# US 2016/0145701 A1 · Stainless steel resistant to delayed cracking and a method for its production

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0145701 A1
- Document ID: US20160145701A1
- Status: Published application
- Kind: A1
- Application number: 14/901,553
- Filed: 2014-06-19
- Published: 2016-05-26
- Earliest claimed: 2013-07-05
- Assignees: Outokumpu Oyj
- Applicants: Outokumpu Oyj
- Inventors: Juho Talonen
- Web page: https://patentgrep.com/patent/US20160145701A1

## CPC

- C21D 3/06: Extraction of hydrogen
- C21D 1/74: Methods of treatment in inert gas, controlled atmosphere, vacuum or pulverulent material
- C21D 6/001: {containing Ni (C21D6/004 takes precedence)}
- C21D 6/002: {containing Cr (C21D6/004 takes precedence)}
- C21D 6/005: {containing Mn}
- C21D 8/0436: {Cold rolling}
- C22C 38/001: {containing N}
- C22C 38/02: containing silicon
- C22C 38/40: with nickel
- C22C 38/42: with copper
- C22C 38/58: with more than 1.5% by weight of manganese
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

The invention relates to a stainless steel exhibiting transformation-induced plasticity (TRIP) effect resistant to delayed cracking and to the method for producing the stainless steel. The resistance to delayed cracking in the stainless steel is achieved limiting the total hydrogen content of the stainless steel measured by inert gas fusion method below 4 weight ppm, preferably below 3 weight ppm by a heat treatment performed at the temperature range between 100° C. and 700° C. for 0.1-300 hours, preferably at 200-600° C. for 1-100 hours, and more preferably at 250-500° C. for 1-100 hours.

## Claims

### Claim 1

Stainless steel exhibiting transformation-induced plasticity (TRIP) effect resistant to delayed cracking, characterized in that the resistance to delayed cracking for a flat stainless steel product is achieved limiting the total hydrogen content of the steel measured by inert gas fusion method below 4 weight ppm, by a heat treatment performed at the temperature range between 100° C. and 700° C. for 0.1-300 hours, preferably at 200-600° C. for 1-100 hours.

### Claim 2 (depends on 1)

Stainless steel exhibiting transformation-induced plasticity (TRIP) effect according to the claim 1, characterized in that the stainless steel is an austenitic stainless steel containing in weight % 0-0.15% C, 0-3% Si, 0-15% Mn, 10-30% Cr, 0-8% Ni, 0-3% Mo, 0-3% Cu, 0-0.5% N, 0-0.5% Nb, 0-0.5% Ti, 0-0.5% V, the balance of Fe and inevitable impurities including hydrogen.

### Claim 3 (depends on 1)

Stainless steel exhibiting transformation-induced plasticity (TRIP) effect according to the claim 1, characterized in that the stainless stainless steel is a duplex austenitic-ferritic stainless steel whose microstructure contains 10-95% ferrite phase and which contains in weight % 0-0.10% C, 0-2% Si, 0-10% Mn, 10-30% Cr, 0-8% Ni, 0-3% Mo, 0-3% Cu, 0-0.4% N, 0-0.5% Nb, 0-0.5% Ti, 0-0.5% V, the balance of Fe and inevitable impurities including hydrogen.

### Claim 4 (depends on 1)

Stainless steel exhibiting transformation-induced plasticity (TRIP) effect according to claim 1, characterized in that the stainless steel is in the form of a flat product such as a plate, a sheet, a strip, a coil.

### Claim 5 (depends on 1)

Stainless steel exhibiting transformation-induced plasticity (TRIP) effect according to claim 1, characterized in that for the stainless steel after deep drawing a drawing ratio up to 2.0 or even higher is achieved without occurrence of delayed cracking.

### Claim 6

Method for producing a stainless steel exhibiting transformation-induced plasticity (TRIP) effect and resistant to delayed cracking, characterized in that for the resistance to delayed cracking the steel is heat treated at the temperature range between 100C and 700° C. for 0.1-300 hours.

### Claim 7 (depends on 6)

Method according to the claim 6, characterized in that the steel is heat treated in a batch furnace, to reduce hydrogen content of the steel and improve the resistance to delayed cracking.

### Claim 8 (depends on 6)

Method according to the claim 6, characterized in that the steel is heat treated in a continuous annealing line to reduce hydrogen content and improve the resistance to delayed cracking.

### Claim 9 (depends on 6)

Method according to the claim 6, characterized in that the heat treatment is performed in atmosphere containing at least partly protective gas to enhance effusion of hydrogen from the steel.

### Claim 10 (depends on 6)

Method according to the claim 6, characterized in that the heat treatment is performed in vacuum to enhance effusion of hydrogen from the steel.

### Claim 11 (depends on 6)

Method according to the claim 6, characterized in that the heat treatment is performed in air atmosphere to enhance effusion of hydrogen from the steel.

### Claim 12 (depends on 6)

Method according to claim 6, characterized in that the steel is strengthened by cold-rolling before the heat treatment.

### Claim 13 (depends on 6)

Method according to claim 6, characterized in that the steel is strengthened by cold-rolling after the heat treatment.