom %, Mn: 0.1 to 4.0 atom %, Nb: 0.1 to 8.0 atom %, and V: 0.1 to 8.0 atom %. The TiAl-based alloy is characterized by having a fine structure of densely arranged lamella grains that are laminated alternately with a Ti3Al phase (α2-phase) and a TiAl phase (γ-phase) and have an average grain size of 1 to 200 μm.

## Claims

### Claim 1

A TiAl-based alloy containing:
Al: 40 to 45 atom %, and
additive elements in the following composition ratio (A) or (B), and the balance Ti with inevitable impurities,
(A) Nb: 7 to 9 atom %,
Cr: 0.4 to 4.0 atom %,
Si: 0.3 to 1.0 atom %, and
C: 0.3 to 1.0 atom %;
(B) at least one of Cr: 0.1 to 2.0 atom %,
Mo: 0.1 to 2.0 atom %,
Mn: 0.1 to 4.0 atom %,
Nb: 0.1 to 8.0 atom %, and
V: 0.1 to 8.0 atom %,
wherein the TiAl-based alloy has a fine structure of densely arranged lamella grains that are laminated alternately with a Ti3Al phase (α2-phase) and a TiAl phase (γ-phase) and have an average grain size of 1 to 200 μm.

### Claim 2 (depends on 1)

A method for producing the TiAl-based alloy according to claim 1, comprising:
a process in which the TiAl-based alloy is held at a coexisting temperature range of a hexagonal close-packed structure phase (α-phase) and a body-centered cubic structure phase (β-phase) and is then subjected to hot forging; and
a process in which the hot-forged TiAl-based alloy material is held in a temperature range of from 1180° C. to 1290° C. for 0.5 to 20 hours and is subjected to a heat treatment at a cooling rate of from 0.3 [° C./min.] to 10 [° C./min.] at the same time.

### Claim 3 (depends on 1)

The TiAl-based alloy according to claim 1, consisting of:
Al: 41 to 45 atom %,
Nb: 7 to 9 atom %,
Cr: 0.4 to 4.0 atom %,
Si: 0.3 to 1.0 atom %, and
C: 0.3 to 1.0 atom %,
and the balance Ti with inevitable impurities,
wherein an alloy element parameter P obtained by the following formula is in the composition range of from 1.1 to 2.3;
P=(41-Al)/3+0.25Nb+0.8Cr-0.8Si-1.7C, and
the TiAl-based alloy has a fine structure in which lamella grains laminated alternately with a Ti3Al phase (α2-phase) and a TiAl phase (γ-phase) are densely arranged and a β-phase is not included, the lamella grains having an average grain size of 1 to 200 μm.

### Claim 4 (depends on 3)

The TiAl-based alloy according to claim 3, further containing 0.1 to 3 atom % total of at least one element selected from the group consisting of W, Mo, B, Hf, Ta, and Zr.

### Claim 5 (depends on 3)

A method for producing a TiAl-based alloy, comprising:
a process in which the TiAl-based alloy according to claim 3 is held at a coexisting temperature range of a hexagonal close-packed structure phase (α-phase) and a body-centered cubic structure phase (β-phase) and is then subjected to hot forging; and
a process in which the hot-forged TiAl-based alloy material is held in a temperature range of from 1230° C. to 1290° C. for 1 to 20 hours and is subjected to a heat treatment at a cooling rate of from 1 [° C./min.] to 10 [° C./min.] at the same time.

### Claim 6 (depends on 5)

The method for producing the TiAl-based alloy according to claim 5, wherein
in the TiAl-based alloy, after the β-phase existing in the forged material is eliminated and thus an α-single phase is once obtained in the process of the heat treatment, transformation of α→α+γ→α2+γ occurs.

### Claim 7 (depends on 3)

A rotor blade for turbine that uses the TiAl-based alloy material produced in such a manner that an ingot having the composition according to claim 3 is produced by a production method comprising:
a process in which the TiAl-based alloy according to claim 3 is held at a coexisting temperature range of a hexagonal close-packed structure phase (α-phase) and a body-centered cubic structure phase (β-phase) and is then subjected to hot forging; and
a process in which the hot-forged TiAl-based alloy material is held in a temperature range of from 1230° C. to 1290° C. for 1 to 20 hours and is subjected to a heat treatment at a cooling rate of from 1 [° C./min.] to 10 [° C./min.] at the same time.

### Claim 8 (depends on 7)

A turbine that uses the rotor blade for turbine according to claim 7.

### Claim 9 (depends on 1)

The TiAl-based alloy according to claim 1, wherein the TiAl-based alloy consists of Al: 40.0 to 42.8 atom % and a Cr equivalent being 1.2 to 2.0 atom % that is obtained by the following formula, and the balance Ti with inevitable impurities;
Cr equivalent=Cr+Mo+0.5Mn+0.25Nb+0.25V, and
the TiAl-based alloy has a fine structure of densely arranged lamella grains that are laminated alternately with a α2-phase and a γ-phase and have an average grain size of 30 to 200 μm.

### Claim 10 (depends on 9)

A method for producing the TiAl-based alloy according to claim 9 that has the fine structure of densely arranged lamella grains that are laminated alternately with the α2-phase and the γ-phase and have the average grain size of 30 to 200 μm, the method comprising:
a process in which the TiAl-based alloy material is held at a coexisting temperature range of an α-phase and a β-phase and is then subjected to hot forging, the TiAl-based alloy material consisting of Al: 40.0 to 42.8 atom % and a Cr equivalent being 1.2 to 2.0 atom % that is obtained by the following formula, and the balance Ti with inevitable impurities;
Cr equivalent=Cr+Mo+0.5Mn+0.25Nb+0.25V, and
a process in which the hot-forged TiAl-based alloy material is held in a temperature range of from 1180° C. to 1260° C. for 0.5 to 20 hours and is subjected to a heat treatment at a cooling rate of from 0.3 [° C./min.] to 10 [° C./min.] at the same time.

### Claim 11 (depends on 10)

The method for producing the TiAl-based alloy according to claim 10, wherein transformation of a α→α+γ→α2+γ occurs in the TiAl-based alloy material during the heat treatment process.