# US 2016/0145149 A1 · Etch rate enhancement at low temperatures

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2016/0145149 A1
- Document ID: US20160145149A1
- Status: Published application
- Kind: A1
- Application number: 14/899,602
- Filed: 2014-06-20
- Published: 2016-05-26
- Earliest claimed: 2013-06-21
- Assignees: Corning Incorporated
- Applicants: Corning Incorporated
- Inventors: Robert Carl Burket; Benedict Yorke Johnson; Samuel Odei Owusu; Tammy Lynn Petriwsky
- Web page: https://patentgrep.com/patent/US20160145149A1

## CPC

- C03C 15/00: Surface treatment of glass, not in the form of fibres or filaments, by etching (etching or surface-brightening compositions, in general C09K13/00)
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS

## Abstract

A method etching a glass material comprises providing an etchant comprising 10-30% HF, 5-15% HNO3, and at least 10% H3PO4 by volume constituted such that the ratio HF:HNO3 by volume is in the range of 1.7:1 to 2.3:1, providing a glass material to be etched, and contacting the glass material with the etchant. The etchant desirably has no other acid components. The method may be performed with the etchant temperature within the range of 20-30° C. The glass material may be an aluminosilicate glass. Ultrasound energy may be applied to the etchant, to the glass material, or both.

## Claims

### Claim 1

A method of etching a glass material comprising:
providing an etchant comprising 10-30% HF, 5-15% HNO3, and at least 10% H3PO4 by volume further wherein the ratio HF:HNO3 by volume is in the range of 1.7:1 to 2.3:1;
providing a glass material to be etched; and
contacting the glass material with the etchant.

### Claim 2 (depends on 1)

The method according to claim 1, further comprising the step of controlling the temperature of the etchant to a temperature within the range of 20-30° C.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the step of providing a glass material to be etched comprises providing an aluminosilicate glass material to be etched.

### Claim 4 (depends on 1)

The method according to claim 1 wherein the step of providing an etchant comprises providing an etchant wherein the ratio HF:HNO3 by volume is in the range of 1.8:1 to 2.2:1.

### Claim 5 (depends on 1)

The method according to claim 1 wherein the step of providing an etchant comprises providing an etchant wherein the ratio HF:HNO3 by volume is in the range of 1.9:1 to 2.1:1.

### Claim 6 (depends on 1)

The method according to claim 1 wherein the step of providing an etchant comprises providing an etchant wherein the ratio HF:HNO3 by volume is in the range of 1.95:1 to 2.05:1.

### Claim 7 (depends on 1)

The method according to claim 1 wherein the step of providing an etchant comprises providing an etchant comprising at least 20% H3PO4.

### Claim 8 (depends on 1)

The method according to claim 1 wherein the step of providing an etchant comprises providing an etchant comprising at least 40% H3PO4.

### Claim 9 (depends on 1)

The method according to claim 1 wherein the step of providing an etchant comprises providing an etchant comprising 15-25% HF and 7.5-12.5% HNO3.

### Claim 10 (depends on 1)

The method according to claim 1 wherein the step of providing an etchant comprises providing an etchant comprising 19-21% HF and 9.5-10.5% HNO3.

### Claim 11 (depends on 1)

The method according to claim 1 wherein the step of providing an etchant comprises providing an etchant containing only three acid components: HF, HNO3, and H3PO4.

### Claim 12 (depends on 1)

The method according to claim 1 wherein the step of providing an etchant comprises providing an etchant containing only water and three acid components: HF, HNO3, and H3PO4.

### Claim 13 (depends on 1)

The method according to claim 1, further comprising the step of controlling the temperature of the etchant to a temperature within the range of 22-28° C.

### Claim 14 (depends on 1)

The method according to claim 1, further comprising the step of applying ultrasound to the etchant.

### Claim 15 (depends on 1)

The method according to claim 1, further comprising the step of applying ultrasound to the glass material to be etched.