# US 2016/0145472 A1 · Adhesive composition and display device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0145472 A1
- Document ID: US20160145472A1
- Status: Published application
- Kind: A1
- Application number: 14/884,589
- Filed: 2015-10-15
- Published: 2016-05-26
- Earliest claimed: 2014-11-24
- Assignees: Samsung Display Co., Ltd.
- Applicants: Samsung Display Co., Ltd.
- Inventors: Junho Kwack; Jongsung You
- Web page: https://patentgrep.com/patent/US20160145472A1

## CPC

- C09J 109/00: Adhesives based on homopolymers or copolymers of conjugated diene hydrocarbons
- C09J 133/00: Adhesives based on homopolymers or copolymers of compounds having one or more unsaturated aliphatic radicals, each having only one carbon-to-carbon double bond, and at least one being terminated by only one carboxyl radical, or of salts, anhydrides, esters, amides, imides, or nitriles thereof; Adhesives based on derivatives of such polymers
- B32B 7/12: using interposed adhesives or interposed materials with bonding properties
- B32B 2037/1253: {curable adhesive}
- B32B 2305/72: Cured, e.g. vulcanised, cross-linked
- B32B 2310/0831: using UV radiation
- B32B 2457/20: Displays, e.g. liquid crystal displays, plasma displays
- C09J 11/06: organic
- C09J: ADHESIVES; NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL; ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE; USE OF MATERIALS AS ADHESIVES (preparation of glue or gelatine C09H)
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM

## Abstract

Disclosed are an adhesive composition that includes: a first photopolymerization initiator having a maximum absorption wavelength in a range of about 350 nm to about 370 nm and a second photopolymerization initiator having a maximum absorption wavelength in a range of about 380 nm to about 390 nm, and a method of manufacturing a display device.

## Claims

### Claim 1

An adhesive composition comprising:
a monomer in an amount of about 15 percentage by weight (wt %) to about 30 wt % with respect to the total weight of the adhesive composition;
an oligomer in an amount of about 20 wt % to about 40 wt % with respect to the total weight of the adhesive composition;
a rubber-based elastic component in an amount of about 25 wt % to about 50 wt% with respect to the total weight of the adhesive composition; and
a photopolymerization initiator in an amount of about 2 wt % to 7 wt % with respect to the total weight of the adhesive composition,
wherein the photopolymerization initiator comprises a first photopolymerization initiator photo-sensitive in a range of a wavelength from about 350 nm to about 370 nm and a second photopolymerization initiator photo-sensitive in a range of a wavelength from about 380 nm to about 390 nm, and
the first photopolymerization initiator and the second photopolymerization initiator have a content ratio of about 5˜2:1.

### Claim 2 (depends on 1)

The adhesive composition of claim 1, wherein the first photopolymerization initiator is represented by at least one of the following Chemical Formulas 1 through 3:

### Claim 3 (depends on 1)

The adhesive composition of claim 1, wherein the second photopolymerization initiator is represented by the following Chemical Formula 4:

### Claim 4 (depends on 1)

The adhesive composition of claim 1, wherein the monomer is at least one selected from the group consisting of isobornyl acrylate, n-octyl acrylate, tetrahydrofurfuryl acrylate, and 4-hydroxy butyl acrylate.

### Claim 5 (depends on 1)

The adhesive composition of claim 1, wherein the oligomer is at least one selected from the group consisting of urethane (meth)acrylate and ester (meth)acrylate that have a weight average molecular weight(Mw) in a range of about 5,000 Mw to about 50,000 Mw.

### Claim 6 (depends on 1)

The adhesive composition of claim 1, wherein the rubber-based elastic component is at least one selected from the group consisting of polybutadiene and polyisoprene that have a weight average molecular weight (Mw) in a range of about 10,000 Mw to about 100,000 Mw.

### Claim 7

A method of manufacturing a display device comprising:
coating an adhesive composition on a surface of a display panel;
performing a first curing of the adhesive composition using a first light source;
disposing a window on the adhesive composition subject to the first curing and compressing the window toward the display panel; and
performing a second curing of the adhesive composition subject to the first curing by irradiating light on the window using a second light source,
wherein the adhesive composition comprises:
a monomer in an amount of about 15 wt % to about 30 wt % with respect to the total weight of the adhesive composition;
an oligomer in an amount of about 20 wt % to about 40 wt % with respect to the total weight of the adhesive composition; and
a rubber-based elastic component in an amount of about 25 wt % to about 50 wt % with respect to the total weight of the adhesive composition;
a photopolymerization initiator in an amount of about 2 wt % to 7 wt % with respect to the total weight of the adhesive composition,
wherein the photopolymerization initiator comprises a first photopolymerization initiator having a photo-sensitive range of a wavelength from about 350 nm to about 370 nm and a second photopolymerization initiator having a photo-sensitive range of a wavelength from about 380 nm to about 390 nm,
the first photopolymerization initiator and the second photopolymerization initiator have a content ratio (i.e., weight ratio) of about 5˜2:1, and
the second light source emits light having a wavelength longer than that of the first light source.

### Claim 8 (depends on 7)

The method of claim 7, wherein the first photopolymerization initiator is represented by at least one of the following Chemical Formulas 1 to 3:

### Claim 9 (depends on 7)

The method of claim 7, wherein the second photopolymerization initiator is represented by the following Chemical Formula 4:

### Claim 10 (depends on 7)

The method of claim 7, wherein the first light source emits an ultraviolet ray having a wavelength in a range of about 350 nm to about 370 nm.

### Claim 11 (depends on 7)

The method of claim 7, wherein the second light source emits an ultraviolet ray having a wavelength in a range of about 380 nm to about 390 nm.

### Claim 12 (depends on 7)

The method of claim 7, wherein the display panel is one of a liquid crystal display panel and an organic light emitting diode display panel.

### Claim 13

A display device comprising:
a display panel;
an adhesive layer on the display panel; and
a window on the adhesive layer,
wherein the adhesive layer comprises an adhesive polymer resin, a rubber-based elastic component, and a photopolymerization initiator, and
the photopolymerization initiator comprises a first photopolymerization initiator having a maximum absorption wavelength in a range of about 350 nm to about 370 nm and a second photopolymerization initiator having a maximum absorption wavelength in a range of about 380 nm to about 390 nm.

### Claim 14 (depends on 13)

The display device of claim 13, wherein the adhesive layer has:
an elasticity in a range of about 0.10 Mpa to about 0.30 Mpa;
an elongation index in a range of about 100% to about 300%;
a refractive index in a range of about 1.49 to about 1.53;
a transmittance more than about 92%; and
a glass transition temperature in a range of about −10° C. to about −5° C.