# US 2016/0145150 A1 · Methods for producing strengthened and durable glass containers

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0145150 A1
- Document ID: US20160145150A1
- Status: Published application
- Kind: A1
- Application number: 14/949,320
- Filed: 2015-11-23
- Published: 2016-05-26
- Earliest claimed: 2014-11-26
- Assignees: Corning Incorporated
- Applicants: Corning Incorporated
- Inventors: Dana Craig Bookbinder; Richard Michael Fiacco; Timothy Michael Gross
- Web page: https://patentgrep.com/patent/US20160145150A1

## CPC

- C03C 15/02: for making a smooth surface
- A61J 1/1468: {Containers characterised by specific material properties}
- C03B 23/11: Reshaping by drawing without blowing, in combination with separating, e.g. for making ampoules
- C03C 4/20: for chemical resistant glass
- C03C 15/00: Surface treatment of glass, not in the form of fibres or filaments, by etching (etching or surface-brightening compositions, in general C09K13/00)
- C03C 17/005: {Coating the outside}
- C03C 17/30: with silicon-containing compounds
- C03C 17/32: with synthetic or natural resins (C03C17/30 takes precedence)
- C03C 21/002: {to perform ion-exchange between alkali ions (C03C21/005 takes precedence)}
- C03C 23/00: Other surface treatment of glass not in the form of fibres or filaments
- C03C 23/0075: {Cleaning of glass (specially adapted to plate glass B08B11/00)}
- A61J 1/05: for collecting, storing or administering blood, plasma or medical fluids {(multiple bags systems for separating or storing blood components A61M1/0209); Infusion or perfusion containers}
- C03C 2217/70: Properties of coatings
- Y02P 40/57: Improving the yield, e-g- reduction of reject rates
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- A61J: CONTAINERS SPECIALLY ADAPTED FOR MEDICAL OR PHARMACEUTICAL PURPOSES; DEVICES OR METHODS SPECIALLY ADAPTED FOR BRINGING PHARMACEUTICAL PRODUCTS INTO PARTICULAR PHYSICAL OR ADMINISTERING FORMS; DEVICES FOR ADMINISTERING FOOD OR MEDICINES ORALLY; BABY COMFORTERS; DEVICES FOR RECEIVING SPITTLE
- C03B: MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A method of forming a glass container including forming a glass container having a sidewall at least partially enclosing an interior volume, at least a portion of an interior surface of the sidewall having an interior surface layer; and contacting the glass container with a substantially fluoride-free aqueous treating medium to remove a thin layer of the interior surface layer having a thickness of from about 100 nm to about 1.0 μm from the interior surface of the sidewall. The interior surface is resistant to delamination. Before contacting the glass container with the substantially fluoride-free aqueous treating medium, the exterior surface of the sidewall comprises strength-limiting surface flaws having a first shape, and after the contacting the exterior surface of the sidewall with the substantially fluoride-free aqueous treating medium, the strength-limiting surface flaws have a second shape.

## Claims

### Claim 1

A method of forming a glass container, the method comprising:
forming a glass container comprising a sidewall at least partially enclosing an interior volume, at least a portion of an interior surface of the sidewall having an interior surface layer; and
contacting the glass container with a substantially fluoride-free aqueous treating medium to remove a thin layer of the interior surface layer having a thickness of from about 100 nm to about 1.0 μm from the interior surface of the sidewall, wherein
the interior surface is resistant to delamination.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the glass container has a delamination factor of less than or equal to 10 after the thin layer of the interior surface layer is removed.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the thin layer of the interior surface layer that is removed has a thickness of from about 100 nm to about 750 nm.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the substantially fluoride-free aqueous treating medium comprises about 0.001 weight percent to about 0.15 weight percent fluoride ions.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the substantially fluoride-free aqueous treating medium is a substantially fluoride-free aqueous acidic treating medium comprising a member selected from the group consisting of HCl, HBr, HNO3, H2SO4, H2SO3, H3PO4, H3PO2, HOAc, citric acid, tartaric acid, ascorbic acid, ethylenediaminetetraacetic acid, methanesulfonic acid, toluenesulfonic acid, a mixture thereof, and a combination comprising at least one of the foregoing acids.

### Claim 6 (depends on 5)

The method according to claim 5, wherein the substantially fluoride-free aqueous acidic treating medium comprises a member selected from the group consisting of HCl, HNO3, H2SO4, and H3PO4.

### Claim 7 (depends on 5)

The method according to claim 5, wherein the substantially fluoride-free aqueous acidic treating medium has a pH of less than or equal to about 3.

### Claim 8 (depends on 1)

The method according to claim 1, wherein the substantially fluoride-free aqueous treating medium comprises about 0.001 weight percent to about 0.015 weight percent fluoride ions.

### Claim 9 (depends on 1)

The method according to claim 1, wherein the glass container is formed from a Type I, Class A or a Type I, Class B glass according to ASTM Standard E438-92.

### Claim 10 (depends on 1)

The method according to claim 1, wherein the glass container is formed from a borosilicate glass.

### Claim 11 (depends on 1)

The method according to claim 1, further comprising contacting an exterior surface of the sidewall with the substantially fluoride-free aqueous treating medium.

### Claim 12 (depends on 11)

The method according to claim 11, wherein, before the exterior surface of the sidewall is contacted with the substantially fluoride-free aqueous treating medium, the exterior surface of the sidewall comprises strength-limiting surface flaws having a first shape, and
after the contacting the exterior surface of the sidewall with the substantially fluoride-free aqueous treating medium, the strength-limiting surface flaws have a second shape.

### Claim 13 (depends on 12)

The method according to claim 12, wherein the second shape comprises blunted crack tips.

### Claim 14 (depends on 11)

The method according to claim 11, wherein the glass container is an ion-exchange-strengthened glass container comprising a surface compressive stress layer on at least the exterior surface of the sidewall.

### Claim 15 (depends on 14)

The method according to claim 14, wherein the exterior surface of the sidewall has a compressive stress of greater than or equal to about 250 MPa.

### Claim 16 (depends on 14)

The method according to claim 14, wherein a level of surface compression is reduced by an amount of from about 0.1% to about 4% by contacting the exterior surface of the sidewall with the substantially fluoride-free aqueous treating medium.

### Claim 17 (depends on 1)

The method according to claim 1, further comprising applying a low-friction coating on at least the exterior surface of the sidewall.

### Claim 18 (depends on 17)

The method according to claim 17, wherein the low-friction coating is thermally stable.

### Claim 19

A method of forming a glass container, the method comprising:
forming a glass container comprising a sidewall at least partially enclosing an interior volume, the sidewall having an exterior surface comprising an exterior surface layer; and
contacting the glass container with a substantially fluoride-free aqueous treating medium to remove a thin layer of the exterior surface layer having a thickness of from about 100 nm to about 1.0 μm from the exterior surface of the sidewall, wherein
before contacting the glass container with the substantially fluoride-free aqueous treating medium, the exterior surface of the sidewall comprises strength-limiting surface flaws having a first shape, and
after the contacting the exterior surface of the sidewall with the substantially fluoride-free aqueous treating medium, the strength-limiting surface flaws have a second shape.

### Claim 20 (depends on 19)

The method according to claim 19, wherein the second shape comprises blunted crack tips.

### Claim 21 (depends on 19)

The method according to claim 19, wherein the thin layer of the exterior surface layer that is removed has a thickness of from about 100 nm to about 750 nm.

### Claim 22 (depends on 19)

The method according to claim 19, wherein the substantially fluoride-free aqueous treating medium comprises about 0.001 weight percent to about 0.15 weight percent fluoride ions.

### Claim 23 (depends on 19)

The method according to claim 19, wherein the glass container is formed from a Type I, Class A or a Type I, Class B glass according to ASTM Standard E438-92.

### Claim 24 (depends on 19)

The method according to claim 19, wherein the substantially fluoride-free aqueous treating medium is a substantially fluoride-free aqueous acidic treating medium comprising a member selected from the group consisting of HCl, HBr, HNO3, H2SO4, H2SO3, H3PO4, H3PO2, HOAc, citric acid, tartaric acid, ascorbic acid, ethylenediaminetetraacetic acid, methanesulfonic acid, toluenesulfonic acid, a mixture thereof, and a combination comprising at least one of the foregoing acids.

### Claim 25 (depends on 19)

The method according to claim 19, wherein the glass container is an ion-exchange-strengthened glass container comprising a surface compressive stress layer on at least the exterior surface of the sidewall.

### Claim 26 (depends on 25)

The method according to claim 25, wherein the exterior surface of the sidewall has a compressive stress of greater than or equal to about 250 MPa.

### Claim 27 (depends on 25)

The method according to claim 25, wherein a level of surface compression is reduced by an amount of from about 0.1% to about 4% by contacting the exterior surface of the sidewall with the substantially fluoride-free aqueous treating medium.

### Claim 28 (depends on 19)

The method according to claim 19, further comprising applying a low-friction coating on at least the exterior surface of the sidewall.

### Claim 29 (depends on 28)

The method according to claim 28, wherein the low-friction coating is thermally stable.